journal article·2020-05

Surface modification of feldspar porcelain by corona discharge and its effect on bonding to resin cement with silane coupling agent

Yuya Komagata, Hiroshi Ikeda, Yuki Fujio, Yuki Nagamatsu, Hiroshi Shimizu

Publisher page

Abstract

This study aims to develop a corona discharge process for a surface treating a glass-ceramic, feldspar porcelain, to improve its bonding to a resin cement with a silane-coupling agent. Corona discharge, a type of plasma process, was performed using a custom-made device on a porcelain surface at temperatures ranging from 25 to 300 °C, for specific treatment times in air. The porcelain was then subjected to a post-heat-treatment at 600 °C to condition the surface state. The resulting surface was primed with a silane-coupling-agent followed by cementing using a resin cement to measure the shear bond strength (SBS). To investigate the effect of surface modifications by the corona discharge treatment, the porcelain was characterized by surface roughness, contact angle, and an X-ray photoelectron spectroscopy analyses. The SBS for the corona-discharge-treated porcelain increased with an increase in treatment-temperature and -time, and reached the maximum value at 200 °C and 5 min. The post-heat-treatment improved the bond durability after thermocycling. The SBS for the corona-discharge-treated porcelain was then compared to that of a conventional hydrofluoric-acid-treated one, which showed that the SBSs were comparable. The results of the surface characterizations indicated that the corona discharge treatment generated silanol groups on the porcelain surface giving hydrophilic properties without roughening the surface. It was found that the corona discharge treatment generates silanol groups on the porcelain surface, resulting in an increased SBS. This study is the first to demonstrate that corona discharge treatment is effective for improving bond strength through the modification of the surface of glass-ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Modification and Superhydrophobicity · Dental materials and restorations · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Simulation of corona discharge in point–plane configuration10.1016/j.elstat.2004.01.021 ↗
2. Microtensile bond strength of resin cement to a feldspathic ceramic10.1089/pho.2009.2746 ↗
3. Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions10.1016/j.dental.2006.11.011 ↗
4. Analysis of tensile bond strengths using Weibull statistics10.1016/j.biomaterials.2004.01.060 ↗
5. Plasma in dentistry10.1016/j.cpme.2014.04.002 ↗
6. Corona discharge processes10.1109/27.125038 ↗
7. A novel approach for improvement of the interfacial binding of ceramics for dental materials: chemical treatment and oxygen plasma etching10.1002/app.28432 ↗
8. Ceramics for dental applications: a review10.3390/ma3010351 ↗
9. Aging effect of atmospheric air on lithium disilicate ceramic after nonthermal plasma treatment10.1016/j.prosdent.2015.11.008 ↗
10. Effect of different times of nonthermal argon plasma treatment on the microtensile bond strength of self-adhesive resin cement to yttria-stabilized tetragonal zirconia polycrystal ceramic10.1016/j.prosdent.2018.03.025 ↗
11. Surface roughness and bond strengths of glass-infiltrated alumina-ceramics prepared using various surface treatments10.1016/j.jdent.2009.06.017 ↗
12. Study of poling behavior of biaxially stretched poly(vinylidene fluoride) films using the constant-current corona triode10.1063/1.359682 ↗
13. An XPS analysis of different SiO2 modifications employing a C 1s as well as an Au 4f7/2 static charge reference10.1002/sia.740180110 ↗
14. Effect of surface modifications on the bond strength of zirconia ceramic with resin cement resin10.1016/j.dental.2016.02.001 ↗
15. Long term water storage deteriorates bonding of composite resin to alumina and zirconia short communication10.2174/1874210601307010123 ↗
16. XPS analysis of the surface of leucite-reinforced feldspathic ceramics10.1016/S0109-5641(00)00032-4 ↗
17. Comparison of two test designs for evaluating the shear bond strength of resin composite cements10.1016/j.dental.2015.11.023 ↗
18. Generation of alkali-free and high-proton concentration layer in a soda lime glass using non-contact corona discharge10.1063/1.4817760 ↗
19. Influence of atmospheric pressure low-temperature plasma treatment on the shear bond strength between zirconia and resin cement10.1016/j.jpor.2016.02.001 ↗
20. Thin film fabrication of PMMA/MEH-PPV immiscible blends by corona discharge coating and its application to polymer light emitting diodes10.1021/la062341h ↗
21. Accelerated formation of sodium depletion layer on soda lime glass surface by corona discharge treatment in hydrogen atmosphere10.1016/j.apsusc.2014.02.024 ↗
22. Alkali ion migration between stacked glass plates by corona discharge treatment10.1016/j.apsusc.2015.02.113 ↗
23. Plasma in dentistry: a review of basic concepts and applications in dentistry10.3109/00016357.2013.795660 ↗
24. Ceramic dental biomaterials and CAD/CAM technology: state of the art10.1016/j.jpor.2014.07.003 ↗
25. Impact of plasma treatment of PMMA-based CAD/CAM blanks on surface properties as well as on adhesion to self-adhesive resin composite cements10.1016/j.dental.2013.06.004 ↗
26. Nonthermal atmospheric plasmas in dental restoration10.1177/0022034516629425 ↗
27. Promoting porcelain-zirconia bonding using different atmospheric pressure gas plasmas10.1016/j.dental.2018.05.004 ↗
28. Effects of surface treatments on bond strength of glass-infiltrated ceramic
29. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
30. Innovative surface treatments for improved ceramic bonding: lithium disilicate glass ceramic10.1016/j.ijadhadh.2017.12.007 ↗
31. Does plasma irradiation improve shear bond strength of acrylic resin to cobalt-chromium alloy?10.1016/j.dental.2003.04.001 ↗
32. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
33. Bonding of resin composites to etchable ceramic surfaces - an insight review of the chemical aspects on surface conditioning10.1111/j.1365-2842.2005.01569.x ↗
34. XPS study of the state of oxygen on a chemically treated glass surface10.1002/sia.740150604 ↗
35. XPS study of non-bridging oxygens in Na2O-SiO2 gels10.1016/0022-3093(88)90466-8 ↗
36. Effect of plasma treatment on adhesion of self-curing repair resin to acrylic denture base10.4012/dmj.23.545 ↗
37. Plasma treatment increased shear bond strength between heat cured acrylic resin and self-curing acrylic resin10.1046/j.1365-2842.2003.01198.x ↗
38. The effect of surface treatment on the shear bond strength of luting cement to a glass-infiltrated alumina ceramic
39. Evidence of Si–OH species at the surface of aged silica10.1116/1.577726 ↗
40. The effect of plasma on shear bond strength between resin cement and colored zirconia10.4047/jap.2017.9.2.118 ↗
41. Thermal poling of silica in air and under vacuum: the influence of charge transport on second harmonic generation10.1063/1.123868 ↗
42. Nonthermal plasma in dentistry: an update10.4103/jispcd.JISPCD_29_17 ↗
43. Dentin surface treatment using a non-thermal argon plasma brush for interfacial bonding improvement in composite restoration10.1111/j.1600-0722.2010.00761.x ↗
44. Hologram replication technique in glass plates using corona charging10.1063/1.2459675 ↗
45. Bonding strength of resin cement to silicate glass ceramics for dental CAD/CAM systems is enhanced by combination treatment of the bonding surface10.4012/dmj.26.713 ↗
46. Bonding efficacy of 4-META/MMA-TBB resin to surface-treated highly translucent dental zirconia
47. Use of metal conditioners to improve bond strengths of autopolymerizing denture base resin to cast Ti-6Al-7Nb and Co-Cr10.1016/j.jdent.2005.05.002 ↗
48. Thermal poling of alkaline earth boroaluminosilicate glasses with intrinsically high dielectric breakdown strength10.1063/1.3703679 ↗
49. Molecular orientation of silane at the surface of colloidal silica10.1177/00220345930720061001 ↗
50. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
51. Surface characterisation and bonding of Y-TZP following non-thermal plasma treatment10.1016/j.jdent.2012.10.002 ↗
52. Cementation of glass-ceramic posterior restorations: a systematic review10.1155/2015/148954 ↗
53. Surface characterization of lithium disilicate ceramic after nonthermal plasma treatment10.1016/j.prosdent.2014.02.021 ↗
54. Evaluation of the bond strength and characteristics of zirconia after different surface treatments10.1016/j.prosdent.2018.01.029 ↗
55. “Digitally oriented materials”: focus on lithium disilicate ceramics10.1155/2016/9840594 ↗
56. The surface chemistry of amorphous silica. Zhuravlev model10.1016/S0927-7757(00)00556-2 ↗