Investigation of material removal mechanisms and ductile-brittle transition zone of zirconia ceramics sintered at various temperatures
Source abstract
Abstract
Sintering is a comprehensive process that involves the complex evolution of material microstructures and properties, being recognized as a critical factor to improve the machinability of ceramics. The present work aims to address the evolution of the material removal mechanisms of the 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) during the sintering process based on the micro scratching tests. The impacts of sintering temperatures on the material removal behaviors, including scratching forces, scratch morphologies, specific scratching energies, and critical transition depths, were rigorously studied. The acquired results indicate that the intergranular bonding strength is a critical factor that determinines the material removal mechanisms of 3Y-TZP, and 1100 °C signifies the transition threshold for the material removal mode. After 1100 °C, the material removal mechanism has gradually converted into the typical ductile-brittle removal regime. Moreover, the critical depth in ductile regime at 1200 °C is about 1.89 times that at 1500 °C, and the critical depth of ductile-brittle transition at 1200 °C is approximately 2.08 times that at 1500 °C.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Dental materials and restorations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Surface quality of yttria-stabilized tetragonal zirconia polycrystal in CAD/CAM milling, sintering, polishing and sandblasting processes10.1016/j.jmbbm.2016.08.021 ↗
2. Nanoindentation characterization of the elasticity, plasticity and machinability of zirconia10.1016/j.msea.2015.01.051 ↗
3. Assessment of elasticity, plasticity and resistance to machining-induced damage of porous pre-sintered zirconia using nanoindentation techniques10.1016/j.jmst.2016.02.009 ↗
4. Machinability of a newly developed pre-sintered zirconia block for dental crown applications10.1016/j.matlet.2019.126996 ↗
5. A predictive model of the critical undeformed chip thickness for ductile–brittle transition in nano-machining of brittle materials10.1016/j.ijmachtools.2012.08.005 ↗
6. Transformation of fracture mechanism and damage behavior of ceramic-matrix composites during nano-scratching10.1016/j.compositesa.2019.105756 ↗
7. Effect of agglomeration on mechanical properties of porous zirconia fabricated by partial sintering10.1111/j.1151-2916.2002.tb00388.x ↗
8. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
9. Ceramics for dental applications: a review10.3390/ma3010351 ↗
10. Low-temperature sintering and microstructural development of nanocrystalline Y-TZP powders10.1016/0955-2219(96)00015-5 ↗
11. Net-shaping of ceramic components by direct ceramic machining10.1108/01445150310501217 ↗
12. Failure process of rock slopes with cracks based on the fracture mechanics method10.1016/j.enggeo.2017.10.020 ↗
13. Processing and properties of advanced porous ceramics: an application based review10.1016/j.ceramint.2014.06.095 ↗
14. Enhanced hydrophilicity and tribological behavior of dental zirconia ceramics based on picosecond laser surface texturing10.1016/j.ceramint.2019.11.210 ↗
15. Influence of sintering temperatures on material properties and corresponding milling machinability of zirconia ceramics10.1016/j.jmapro.2021.05.012 ↗
16. Toward the mechanisms of surface texturing on the wear behavior of dental zirconia ceramics under dry and saliva lubricated conditions10.1016/j.wear.2021.203845 ↗
17. Densification and grain growth of nanocrystalline 3Y-TZP during two-step sintering10.1016/j.jeurceramsoc.2008.04.030 ↗
18. Effect of laser surface texturing on primary stability and surface properties of zirconia implants10.1016/j.ceramint.2017.08.058 ↗
19. An overview of the current status of national reporting systems for adverse reactions to dental materials10.1016/j.jdent.2004.02.001 ↗
20. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
21. Grain growth kinetics of 3 mol. % yttria-stabilized zirconia during flash sintering10.1016/j.jeurceramsoc.2018.11.032 ↗
22. Brittle-ductile transition phenomena in microindentation and micromachining10.1016/S0007-8506(07)62377-4 ↗
23. Study and characterization of the ductile-brittle transition zone in sintered zirconia10.1016/j.jmapro.2020.08.057 ↗
24. The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio10.1007/s00784-012-0692-6 ↗
25. A computer program of master sintering curve model to accurately predict sintering results
26. Abrasive machining of silicon10.1016/S0007-8506(07)62999-0 ↗
27. Corrosion of alloys used in dentistry: a review10.1016/j.msea.2006.05.003 ↗
28. Influence of microstructure on indentation and machining of dental glass-ceramics10.1557/JMR.1996.0296 ↗
29. Maximum undeformed equivalent chip thickness for ductile-brittle transition of zirconia ceramics under different lubrication conditions10.1016/j.ijmachtools.2017.06.003 ↗
30. Investigation of ductile-brittle transition in machining of yttrium-stabilized zirconia (YSZ)10.1016/j.promfg.2018.07.052 ↗
31. Surface characterization of zirconia dental implants