Fatigue limit of monolithic Y-TZP three-unit-fixed dental prostheses: Effect of grinding at the gingival zone of the connector
Source abstract
Abstract
Objectives To determine the fatigue limits of three-unit monolithic zirconia fixed dental prosthesis (FDPs) before and after grinding of the gingival areas of connectors with diamond burs. Material and methods FDPs were milled from pre-sintered blocks of zirconia simulating the absence of the first mandibular molar. Half of the specimens were subjected to grinding, simulating clinical adjustment, and all of them were subjected to glazing procedure. Additional specimens were manufactured for roughness analysis. FDPs were adhesively cemented onto glass-fiber reinforced epoxy resin abutments. Fatigue limits and standard deviations were obtained using a staircase fatigue method (n=20, 100,000 loading cycles/5Hz). The initial test load was 70% of the mean load-to-fracture (n=3) and load increments were 5% of the initial test load for both the control and ground specimens. Data were compared by Student's T-test (α≤0.05). Results Both the control and ground groups exhibited similar values of load-to-fracture and fatigue limits. Neither the surface treatments nor ageing affected the surface roughness of the specimens. Conclusions The damage induced by grinding with fine-grit diamond bur in the gingival area of the connectors did not decrease the fatigue limit of the three-unit monolithic zirconia FDP.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach10.1016/j.dental.2008.09.001 ↗
2. Fatigue behavior of Y-TZP ceramic after surface treatments
3. Adhesive cementation promotes higher fatigue resistance to zirconia crowns10.2341/16-002-L ↗
4. The clinical success of all-ceramic restorations
5. Strength determination of brittle materials as curved monolithic structures10.1177/0022034514523621 ↗
6. Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns10.3109/00016357.2013.822098 ↗
7. The effect of low temperature aging on the mechanical property & phase stability of Y-TZP ceramics10.4047/jap.2009.1.3.113 ↗
8. Concerns of hydrothermal degradation in CAD/CAM zirconia10.1177/0022034509354193 ↗
9. Influence of preliminary damage on the load-bearing capacity of zirconia fixed dental prostheses10.1111/j.1532-849X.2010.00640.x ↗
10. Initial bacterial adhesion on resin, titanium and zirconia in vitro10.4047/jap.2011.3.2.81 ↗
11. Six-year clinical performance of lithium disilicate fixed partial dentures
12. Effect of connector design on the fracture resistance of all-ceramic fixed partial dentures10.1067/mpr.2002.123850 ↗
13. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging10.1016/j.jmbbm.2016.01.006 ↗
14. Effect of low-temperature aging on the mechanical behavior of ground Y-TZP10.1016/j.jmbbm.2014.12.009 ↗
15. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
16. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: multiple-unit FDPs10.1016/j.dental.2015.02.013 ↗
17. Randomized controlled clinical trial of zirconia-ceramic and metal-ceramic posterior fixed dental prostheses: a 3-year follow-up
18. Prospective clinical study of zirconia-based posterior four-unit fixed dental prostheses: four-year follow-up
19. Zirconia posterior fixed partial dentures: 5-year clinical results of a prospective clinical trial
20. Survival rates of a lithium disilicate-based core ceramic for three-unit esthetic fixed partial dentures: a 10-year prospective study10.11607/ijp.3045 ↗
21. Effects of two grading techniques of zirconia material on the fatigue limit of full-contour 3-unit fixed dental prostheses10.1016/j.dental.2016.12.010 ↗
22. Clinical outcome of three-unit lithium-disilicate glass–ceramic fixed dental prostheses: up to 8 years results10.1016/j.dental.2009.05.003 ↗
23. Role of H2O on the degradation process of Y-TZP10.1007/BF01756800 ↗