Corrosion induced fracture of NiTi wires in simulated oral environments
Source abstract
Abstract
This work aims to assess the influence of corrosion on fracture of nickel titanium (NiTi) superelastic wires in physiological solutions (9 g/l NaCl) with and without addition of 1 g/l NaF. The electrochemical cell was coupled to a Hounsfield Tensiometer tensile machine commonly used for corrosion investigation of alloys under stress and strain. Corrosion tests were performed on unstrained and strained conditions up to 4% total strain. This strain limit corresponds to 50% of the total elongation achieved into the superelastic stress plateau of the alloy. All wire specimens were analyzed after testing by scanning electron microscopy (SEM). The results showed that localized corrosion occurred for NiTi wires in solution containing fluoride, while no corrosion attack was detected in NaCl 9 g/l solution. There was no significant difference between the corrosion resistance of unstrained and strained wires. However, brittle like fracture occurred in NaCl + NaF solution within the superelastic domain of the material. The most relevant conclusion achieved is that the use of superelastically strained NiTi in oral environments in the presence of fluoride is followed by significant risk of corrosion induced fracture.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Metal ion release from fixed orthodontic appliances - an in vivo study10.1093/ejo/cjq181 ↗
2. Decrease in the fatigue resistance of nickel-titanium rotary instruments after clinical use in curved root canals10.1016/j.tripleo.2004.10.013 ↗
3. Effect of fluoride agents on surface characteristics of NiTi wires. An ex vivo investigation10.1016/j.jobcr.2020.07.006 ↗
4. Effect of surface treatment of NiTi alloy on its corrosion behavior in Hanks' solution10.1002/jbm.10114 ↗
5. Investigation on the biological effect of fluorine present on the surface of titanium implants. Analysis of the reaction fluoride-titanium oxide
6. Strain induced localized corrosion of NiTi, NiTiCo and NiTiCr alloys in 0.9% NaCl
7. Galvanic corrosion of Ti6Al4V coupled with NiCr as a dental implant alloy in fluoride solutions10.20964/2020.01.07 ↗
8. Pitting corrosion
9. Variation of the superelastic properties and nickel release from original and reused NiTi orthodontic archwires10.1016/j.jmbbm.2011.11.005 ↗
10. Effect of fluoride and albumin concentration on the corrosion behavior of Ti–6Al–4V alloy10.1016/S0142-9612(02)00315-0 ↗
11. Cytotoxicity of orthodontic wire corroded in fluoride solution in vitro10.2319/0003-3219(2007)077[0349:COOWCI]2.0.CO;2 ↗
12. Assessment of nickel titanium and beta titanium corrosion resistance behavior in fluoride and chloride environments10.2319/091712-740.1 ↗
13. Effect of ternary element addition on the corrosion behaviour of NiTi shape memory alloys10.1002/maco.201206587 ↗
14. Effect of compressive straining on corrosion resistance of a shape memory Ni‐Ti alloy in ringer's solution10.1002/(SICI)1097-4636(199612)32:4<583::AID-JBM11>3.0.CO;2-F ↗
15. Effect of fluoride concentration and pH on corrosion behavior of titanium for dental use10.1177/00220345990780091201 ↗
16. Rotary NiTi instrument fracture and its consequences10.1016/j.joen.2006.06.008 ↗
17. Electrolytic processing of NiTi shape memory alloys10.1016/j.msea.2003.11.080 ↗
18. Environmental fatigue of superelastic NiTi wire with two surface finishes10.1016/j.jmbbm.2020.104028 ↗
19. Thermo-mechanical characterization of NiTi orthodontic archwires with graded actuating forces10.1016/j.jmbbm.2020.103747 ↗
20. Evaluation by electrochemical tests of the passive film stability of equiatomic Ni‐Ti alloy also in presence of stress‐induced martensite10.1002/(SICI)1097-4636(200007)51:1<47::AID-JBM7>3.0.CO;2-P ↗
21. Influence of stress and phase on corrosion of a superelastic nickel-titanium orthodontic wire10.1016/j.ajodo.2007.04.042 ↗
22. Biocompatibility and biostability of metallic endovascular implants: state of the art and perspectives10.1177/152660280301000419 ↗
23. Effect of fluoride prophylactic agents on the mechanical properties of nickel-titanium-based orthodontic wires10.1016/j.ajodo.2005.01.015 ↗
24. Stress corrosion cracking of NiTi in artificial saliva10.1016/j.dental.2006.01.001 ↗
25. Degradation and fracture of Ni–Ti superelastic wire in an oral cavity10.1016/S0142-9612(00)00414-2 ↗
26. Symptoms of titanium and nickel allergic sensitization in orthodontic treatment10.1186/s40510-020-00318-4 ↗
27. Why do nickel-titanium archwires fracture intraorally? Fractographic analysis and failure mechanism of in-vivo fractured wires10.1016/j.ajodo.2005.11.039 ↗