journal article·2020-09

Grinding the intaglio surface of yttria partially- and fully-stabilized zirconia polycrystals restorations: Effect on their fatigue behavior

Camila Pauleski Zucuni, Bruna Dias Ilha, Michele Mirian May, Liliana Gressler May, Luiz Felipe Valandro

Publisher page

Abstract

This study evaluated the effects of diamond bur grinding the intaglio surface of second (yttria partially-stabilized zirconia polycrystals, PSZ) and third-generation zirconia (fully-stabilized zirconia polycrystals, FSZ) adhesively cemented to dentin analogue substrate on the fatigue failure load, cycle number until failure, surface micromorphology and phase transformation. Disc-shaped specimens were produced from second (Katana ML-HT, Kuraray) and third-generation zirconia (Katana STML, Kuraray) and randomly allocated (n = 15) into two groups according to the intaglio surface treatment: Control - Ctrl (without grinding); Grinding - Gr (grinding at the center of the intaglio surface). The ceramic discs were adhesively cemented (Multilink Automix System) onto dentin analogue discs. Fatigue tests were executed by the step-stress method. The obtained data were analyzed by Kaplan Meier and Mantel-Cox tests. In addition, surface topography, roughness, phase transformation and fractography analyses were performed. SEM analysis showed that grinding increased the surface roughness and introduced defects in zirconia from both generations. Grinding increased the fatigue failure load, number of cycles to failure and survival rates of the second-generation zirconia statistically (control: 1373.33 N < grinding: 1600 N), while these same outcomes were reduced by grinding for the third-generation zirconia significantly (control: 766.67 N > grinding: 620 N). Thus, clinical adjustments with diamond burs damage the fatigue behavior of adhesively cemented third-generation zirconia.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
2. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
3. Air-abrasion using new silica-alumina powders containing different silica concentrations: effect on the microstructural characteristics and fatigue behavior of a Y-TZP ceramic10.1016/j.jmbbm.2019.05.032 ↗
4. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
5. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
6. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
7. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
8. Loading frequencies up to 20 Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
9. Surface micro-morphology, phase transformation, and mechanical reliability of ground and aged monolithic zirconia ceramic10.1016/j.jmbbm.2016.10.008 ↗
10. Transformation toughening in zirconia containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
11. Geometrical product specifications (GPS)–surface texture: profile method, terms definitions and surface texture parameters
12. Fracture surface analysis of dental ceramics; clinically failed restorations
13. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
14. New multi-layered zirconias: composition, microstructure and translucency10.1016/j.dental.2019.02.017 ↗
15. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
16. Zirconia-based versus metal-based single crowns veneered with over pressing ceramic for restoration of posterior endodontically treated teeth: 5-year results of a randomized controlled clinical study10.1016/j.jdent.2017.07.004 ↗
17. Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: effect of ceramic thickness10.1016/j.dental.2018.03.004 ↗
18. Fatigue strength of several dental ceramics indicated for CAD-CAM monolithic restorations10.1590/1807-3107bor-2018.vol32.0053 ↗
19. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading
20. Effect of grinding with diamond-disc and-bur on the mechanical behavior of a Y-TZP ceramic10.1016/j.jmbbm.2014.05.010 ↗
21. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review10.1016/j.jmbbm.2016.06.028 ↗
22. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
23. Lithium disilicate glass-ceramic vs translucent zirconia polycrystals bonded to distinct substrates: fatigue failure load, number of cycles for failure, survival rates, and stress distribution10.1016/j.jmbbm.2018.12.010 ↗
24. Zirconia as a ceramic biomaterial, a review10.1016/S0142-9612(98)00010-6 ↗
25. Hydrofluoric acid concentrations: effect on the cyclic load to failure of machined lithium disilicate restorations10.1016/j.dental.2018.06.028 ↗
26. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
27. Dental ceramics: an update10.4103/0972-0707.73379 ↗
28. Effect of grinding and multi-stimuli aging on the fatigue strength of a Y-TZP Ceramic10.1590/0103-6440201801735 ↗
29. Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
30. Three generations of zirconia: from veneered to monolithic. Part I
31. Effect of different treatments on the flexural strength of fully versus partially stabilized monolithic zirconia10.1016/j.prosdent.2016.10.031 ↗
32. Surface and intra-pulpal temperature rises during tooth bleaching: an in vitro study10.1038/sj.bdj.4812558 ↗
33. Characterization of three commercial Y-TZP ceramics produced for their high-translucency, high-strength and high-surface area10.1016/j.ceramint.2015.09.033 ↗
34. The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic10.1016/j.prosdent.2004.12.002 ↗
35. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
36. Fracture-resistant monolithic dental crowns10.1016/j.dental.2015.12.010 ↗
37. Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations10.1016/j.jmbbm.2018.11.009 ↗