journal article·2021-12

Toughening by revitrification of Li2SiO3 crystals in Obsidian® dental glass-ceramic

Julia Lubauer, Katrin Hurle, Maria Rita Cicconi, Anselm Petschelt, Herwig Peterlik, Ulrich Lohbauer, Renan Belli

Publisher page

Abstract

As a predominantly lithium-metasilicate-containing glass-ceramic, Obsidian® (Glidewell Laboratories, USA) has a peculiar composition and microstructure among other dental lithium silicates, warranting an evaluation of the crystallization process to establish relationships between microstructural evolution and mechanical properties. Blocks of the pre-crystallized material were processed into slices measuring 12 × 12 × 1.5 mm3 and subjected to the mandatory crystallization firing by interruption the heating ramp at temperatures between 700 °C and 820 °C (dwell time between 0 min and 10 min). The crystallization peaks of the base and the pre-crystallized glass were obtained by differential scanning calorimetry (DSC). The coefficient of thermal expansion and the glass transition temperature were derived from differential thermal analysis (DTA). X-ray diffraction (XRD) was performed to quantify and characterize the crystal phase fraction, whose microstructural changes were visualised using FE-SEM. The ball-on-three-balls surface crack in flexure method was used to track the evolution of fracture toughness. The microstructural evolution during crystallization firing was characterized by two regimes of growth: (i) the progressive revitrification (dissolution) of the 5 μm-sized Li2SiO3 polycrystals manifested at the boundaries of nanometric single coherent scattering domains (CSDs); (ii) the non-isothermal period is marked by an Ostwald ripening process characterized by the growth of the single crystalline structures into 0.5 μm polycrystals. The decrease in the crystal fraction of Li2SiO3 crystals from 41 vol.% to 37 vol.% is accompanied by the formation of a small amount of Li3PO4 (6 vol.%), maintaining the total crystal phase fraction mostly constant. The KIc accompanied the reverse trend of crystallinity, departing from 1.63 ± 0.02 MPa√m at the pre-crystallized stage to 1.84 ± 0.06 MPa√m after 10 min at 820 °C in a linear trend. Toughening appeared counter-intuitive in view of the decreasing crystal fraction and size, to rather relate to the relaxation of the residual stresses in the interstitial glass due to the spheroidization of the initially anisotropic, elongated Li2SiO3 crystals into round, nearly equiaxed particles, as let suggest from the disappearance of the extensive microcracking.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear materials and radiation effects · Advanced ceramic materials synthesis · X-ray Diffraction in Crystallography

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. 2010
2. Fracture anisotropy in texturized lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2017.11.040 ↗
3. Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs10.1016/j.jeurceramsoc.2018.08.012 ↗
4. Practical and theoretical considerations on the fracture toughness testing of dental restorative materials10.1016/j.dental.2017.11.016 ↗
5. Crack-healing during two-stage crystallization of biomedical lithium (di)silicate glass-ceramics10.1016/j.dental.2019.05.013 ↗
6. Phase evolution in lithium disilicate glass-ceramics based on non-stoichiometric compositions of a multi-component system: structural studies by 29Si single and double resonance solid state NMR10.1039/c0cp01440k ↗
7. Castillo · 2011
8. Correlation between fracture toughness and leucite content in dental porcelains10.1016/j.jdent.2005.02.001 ↗
9. Biaxial tensile strength test for brittle rectangular plates10.2109/jcersj.114.1054 ↗
10. Ectors · 2016
11. A generalized geometric approach to anisotropic peak broadening due to domain morphology10.1107/S1600576714026557 ↗
12. Routine (an)isotropic crystallite size analysis in the double-Voigt approximation done right?
13. A micromechanical basis for partitioning the evolution of grain bridging in brittle materials10.1016/j.jmps.2006.10.009 ↗
14. The roles of P2O5 and SiO2/Li2O ratio on the network structure and crystallization kinetics of non-stoichiometric lithium disilicate based glasses10.1016/j.jnoncrysol.2017.11.034 ↗
15. The ball on three ball test: strength testing of specimens of different sizes and geometries
16. Refinement of the crystal structure of lithium polysilicate10.1107/S0567740877004932 ↗
17. Heat transport properties of cristobalite and discussion of „snowflake“ formation10.3749/canmin.51.5.705 ↗
18. Höland · 2012 · 86
19. Mechanisms of nucleation and controlled crystallization of needle-like apatite in glass-ceramics of the SiO2-Al2O3-K2O-CaO-P2O5 system10.1016/S0022-3093(99)00351-8 ↗
20. Studies of crystal phase formations in high-strength lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2006.06.039 ↗
21. Residual thermal stresses in ceramic composites. Part I: with ellipsoidal inclusions10.1016/0921-5093(96)10176-3 ↗
22. Nucleation and crystallization kinetics of a multicomponent lithium disilicate glass by in situ and real-time synchrotron X-ray diffraction10.1021/cg400835n ↗
23. Phase characterization of lithium silicate biomedical glass-ceramics produced by two-stage crystallization10.1016/j.jnoncrysol.2019.01.027 ↗
24. International Union for Crystallography · 2004
25. Does Ordinary Portland Cement contain amorphous phase? A quantitative study using an external standard method10.1154/1.3549186 ↗
26. The early hydration of Ordinary Portland Cement (OPC): an approach comparing measured heat flow with calculated heat flow from QXRD10.1016/j.cemconres.2011.09.001 ↗
27. Glidewell Laboratories, Obsidian All-ceramic. Available from: https://glidewelldental.com/solutions/crown-and-bridge/glass-ceramics/obsidian-all-ceramic.
28. Effects of crystal size on the mechanical properties of a lithium disilicate glass-ceramic10.1016/j.msea.2016.05.068 ↗
29. Concurrent kinetics of crystallization and toughening in multicomponent biomedical SiO2-Li2O-P2O5-ZrO2 glass-ceramics10.1016/j.jnoncrysol.2020.120607 ↗
30. A fracture toughness test using the ball-on-three-balls test10.1111/jace.13842 ↗
31. The origin of color in "fire" obsidian10.2113/gscanmin.45.3.551 ↗
32. Much more than a glass: the complex magnetic and microstructural properties of Obsidian10.1021/acs.jpcc.6b08387 ↗
33. Anisotropic residual stresses in partially crystallized Li2O-2SiO2 glass-ceramics10.1016/S0022-3093(99)00038-1 ↗
34. The secret lives of minerals
35. Obsidian: a restorative solution inspired by stone-age technology
36. Effect of heat treatment on fracture toughness (KIc) and microstructure of a fluorcanasite-based glass-ceramic10.1111/j.1532-849X.2007.00233.x ↗
37. An in situ and ex situ study of the microstructural evolution of a novel lithium silicate glass-ceramic during crystallization firing10.1016/j.dental.2020.03.011 ↗
38. Surface and bulk residual stresses in Li2O center dot 2SiO2 glass-ceramics10.1016/j.jnoncrysol.2007.04.007 ↗
39. Effect of lateral cracks on fracture toughness determined by the surface-crack-in-flexure method10.1111/j.1151-2916.2002.tb00186.x ↗
40. Influence of microstructure and chemistry on the fracture toughness of dental ceramics10.1016/S0109-5641(03)00002-2 ↗
41. Fracture characteristics of SiC particle reinforced oxynitride glass using chevron-notch three-point bend specimens10.1023/A:1007474415485 ↗
42. Microstructure and mechanical properties of nucleant-free Li2O-CaO-SiO2 glass-ceramics10.1016/j.actamat.2017.03.010 ↗
43. Internal stresses in ceramics10.1111/j.1151-2916.1961.tb15475.x ↗
44. Internal residual stresses in sintered and commercial low expansion Li2O-Al2O3-SiO2 glass-ceramics10.1111/j.1551-2916.2010.04220.x ↗
45. Internal residual stresses in partially crystallized photo-thermo-refractive glass10.1111/j.1551-2916.2010.04372.x ↗
46. Crystallization toughening of a model glass-ceramic10.1016/j.actamat.2014.12.007 ↗
47. Mechanical properties of lithium metasilicate after short-term thermal treatments10.1016/j.jmbbm.2019.06.011 ↗
48. TEM and XRD study of early crystallization of lithium disilicate glasses10.1016/j.jnoncrysol.2003.08.075 ↗
49. Surface crack in tension or in bending – a reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials10.1016/j.jeurceramsoc.2012.01.011 ↗
50. Fracture toughness testing of small ceramic discs and plates10.1016/j.jeurceramsoc.2013.12.021 ↗
51. Surface crack in tension or in bending - a reassessment of the Newman and Raju formula in respect to fracture toughness measurements in brittle materials (vol 32, pg 1491, 2012)10.1016/j.jeurceramsoc.2017.05.008 ↗
52. Toughening of a particulate-reinforced ceramic-matrix composite by thermal residual-stress10.1111/j.1151-2916.1990.tb05209.x ↗
53. Residual stress effect on the fracture toughness of lithium disilicate glass-ceramics10.1111/jace.16664 ↗
54. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
55. Fracture toughness of dental porcelains evaluated by IF, SCF, and SEPB methods10.1111/j.1551-2916.2005.00334.x ↗
56. Die Kristallstruktur von Lithiumphosphat, Li3PO410.1107/S0365110X60002132 ↗