journal article·2019-10

Air-abrasion using new silica-alumina powders containing different silica concentrations: Effect on the microstructural characteristics and fatigue behavior of a Y-TZP ceramic

Ana Carolina Cadore-Rodrigues, Catina Prochnow, Marília Pivetta Rippe, Jivago Schumacher de Oliveira, Sérgio Luiz Jahn, Edson Luiz Foletto, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro

Publisher page

Abstract

This study assessed the fatigue performance (biaxial flexure fatigue strength), surface characteristics (topography and roughness) and structural stability (t-m phase transformation) of a Y-TZP ceramic subjected to air-abrasion using new powders (7% and 20% silica-coated aluminum oxide particles) in comparison to commercially available powders. Disc-shaped specimens were manufactured (ISO 6872-2015) and randomly allocated into four groups considering the air-abrasion materials: SiC: commercially available silica-coated aluminum oxide; AlOx: commercially available aluminum oxide; 7%Si and 20%Si: experimentally produced materials consisting of 7% and 20% silica-coated AlOx, respectively. Air-abrasion was executed by a blinded researcher (1 cm distance from the tip to the specimen surface, under 2.8 bar pressure for 10 s). The fatigue tests (n = 15) were performed by the staircase method under a piston-on-three-balls assembly. Topography and roughness assessments (n = 30) of abraded samples and fractography of failed discs were performed. The highest fatigue strength (MPa) was observed for 7%Si (887.20 ± 50.54) and SiC (878.16 ± 29.81), while the lowest fatigue strength for 20%Si (773.89 ± 46.44) and AlOx (796.70 ± 46.48). Topography analysis depicted similar surface morphology for all conditions. However, roughness (μm) was only statistically different between 7%Si (Ra = 0.30 ± 0.09; Rz = 2.31 ± 0.63) and SiC (Ra = 0.26 ± 0.04; Rz = 1.99 ± 0.34). Monoclinic phase grains appeared on Y-TZP surface in a similar content (≈11-12%) for the protocols. Fractography showed all failures starting on air-abraded surface/sub-surface defects from the tensile side. In terms of roughness, phase transformation and fatigue, the new 7% silica-coated aluminum oxide presented similar behavior to the commercially available powder. Increasing silica-coating concentration to 20% did not lead to a gentle air-abrasion protocol.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Orthopaedic implants and arthroplasty · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Innovations in bonding to zirconia-based materials: Part I10.1016/j.dental.2008.02.010 ↗
2. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
3. Fatigue behavior of Y-TZP ceramic after surface treatments10.1016/j.jmbbm.2015.11.042 ↗
4. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
5. Phase transformation and subsurface damage in 3Y-TZP10.1016/j.dental.2013.03.005 ↗
6. Collins · 1993
7. The influence of surface modification techniques on the performance of a Y-TZP dental ceramic10.1016/j.jdent.2005.06.006 ↗
8. Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic10.1016/j.dental.2008.05.012 ↗
9. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
10. Loading frequencies up to 20 Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
11. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
12. Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic10.1016/j.dental.2004.07.010 ↗
13. Effect of blasting pressure, abrasive particle size and grade on phase transformation and morphological change of dental zirconia surface10.1016/j.surfcoat.2012.04.043 ↗
14. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
15. International Organization for Standardization · 1997
16. International Organization for Standardization · 2015
17. Perspectives on strength10.1016/0109-5641(95)80043-3 ↗
18. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
19. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
20. Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement10.1016/j.ceramint.2015.09.104 ↗
21. Efeito do jateamento de partículas na resistência de união e comportamento mecânico de cerâmicas à base de zircônia -Revisão (Effect of particle sandblasting on the bond strength and mechanical behavior of zirconia-based ceramics -Review)10.1590/S0366-69132014000200003 ↗
22. Adhesion to zirconia used for dental restorations: a systematic review and meta-analysis
23. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
24. A brief history and current status of metal-and ceramic surface-conditioning concepts for resin bonding in dentistry
25. Effect of particle deposition parameters on silica coating of zirconia using a chairside air-abrasion device
26. Low-temperature degradation of Y-TZP ceramics: a systematic review and meta-analysis10.1016/j.jmbbm.2015.10.017 ↗
27. Zirconia as a ceramic biomaterial, A Review10.1016/S0142-9612(98)00010-6 ↗
28. NIST recommended practice guide: fractography of ceramics and glasses
29. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment10.4012/dmj.27.408 ↗
30. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles10.1016/j.dental.2010.10.003 ↗
31. Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
32. Three generations of zirconia: from veneered to monolithic. Part I
33. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
34. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
35. Effects of alumina-blasting and adhesive primers on bonding between resin luting agent and zirconia ceramics10.4012/dmj.25.669 ↗
36. Effects of two grading techniques of zirconia material on the fatigue limit of full-contour 3-unit fixed dental prostheses10.1016/j.dental.2016.12.010 ↗
37. Silica coating on ultrafine α-alumina particles10.1016/j.msea.2004.12.007 ↗
38. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗
39. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
40. Damage accumulation and fatigue life of particle-abraded ceramics