journal article·2023-03

Ceramic surface conditioning, resin cement viscosity, and aging relationships affect the load-bearing capacity under fatigue of bonded glass-ceramics

Kiara Serafini Dapieve, Helder Callegaro Velho, Lucas Saldanha da Rosa, Jordana Pavanelo Pivetta, Fernanda Cocco Maidana, Andressa Borin Venturini, Cornelis Johannes Kleverlaan, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro

Publisher page

Abstract

This study aimed to evaluate the influence of ceramic surface treatments, resin cement viscosities, and storage regimens on the fatigue performance of bonded glass-ceramics (lithium disilicate, LD; feldspathic, FEL). Ceramic discs (Ø = 10 mm; thickness = 1.5 mm) were allocated into eight groups per ceramic (n = 15), considering three factors: "ceramic surface treatment" in two levels - 5% hydrofluoric acid etching and silane-based coupling agent application (HF), or self-etching ceramic primer (E&P); "resin cement viscosity" in two levels - in high or low viscosity; and "storage regimen" in two levels - baseline, 24 h to 5 days; or aging, 180 days + 25,000 thermal cycles. Adhesive luting was performed onto glass fiber-reinforced epoxy resin discs (Ø = 10 mm; thickness = 2 mm) and the bonded assemblies were subjected to cyclic fatigue tests: initial load = 200 N; step-size = 25 N (FEL) and 50 N (LD); 10,000 cycles/step; 20 Hz. Scanning electron microscopy (SEM) inspections were performed. Regarding the LD ceramic, the fatigue behavior was reduced after aging for HF_HIGH and E&P_LOW conditions, while stable performance was observed for HF_LOW and E&P_HIGH. Regarding the FEL results, aging negatively affected HF_HIGH, E&P_HIGH, and E&P_LOW, being that only the HF_LOW condition presented a stable behavior. The failure initiated from defects on the etched surface of the ceramics, where the cross-sectional analysis commonly revealed unfilled areas. Long-term aging might induce a decrease in mechanical behavior. The 'ceramic microstructure/surface conditioning/resin cement viscosity relationships' modulate the fatigue performance of lithium disilicate and feldspathic glass-ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach10.1016/j.dental.2016.11.015 ↗
2. Fatigue failure and success rate of lithium disilicate table-tops as a function of cement thickness10.2186/jpr.JPR_D_20_00220 ↗
3. Influence of inorganic filler content of resin luting agents and use of adhesive on the performance of bonded ceramic10.1016/j.prosdent.2019.09.013 ↗
4. Effect of finishing and polishing on the surface roughness and gloss of feldspathic ceramic for chairside CAD/CAM systems10.2341/15-174-L ↗
5. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
6. Does adhesive luting promote improved fatigue performance of lithium disilicate simplified crowns?10.1016/j.jmbbm.2022.105373 ↗
7. Weak adhesion between ceramic and resin cement impairs the load-bearing capacity under fatigue of lithium disilicate glass-ceramic crowns
8. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
9. Do resin cement viscosity and ceramic surface etching influence the fatigue performance of bonded lithium disilicate glass-ceramic crowns?10.1016/j.dental.2021.12.015 ↗
10. Silane reactivity and resin bond strength to lithium disilicate ceramic surfaces10.1016/j.dental.2019.05.002 ↗
11. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
12. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
13. Influence of the resin cement thickness on the fatigue failure loads of CAD/CAM feldspathic crowns10.1016/j.dental.2015.04.019 ↗
14. Recent advances in materials for all-ceramic restorations10.1016/j.cden.2007.04.006 ↗
15. Effect of microstructure on the mechanical properties of lithium disilicate glass-ceramics10.1016/j.jmbbm.2018.02.032 ↗
16. Ceramic materials in dentistry: historical evolution and current practice10.1111/j.1834-7819.2010.01299.x ↗
17. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
18. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
19. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
20. Effects of thermal and mechanical cycling on the mechanical strength and surface properties of dental CAD-CAM restorative materials
21. Reduction of load-bearing capacity of all-ceramic crowns due to cement aging10.1016/j.jmbbm.2012.08.003 ↗
22. Cements and adhesives for all-ceramic restorations10.1016/j.cden.2011.01.011 ↗
23. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
24. Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: a systematic review and meta-analysis
25. Survival and complications of monolithic ceramic for tooth-supported fixed dental prostheses: a systematic review and meta-analysis10.1016/j.prosdent.2021.01.020 ↗
26. Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: Effect of etching time and hydrofluoric acid concentration10.1016/j.jmbbm.2017.09.028 ↗
27. Measurement of masticatory forces and implant loads: a methodologic clinical study
28. Two-Year follow-up of self-etching ceramic primer as surface treatment for feldspathic veneers: a clinical case review10.2341/20-036-T ↗
29. Surface/interface morphology and bond strength to glass ceramic etched for different periods10.2341/09-152-L ↗
30. Influence of accelerated ageing on the physical properties of CAD/CAM restorative materials10.1007/s00784-019-03101-w ↗
31. In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: effect on the fatigue behavior of the bonded ceramic10.1016/j.jmbbm.2021.104604 ↗
32. Ceramic surface treatment with a single-component primer: resin adhesion to glass ceramics
33. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
34. Adhesion to a lithium disilicate glass ceramic etched with hydrofluoric acid at distinct concentrations10.1590/0103-6440201802080 ↗
35. Hydrofluoric acid concentrations: Effect on the cyclic load-to-failure of machined lithium disilicate restorations10.1016/j.dental.2018.06.028 ↗
36. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
37. Fracture resistance of lithium disilicate ceramics bonded to enamel or dentin using different resin cement types and film thicknesses10.1111/jopr.12372 ↗
38. Effects of surface treatments on the bond strength between resin cement and a new zirconia-reinforced lithium silicate ceramic10.2341/14-357-L ↗
39. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
40. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
41. Effect of water storage time and composite cement thickness on fatigue of a glass-ceramic trilayer system10.1002/jbm.b.30851 ↗
42. Evaluation of five CAD/CAM materials by microstructural characterization and mechanical tests: a comparative in vitro study10.1186/s12903-017-0458-2 ↗
43. Two-year follow-up of ceramic veneers and a Full crown treated with self-etching ceramic primer: a case report10.2341/19-090-R ↗
44. Ceramic strengthening by tuning the elastic moduli of resin-based luting agents10.1016/j.dental.2017.01.002 ↗
45. Strengthening of porcelain provided by resin cements and flowable composites10.2341/15-025-L ↗
46. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
47. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
48. Influence of ceramic material, thickness of restoration and cement layer on stress distribution of occlusal veneers10.1590/1807-3107bor-2018.vol32.0118 ↗
49. Effect of cement layer thickness on the immediate and long-term bond strength and residual stress between lithium disilicate glass-ceramic and human dentin10.3390/ma14185153 ↗
50. Elastic properties of lithium disilicate versus feldspathic inlays: effect on the bonding by 3D finite element analysis10.1111/jopr.12550 ↗
51. A brief review on fatigue test of ceramic and some related matters in Dentistry10.1016/j.jmbbm.2022.105607 ↗
52. Editorial: the VALUE and remaining NEED of bond-strength testing
53. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
54. Cyclic fatigue tests on non-anatomic specimens of dental ceramic materials: a scoping review10.1016/j.jmbbm.2021.104985 ↗
55. Fatigue performance of adhesively cemented glass-, hybrid- and resin-ceramic materials for CAD/CAM monolithic restorations10.1016/j.dental.2019.01.013 ↗
56. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
57. Effect of hydrofluoric acid concentration on resin adhesion to a feldspathic ceramic
58. Effect of resin cement space on the fatigue behavior of bonded CAD/CAM leucite ceramic crowns10.1016/j.jmbbm.2020.103893 ↗
59. Dental ceramics for restoration and metal veneering10.1016/j.cden.2017.06.005 ↗