The aim was to quantify effects of polylysine (PLS, 2 or 5wt%) and monocalcium phosphate (MCP, 4 or 8wt%) on properties of dental composites. Light-activated, lower surface polymerisation kinetics versus sample depth (1–4 mm) of 4 formulations were quantified using ATR-FTIR. Water sorption and solubility (at 1 week) were assessed following ISO/4049. PLS release (over 1 month) and biaxial flexural strength (over 6 months) of fully-cured, water-immersed, 1 mm thick discs were determined. Surface mineral precipitation, following immersion in simulated body fluid (SBF), was assessed by SEM. Z250 was used as a conventional composite comparator. With 40s light exposure, increasing depth (from 1-4mm) led to enhanced delay before polymerisation (from 3-17s) and decreased final conversion (72-66%) irrespective of PLS and MCP level. Increasing PLS and MCP raised solubility (4–13 μg/mm3). Water sorption (between 32-55 μg/mm3) and final PLS release (8–13% of disc content) were raised primarily by increasing PLS. Higher PLS also reduced strength. Strength reached minimum values (69–94 MPa) at 3 months. Surface mineral deposition was enhanced by increased MCP. For Z250, polymerisation delays (3-6s) and final conversions (55-54%) at 1-4mm depth, solubility (0 μg/mm3), water sorption (16 μg/mm3) and strength (180 MPa) were all significantly different. Delay time increased whilst final conversion decreased with thicker samples. Higher PLS enhances its percentage release, but lower level is required to keep water sorption, solubility and mechanical properties within ISO 4049 recommendations. Doubling MCP raises solubility and enhances minerals reprecipitation with minimal mechanical property compromise.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Conversion, shrinkage, water sorption, flexural strength and modulus of re-mineralizing dental composites10.1016/j.dental.2015.08.149 ↗
2. Alkhouri · 2020
3. Renewal MI dental composite etch and seal properties10.3390/ma15155438 ↗
4. 2009
5. Restorations in primary teeth: a systematic review on survival and reasons for failures10.1111/ipd.12346 ↗
6. Flexural strength of dental composite restoratives: comparison of biaxial and three-point bending test10.1002/jbm.b.30103 ↗
7. Methacrylate peak determination and selection recommendations using ATR-FTIR to investigate polymerisation of dental methacrylate mixtures10.1371/journal.pone.0252999 ↗
8. Varying 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP) level improves polymerisation kinetics and flexural strength in self-adhesive, remineralising composites10.1016/j.dental.2021.06.006 ↗
9. England · 2018
10. 2014 · 295
11. In vitro and in vivo studies on the toxicity of dental resin components: a review10.1007/s00784-007-0162-8 ↗
12. Clinical efficacy of resin-based direct posterior restorations and glass-ionomer restorations - an updated meta-analysis of clinical outcome parameters. Dental materials10.1016/j.dental.2021.10.018 ↗
13. Evaluating acrylic and glass-ionomer cement strength using the biaxial flexure test10.1016/S0142-9612(00)00324-0 ↗
14. Implants · 2014
15. Monomer conversion, dimensional stability, strength, modulus, surface apatite precipitation and wear of novel, reactive calcium phosphate and polylysine-containing dental composites10.1371/journal.pone.0187757 ↗
16. The survival of class V composite restorations and analysis of marginal discoloration10.2341/16-186-C ↗
17. Early polylysine release from dental composites and its effects on planktonic Streptococcus mutans growth10.3390/jfb11030053 ↗
18. High strength re-mineralizing, antibacterial dental composites with reactive calcium phosphates10.1016/j.dental.2013.01.010 ↗
19. Water sorption and solubility of bulk-fill composites polymerized with a third generation LED LCU10.1590/1807-3107bor-2017.vol31.0080 ↗
20. Evaluation of ISO 4049: water sorption and water solubility of resin cements10.1111/eos.12339 ↗
21. Son · How light attenuation and filler content affect the microhardness and polymerization shrinkage and translucency of bulk-fill composites? · 2017 · 21 · 559
22. Mechanical properties of contemporary composite resins and their interrelations10.1016/j.dental.2013.04.025 ↗
23. Poly(propylene glycol) and urethane dimethacrylates improve conversion of dental composites and reveal complexity of cytocompatibility testing10.1016/j.dental.2015.11.017 ↗
24. Effect of novel antibacterial composites on bacterial biofilms10.3390/jfb11030055 ↗
25. Statistical methods and common problems in medical or biomedical science research
26. FTIR investigation of monomer polymerisation and polyacid neutralisation kinetics and mechanisms in various aesthetic dental restorative materials10.1016/S0142-9612(03)00599-4 ↗