Mechanical properties of cracked teeth with different dental materials and crown parameters: An in vitro proof-of-concept

Jianpeng Sun, Jingang Jiang, Zhonghao Xue, Hongyuan Ma, Jie Pan, Kun Qian

Publisher page

Abstract

Objective This work analyzed and compared the mechanical properties of identical cracked tooth models treated with different materials and crown parameters. Thus, to provide dentists with a more structured way to select materials and geometric parameters and determine the strongest restoration model for cracked teeth. Methods This work used finite element analysis (FEA). We applied 25 restorative models, including five restorative materials, and three preparation parameters. Seven mechanical properties of the cracked tooth preparation were analyzed using correlation analysis. Results The highest lifetime of the cracked preparation was obtained for crowns with a 5° of polymerization, width = 0.8 mm, and a length offset of 0.2 mm. The highest lifetime was obtained with ZC crown material, but the least deformation of the cracked tip was obtained with LU material. Significance The results showed that the larger MOE material for the crown and a reasonable increase in the thickness and length of the crown is a favorable method to prevent further cracks to extend. This FEA study, thereby forming a novel basis for clinical guidance as to preparation of dental crowns applicable to cracked teeth.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Mechanical behavior of endodontic ally restored canine teeth: effects of ferrule, post material and shape10.1016/j.dental.2017.10.009 ↗
2. Fatigue resistance of 2 different CAD/CAM glass-ceramic materials used for single-tooth implant crowns10.1097/ID.0b013e3182310e61 ↗
3. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
4. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
5. Influence of endodontic treatment, post insertion, and ceramic restoration on the fracture resistance of maxillary premolars10.1111/j.1365-2591.2010.01701.x ↗
6. Reparative dentistry: possibilities and limitations10.1007/s40496-018-0191-1 ↗
7. Influence of thread shape and inclination on the biomechanical behaviour of plateau implant systems10.1016/j.dental.2018.01.012 ↗
8. The cracked tooth syndrome: additional findings10.14219/jada.archive.1976.0034 ↗
9. Fracture resistance of various thickness e.max CAD lithium disilicate crowns cemented on different supporting substrates: an in vitro study10.1111/jopr.13108 ↗
10. 3D-Finite element analysis of molars restored with endocrowns and posts during masticatory simulation10.1016/j.dental.2013.09.014 ↗
11. Fatigue resistance of CAD/CAM resin composite molar crowns
12. Effect of crown-to-implant ratio and crown height space on marginal bone stress: a finite element analysis10.1186/s40729-021-00368-1 ↗
13. Comparison of metal full crown retention forces with different axial wall aggregation
14. Influence of polymerization of all-ceramic crown preparations on the marginal fit and compressive strength of all-ceramic crowns
15. Adjacent surface trajectory planning of robot-assisted tooth preparation based on augmented reality
16. Stress intensity factor of a cracked molar restored with different materials and designs: a 3D-FEA
17. Effects of abutment length and platform size on the retention of implant-supported CAD/CAM crowns using six different cements10.1016/j.jds.2021.04.013 ↗
18. Wear, strength, modulus and hardness of CAD/CAM restorative materials10.1016/j.dental.2016.08.222 ↗
19. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
20. Fractographic analyses of all-ceramic crowns: a study of 27 clinically fractured crowns10.1016/j.dental.2013.03.018 ↗
21. The effectiveness of bonded composite restorations in the treatment of painful, cracked teeth: six-month clinical evaluation
22. Seven-year clinical evaluation of painful cracked teeth restored with a direct composite restoration10.1016/j.joen.2008.04.011 ↗
23. Influence of implant position on clinical crown length and peri-implant soft tissue dimensions at implant-supported single crowns replacing maxillary central incisors10.11607/prd.1573 ↗
24. CAD-FEA modeling and analysis of different full crown monolithic restorations10.1016/j.dental.2018.06.024 ↗
25. Microleakage of various cementing agents for full cast crowns10.1016/j.dental.2004.07.009 ↗
26. Effect of cement space on stress distribution in Y-TZP based crowns10.1016/j.dental.2016.11.006 ↗
27. Fracture strength of secondary crown with different taper and thickness in zirconia double crown attachments10.4012/dmj.2020-295 ↗
28. Occlusal stress distribution and remaining crack propagation of a cracked tooth treated with different materials and designs: 3D finite element analysis10.1016/j.dental.2021.01.020 ↗
29. Fracture resistance and marginal fit of the zirconia crowns with varied occlusal thickness10.4047/jap.2020.12.5.283 ↗
30. Endocrown restorations: influence of dental remnant and restorative material on stress distribution10.1016/j.dental.2018.06.012 ↗
31. Elastic properties of lithium disilicate versus felds pathicinlays: effect on the bonding by 3D finite element analysis10.1111/jopr.12550 ↗
32. Which dentine analogue material can replace human dentine for crown fatigue test?10.1016/j.dental.2022.11.020 ↗
33. Fracture-resistant monolithic dental crowns10.1016/j.dental.2015.12.010 ↗
34. Effects of design parameters on fracture resistance of glass simulated dental crowns10.1016/j.dental.2015.11.018 ↗
35. In vitro study on the wear behaviour of human tooth enamel in citric acid solution10.1016/j.wear.2010.11.027 ↗