Effects of Cr addition on Ti implant alloys (Ti-Cr/Ti-Al-V-Cr) to enhance corrosion and wear resistance

Maria Herbster, Bernd Garke, Karsten Harnisch, Oliver Michael, Alexandra Lieb, Ulf Betke, Mandy Könnecke, Andreas Heyn, Paulina Kriegel, Henrike Thärichen, Jessica Bertrand, Manja Krüger, Thorsten Halle

Abstract

Due to their excellent biocompatibility, favorable strength-to-weight ratio and mechanical properties, Ti-based alloys are most commonly used for long-term implants in the human body. Nevertheless, low wear resistance and increased degradation due to corrosion under critical in vivo conditions impair the service life of these implants. This fact opens the potential for optimization, which can be exploited by chemical alloying with Cr. This study investigates the effect of Cr alloying on the mechanical, tribological, corrosion properties and cytocompatibility of cp Ti and TiAl6V4 alloys. Argon-arc melting was used to cast binary and quaternary specimens of varying Cr content (0.1, 0.2, 0.4, 1, 2, 4, 8, 10, 15 and 20 m%). After homogenization (1100 °C, 30 min), microstructures were characterized by means of XRD and EBSD and correlated with mechanical properties using hardness and compression tests. At up to 2 m% Cr, a martensitic α′ microstructure is formed. A Cr content of 4 m% reveals two phase α’ + β alloys. Alloying with ≥8 m% Cr results in complete β phase, whereas the significantly reduced fracture compression indicates the formation of metastable ω phase for Cr content of 8–10 m%. Based on XPS analysis, a change in the composition of the passive layers by incorporation of Cr 2 O 3 and CrO x is verified. These modified passive layers result in a reduction in corrosion current densities under mimicked severe inflammatory conditions (PBS with HCl and H 2 O 2 ). In addition, the tribological behavior is significantly improved by a reduced wear rate for binary Ti-2/4Cr and quaternary TiAlV-4/8Cr alloys. Cell viability is not inhibited by Cr alloying, but reduced calcification is observed for all Cr modified specimens. These findings highlight the tremendous potential of Ti alloying with Cr for improved implant properties, with the alloy range of 2–4 m% Cr being the most suitable.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Corrosion behavior of Ti-6Al-4V with different thermomechanical treatments and microstructures10.5006/1.3452400 ↗
2. A review of the metastable omega phase in beta titanium alloys: the phase transformation mechanisms and its effect on mechanical properties10.1080/09506608.2022.2036401 ↗
3. Beta titanium alloys and their role in the titanium industry10.1007/BF03220742 ↗
4. Determinants of corrosion resistance of Ti-6Al-4V alloy dental implants in an in Vitro model of peri-implant inflammation10.1371/journal.pone.0210530 ↗
5. Brunette · 2001
6. Ionic cobalt but not metal particles induces ROS generation in immune cells in vitro10.1002/jbm.b.34217 ↗
7. Higher accuracy analysis of instrumented indentation data obtained with pointed indenters10.1088/0022-3727/41/21/215407 ↗
8. Davis · 1998
9. 2016
10. 2015
11. 2018
12. Behavior of commercially pure titanium and Ti-318 (Ti-6Al-4V) in orthopedic implants
13. Donachie · 2000
14. The effects of cobalt and chromium ions on transforming growth factor-beta patterns and mineralization in human osteoblast-like MG63 and SaOs-2 cells10.1002/jbm.a.36409 ↗
15. Differential effect of cobalt and chromium ions as well as CoCr particles on the expression of osteogenic markers and osteoblast function10.3390/ijms19103034 ↗
16. 2012
17. 2021
18. The martensite transformation in Ti-Cr binary alloys10.1016/0001-6160(69)90114-X ↗
19. The omega phase transformation in titanium alloys as an example of displacement controlled reactions10.1016/0001-6160(71)90047-2 ↗
20. In vivo oxide-induced stress corrosion cracking of Ti-6Al-4V in a neck-stem modular taper: emergent behavior in a new mechanism of in vivo corrosion10.1002/jbm.b.31943 ↗
21. Graft WH, Rostoker W. The measurement of elastic modulus of titanium alloys. In: Staff CB-2, editor. Symposium on Titanium. 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959: ASTM International; 1957, 130-130-15.10.1520/STP44151S ↗
22. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗
23. Corrosion of modular junctions in femoral and acetabular components for hip arthroplasty and its local and systemic effects
24. Metal sensitivity in patients with orthopaedic implants10.2106/00004623-200103000-00017 ↗
25. Deformation behaviour of retained beta phase in beta-eutectoid Ti-Cr alloys10.1007/BF01106518 ↗
26. Characterization of surface film formed on titanium in electrolyte using XPS10.1016/0169-4332(92)90178-Z ↗
27. Repassivation of titanium and surface oxide film regenerated in simulated bioliquid10.1002/(SICI)1097-4636(19980615)40:4<530::AID-JBM3>3.0.CO;2-G ↗
28. Effect of chromium content on mechanical properties of casting Ti-Cr alloys10.4012/dmj.2009-118 ↗
29. Surface modified Ti6Al4V for enhanced bone bonding ability – effects of silver and corrosivity at simulated physiological conditions from a corrosion and metal release perspective10.1016/j.corsci.2020.108566 ↗
30. Microstructure-dependent crevice corrosion damage of implant materials CoCr28Mo6, TiAl6V4 and REX 734 under severe inflammatory conditions10.1002/jbm.b.35030 ↗
31. Microstructural modification of TiAl6V4 alloy to avoid detrimental effects due to selective in vivo crevice corrosion10.3390/ma15165733 ↗
32. In vivo corrosion on retrieved hip endoprostheses and in vitro effects of corrosion products on bone mineralization10.1016/j.bone.2023.116852 ↗
33. Mechanical properties and deformation behavior of cast binary Ti–Cr alloys10.1016/j.jallcom.2008.01.046 ↗
34. Electrochemical behavior of Ti–Cr alloys in artificial saliva10.1016/j.jallcom.2009.07.172 ↗
35. Structure and grindability of dental Ti–Cr alloys10.1016/j.jallcom.2008.09.116 ↗
36. 2014 · 14242
37. 2017 · 65
38. The effect of α phase on the deformation mechanisms of β titanium alloys10.1361/105994905X75565 ↗
39. Localized corrosion: crevice corrosion
40. Evaluation of Ti-Cr-Cu alloys for dental applications10.1361/105994905X75600 ↗
41. A review of metastable beta titanium alloys10.3390/met8070506 ↗
42. Deformation-induced changeable Young's modulus with high strength in β-type Ti-Cr-O alloys for spinal fixture10.1016/j.jmbbm.2013.11.001 ↗
43. Mechanical properties and cytocompatibility of oxygen-modified β-type Ti-Cr alloys for spinal fixation devices10.1016/j.actbio.2014.10.014 ↗
44. Lütjering · 2007
45. Espèces réactives de l'oxygène et stress oxydant10.1051/medsci/2011274017 ↗
46. Passive film on orthopaedic TiAlV alloy formed in physiological solution investigated by X-ray photoelectron spectroscopy10.1016/S0142-9612(00)00145-9 ↗
47. Self-adjustment of Young's modulus in biomedical titanium alloys during orthopaedic operation10.1016/j.matlet.2010.11.006 ↗
48. 2012
49. 2021
50. 2015
51. 2007
52. Discoloration and dissolution of titanium and titanium alloys with immersion in peroxide- or fluoride-containing solutions10.4012/dmj.27.117 ↗
53. 2016
54. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
55. Electrochemical and XPS studies of titanium for biomaterial applications with respect to the effect of hydrogen peroxide10.1002/jbm.820280115 ↗
56. Variation of oxide films on titanium induced by osteoblast-like cell culture and the influence of an H2O2 pretreatment10.1002/(SICI)1097-4636(199805)40:2<244::AID-JBM9>3.0.CO;2-L ↗
57. An electrochemical study of the crevice corrosion of titanium10.1590/S0103-50531997000200009 ↗
58. Cytocompatibility of pure metals and experimental binary titanium alloys for implant materials10.1016/j.jdent.2013.09.003 ↗
59. The cleavage strength of polycrystals
60. Microstructural aspects of Ti6Al4V degradation in H2O2-containing phosphate buffered saline10.1016/j.corsci.2021.109640 ↗
61. In vivo severe corrosion and hydrogen embrittlement of retrieved modular body titanium alloy hip-implants10.1002/jbm.b.31171 ↗
62. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
63. On the stability of passivity of Ti-Al alloys in acidic environment10.1524/zpch.2005.219.11.1447 ↗
64. Fretting corrosion behavior of experimental Ti-20Cr compared to titanium10.3390/ma10020194 ↗
65. On the ω phase formation in Cr–Al and Ti–Al–Cr alloys10.1016/S1359-6454(00)00168-3 ↗
66. Surface characterization of implant materials c.p. Ti, Ti-6Al-7Nb and Ti-6Al-4V with different pretreatments10.1023/A:1008840026907 ↗
67. New insights into the corrosion of orthopedic Ti-6Al-4V under cathodic polarization10.1016/j.corsci.2024.112354 ↗
68. Corrosion mechanism of Ti-Cr alloys in solution containing fluoride10.1016/j.dental.2008.09.005 ↗
69. Corrosion of modular titanium alloy stems in cementless hip replacement10.1520/JAI12810 ↗
70. Direct observations and analyses of dislocation substructures in the α phase of an α/β Ti-alloy formed by nanoindentation10.1016/j.actamat.2005.07.030 ↗
71. A synergistic effect of albumin and H₂O₂ accelerates corrosion of Ti6Al4V10.1016/j.actbio.2015.07.046 ↗
72. Optimization of Cr content of metastable β-type Ti-Cr alloys with changeable Young's modulus for spinal fixation applications10.1016/j.actbio.2012.02.010 ↗
73. New kind of titanium alloys for biomedical application