Fatigue behavior in Co–Cr–Ni–Mo medical wires drawn with different drawing practices
Source abstract
Abstract
35%Co-20%Cr-35%Ni-10%Mo alloy (MP35N) with a low titanium (LT) content is commonly used as the material for the manufacture of leads in medical applications such as Cardiac Rhythmic Management (CRM), neurostimulation and Deep Brain Stimulation (DBS). The material is drawn to thin wires, and this involves subjecting the material to extensive plastic deformation to obtain the desired mechanical and fatigue properties. The critical part in the medical device design requires understanding the relationship between the processing method, microstructure and their impact on the cyclic performance. In this study, the influence of drawing practices namely Full Die Drawing (FDD) and Half Die Drawing (HDD) on the cyclic performance of MP35NLT wires have been investigated, by differing the amount of plastic strain applied on the material. The as-drawn wires were subjected to rotary beam fatigue tests (R = -1) with varying stress amplitudes, and the microstructural factors controlling the Low Cycle Fatigue (LCF) and High Cycle Fatigue (HCF) performance were determined through post fatigued TEM investigations. The results conclude that there is a significant impact on the drawing techniques on the fatigue performance of MP35NLT wires, with the FDD wires having a higher endurance limit than the HDD drawn wire until 75% CW, but there was a slight drop in the fatigue performance when the CW was increased to 95%. This was attributed to the difference in grain sizes, dislocation structures, twin density, twin spacing, and grain boundary orientations observed between the two wires which contributed to contrasting cyclic behavior. The drop-in fatigue performance of the FDD wire upon an increased strain to 95% has been attributed to the shear band formations in the material, which increased the stress localization in the material bestowing to drop-in fatigue performance.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. ASTM E2948-16a Standard Test Method for Conducting Rotating Bending Fatigue Tests of Solid Round Fine Wire.
2. Cyclic softening of ultrafine grain copper10.1016/S0921-5093(97)00689-8 ↗
3. Role of nanotwins on fatigue crack growth resistance–experiments and theory10.1016/j.ijfatigue.2015.11.012 ↗
4. Rotary bending fatigue of coils and wires used in cardiac lead design10.1002/(SICI)1097-4636(199821)43:1<21::AID-JBM3>3.0.CO;2-O ↗
5. Bradley · 2003
6. Dislocation plasticity in persistent slip bands10.1016/S0921-5093(00)00662-6 ↗
7. Persistent slip bands in cyclically deformed nickel polycrystals110.1016/S0142-1123(01)00013-5 ↗
8. Roles of microstructure in fatigue crack initiation10.1016/j.ijfatigue.2009.10.005 ↗
9. Predicting fatigue resistance of nano-twinned materials: Part I–Role of cyclic slip irreversibility and Peierls stress10.1016/j.ijfatigue.2014.05.014 ↗
10. Deformation twinning10.1016/0079-6425(94)00007-7 ↗
11. Clark · 2016
12. A review of deformation and fatigue of metals at small size scales10.1111/j.1460-2695.2005.00951.x ↗
13. Fatigue behaviour of light alloys with ultrafine grain structure produced by severe plastic deformation: an overview10.1016/j.ijfatigue.2009.06.022 ↗
14. Cyclic stress-strain response of FCC metals and alloys—II Dislocation structures and mechanisms10.1016/0001-6160(67)90138-1 ↗
15. Fatigue testing of thin CoNiCr wire up to 1010 cycles10.1016/j.ijfatigue.2017.01.027 ↗
16. Fatigue and fracture of wires and cables for biomedical applications10.1080/09506608.2016.1152347 ↗
17. Applications of the FIB lift‐out technique for TEM specimen preparation10.1002/(SICI)1097-0029(19980515)41:4<285::AID-JEMT1>3.0.CO;2-Q ↗
18. Giannuzzi · 2005 · 201
19. A review of focused ion beam milling techniques for TEM specimen preparation10.1016/S0968-4328(99)00005-0 ↗
20. Formation process of shear bands and protrusions in ultrafine grained copper under cyclic stresses10.1016/j.scriptamat.2006.03.001 ↗
21. Nanotwinned metals: it's all about imperfections10.1038/nmat3721 ↗
22. Influence of drawing practices on the mechanical, texture and work hardening characteristics of Co-Cr-Ni-Mo wires10.1016/j.msea.2017.12.063 ↗
23. Plastic Instability in Co-Cr-Ni-Mo alloy wires drawn with different drawing practices10.1016/j.msea.2019.01.059 ↗
24. Study on the deformation homogeneity and electrical conductivity in Co-Cr-Ni-Mo wires drawn with different drawing practices10.1007/s11665-018-3755-2 ↗
25. Gvk · 2019
26. Fracture prediction of cardiac lead medical devices using Bayesian networks10.1016/j.ress.2013.11.005 ↗
27. Grain size effects on the fatigue response of nanocrystalline metals10.1016/S1359-6462(03)00393-2 ↗
28. Microstructural deformation in fatigued nanotwinned copper alloys10.1016/j.actamat.2017.10.057 ↗
29. Quantitative, low cycle, crack initiation fatigue testing of fine wires and CENELEC standard pacing coil10.1002/(SICI)1097-4636(1999)48:3<251::AID-JBM8>3.0.CO;2-7 ↗
30. An overview: fatigue behaviour of ultrafine-grained metals and alloys10.1016/j.ijfatigue.2005.08.014 ↗
31. Kamino · 2005 · 229
32. The ‘size effect’on the stress–strain, fatigue and fracture properties of thin metallic foils10.1016/S0921-5093(01)01043-7 ↗
33. Korpas · 2013
34. Kramme · 2011
35. Fatigue strength, microstructural stability and strain localization in ultrafine-grained copper10.1016/j.msea.2006.02.029 ↗
36. Focused ion beams techniques for nanomaterials characterization10.1002/jemt.20324 ↗
37. Tension and fatigue behavior of silver-cored composite multi-strand cables used as implantable cables and electrodes10.1016/j.msea.2008.03.016 ↗
38. Effect of stress relief process on mechanical performance of MP35N cable as lead conductor in medical device
39. Recent advances in FIB–TEM specimen preparation techniques10.1016/j.matchar.2005.12.007 ↗
40. Controllable fatigue cracking mechanisms of copper bicrystals with a coherent twin boundary10.1038/ncomms4536 ↗
41. Difference in fatigue cracking behaviors of Cu bicrystals with the same component grains but different twin boundaries10.1016/j.scriptamat.2014.09.021 ↗
42. The role of shear banding on the fatigue ductility of ultrafine-grained aluminium10.1016/j.scriptamat.2012.10.038 ↗
43. The effect of grain size on low-cycle fatigue behavior of Al-2024 polycrystalline alloy10.1007/s11661-004-0218-1 ↗
44. Influence of grain size and texture on the cyclic stress-strain response of nickel10.1016/0921-5093(94)90326-3 ↗
45. Cyclic deformation and fatigue properties of very fine-grained metals and alloys10.1016/j.ijfatigue.2009.10.007 ↗
46. The application of focused ion beam microscopy in the material sciences10.1016/j.matchar.2008.11.014 ↗
47. Narushima · 2015 · 157
48. Dual-versus single-coil implantable defibrillator leads: review of the literature10.1007/s00392-011-0407-z ↗
49. Corrosion resistance, chemical passivation, and metal release of 35N LT and MP35N for biomedical material application10.1149/1.2754073 ↗
50. Microstructure and mechanical behavior of an as-drawn MP35N alloy wire10.1016/j.msea.2014.05.046 ↗
51. Microstructure and mechanical behavior of annealed MP35N alloy wire10.1016/j.msea.2015.03.103 ↗
52. The physics of fatigue crack initiation10.1016/j.ijfatigue.2012.10.009 ↗
53. Superior fatigue crack growth resistance, irreversibility, and fatigue crack growth–microstructure relationship of nanocrystalline alloys10.1016/j.actamat.2011.07.058 ↗
54. A probabilistic approach to modeling microstructural variability and fatigue behavior in ASTM F562 medical grade wire
55. An examination of fatigue initiation mechanisms in thin 35Co-35Ni-20Cr-10Mo medical grade wires10.1520/JAI101567 ↗
56. A study of the fatigue properties of small diameter wires used in intramuscular electrodes10.1002/jbm.820250504 ↗
57. Improvement of low-cycle fatigue resistance in TWIP steel by regulating the grain size and distribution10.1016/j.actamat.2017.05.004 ↗
58. Fracture toughness and fatigue crack growth characteristics of nanotwinned copper10.1016/j.actamat.2010.12.043 ↗
59. Wire failure prediction for a rotary beam fatigue tester10.1016/j.csndt.2014.04.001 ↗
60. In situ lift-out dedicated techniques using FIB–SEM system for TEM specimen preparation10.1016/j.micron.2012.05.006 ↗
61. Venugopalan · 2006
62. Fatigue limit and crack growth in ultra-fine grain metals produced by severe plastic deformation10.1007/s10853-006-0973-z ↗
63. Embrittlement phenomenon of Ag core MP35N cable as lead conductor in medical device10.1016/j.jmbbm.2012.09.016 ↗
64. Evolution of dislocations and twins in high cycle fatigue of a twinning-induced plasticity steel10.1016/j.msea.2015.09.017 ↗
65. Cyclic deformation of ultrafine-grained aluminum10.1016/j.actamat.2006.09.002 ↗
66. Shear bands in cyclically deformed ultrafine grained copper processed by ECAP10.1016/j.msea.2003.12.087 ↗
67. The impact of twin lamella thickness distribution on strength and endurance limit in nanotwinned copper10.1016/j.mechmat.2015.01.017 ↗
68. Plastic anisotropy and associated deformation mechanisms in nanotwinned metals10.1016/j.actamat.2012.09.052 ↗
69. Measuring mechanical properties of fine‐wire cross‐sections used in medical devices10.1002/jbm.b.30027 ↗
70. Twin boundary: stronger or weaker interface to resist fatigue cracking?10.1016/j.scriptamat.2012.01.028 ↗
71. Comparison of fatigue cracking possibility along large-and low-angle grain boundaries10.1016/S0921-5093(00)00796-6 ↗
72. What types of grain boundaries can be passed through by persistent slip bands?10.1557/JMR.2003.0141 ↗
73. Observations on persistent slip bands transferring through a grain boundary in a copper bicrystal by the electron channelling contrast in scanning electron microscopy technique10.1080/095008399177291 ↗