journal article·2023-07Open access

Prewarming effect on adaptation, porosities, and strength of a composite resin

K.H. Bolding, A.E. Hill, D. Tantbirojn, A. Versluis

Abstract

Warming composite resin before insertion to reduce viscosity is advocated for improving adaptation and reducing voids. This study evaluated how prewarming altered porosities, adaptation, and strength. Twenty composite restorations were placed in 2 increments in typodont teeth with a large Class II preparation. The composite was either at room temperature (control) or prewarmed to 68 °C (n = 10/group). Each increment was light-cured for 20s. After 24h, the restored teeth were sectioned and imaged under a stereomicroscope. Examiners ranked the quality of adaptation to walls and between increments, and the presence of voids on a 0-3 scale. Results were statistically analyzed using Mann-Whitney U Test. Diametral tensile strength of monolithic or incrementally-filled composite cylinders (6 mm diameter × 4 mm height; n = 10/group) made with room temperature or prewarmed composite were tested at 0.5 mm/min. Strength results were analyzed using ANOVA statistics followed by pairwise comparisons. Restorations made with prewarmed composite had significantly fewer large voids and better adaptation to cavity walls and between layers (P < 0.05). Strength of prewarmed composite was higher than room temperature composite, and was significantly higher in monolithic specimens (P < 0.05). It was concluded that prewarming conventional composite can improve its handling, making it handle more like a flowable composite without jeopardizing physical properties. The prewarmed composite was found to have better adaptation and fewer voids, and attained higher strength than composite that was not prewarmed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Effect of preheating and fatiguing on mechanical properties of bulk-fill and conventional composite resin10.2341/19-092-L ↗
2. Improving composite resin performance through decreasing its viscosity by different methods10.2174/1874210601509010235 ↗
3. Shrinkage behaviour of flowable resin-composites related to conversion and filler-fraction10.1016/j.jdent.2007.05.001 ↗
4. A characterization of first-generation flowable composites10.14219/jada.archive.1998.0274 ↗
5. Brady
6. Monomer conversion of pre-heated composite10.1177/154405910508400716 ↗
7. Polymerization kinetics of pre-heated composite10.1177/154405910608500106 ↗
8. Clinically relevant issues related to preheating composites10.1111/j.1708-8240.2006.00046.x ↗
9. Pre-warming of dental composites10.1016/j.dental.2010.11.009 ↗
10. Longevity of posterior composite restorations: not only a matter of materials10.1016/j.dental.2011.09.003 ↗
11. Effect of pre-heating on the monomer elution and porosity of conventional and bulk-fill resin-based dental composites10.3390/ijms232416188 ↗
12. The strength of layering technique in visible light-cured composites10.1016/0022-3913(89)90104-2 ↗
13. An update on the reasons for placement and replacement of direct restorations10.1016/j.jdent.2018.03.001 ↗
14. Internal adaptation and overhang formation of direct Class II resin composite restorations10.1007/s007840050103 ↗
15. Warming up to composites
16. Composite pre-heating: effects on marginal adaptation, degree of conversion and mechanical properties10.1016/j.dental.2010.03.023 ↗
17. Clinical efficacy of resin-based direct posterior restorations and glass-ionomer restorations – an updated meta-analysis of clinical outcome parameters10.1016/j.dental.2021.10.018 ↗
18. Effect of preheated bulk-fill composite temperature on intrapulpal temperature increase in vitro10.1111/jerd.12503 ↗
19. Lively
20. Heating and preheating of dental restorative materials-a systematic review10.1007/s00784-020-03637-2 ↗
21. Effect of precuring warming on mechanical properties of restorative composites10.1155/2011/536212 ↗
22. Quantification of porosity in composite resins delivered by injectable syringes using X-ray microtomography
23. Porosities and voids in class I restorations placed by six operators using a packable or syringable composite10.1016/S0109-5641(01)00020-3 ↗
24. Longevity of posterior composite restorations: a systematic review and meta-analysis10.1177/0022034514544217 ↗
25. Characterization and comparative analysis of voids in class II composite resin restorations by optical coherence tomography10.2341/18-290-L ↗
26. Diametral tensile strength and dental composites10.1016/S0109-5641(87)80062-3 ↗
27. Determinants of in vitro gap formation of resin composites10.1016/j.jdent.2003.08.008 ↗
28. Clinical challenges and the relevance of materials testing for posterior composite restorations10.1016/j.dental.2004.10.001 ↗
29. Schmedding
30. Hardness and postgel shrinkage of preheated composites
31. Use of near-IR to monitor the influence of external heating on dental composite photopolymerization10.1016/j.dental.2004.02.003 ↗
32. Effect of preheating on the mechanical properties of resin composites
33. Effect of pre-heating resin composite on restoration microleakage10.2341/07-41 ↗
34. Pre-Heating effects on extrusive force, stickiness and packability of resin-based composite10.1016/j.dental.2019.08.101 ↗