Effect of butylated hydroxytoluene (BHT) concentrations on polymerization shrinkage stress and other physicochemical properties of experimental resin composites
Source abstract
Abstract
The present study examined different concentrations of the butylated hydroxytoluene (BHT) inhibitor on the kinetics of conversion, polymerization shrinkage stress, and other correlated physicochemical properties of experimental resin composites (ERC). A model composite was formulated with 75 wt% filler containing 0.5 wt% camphorquinone and 1 wt% amine with BHT concentrations of 0.01 wt% (BHT-0.01); 0.1 wt% (BHT-0.1); 0.25 wt% (BHT-0.25); 0.5 wt% (BHT-0.5); 1 wt% (BHT-1), and control (no BHT). They were tested on polymerization shrinkage stress (PSS; n = 5), degree of conversion (DC; n = 3), maximum polymerization rate (RpMAX; n = 5), water sorption (Wsp; n = 0), and solubility (Wsl; n = 10), flexural strength (FS; n = 10), flexural modulus (FM; n = 10), Knoop microhardness (KH; n = 10), and microhardness reduction (HR; n = 10). Data concerning these tests were submitted to one-way ANOVA and Tukey's test (α = 0.05; β = 0.2). BHT-0.25, BHT-0.5, and BHT-1 showed a gradually significant decrease in PSS (p = 0.037); however, BHT-1 demonstrated a decrease in the physicochemical properties tested. Thus, within the limitations of this study, it was possible to conclude that BHT concentrations between 0.25 and 0.5 wt% are optimal for reducing shrinkage stress without affecting other physicochemical properties of ERCs.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Photopolymerization techniques and applications · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Anusavice · 2003
2. Influence of selected components on crosslink density in polymer structures10.1034/j.1600-0722.2001.00057.x ↗
3. Influence of pulse-delay curing on softening of polymer structures10.1177/00220345010800061801 ↗
4. Two-step curing: influence on conversion and softening of a dental polymer10.1016/S0109-5641(02)00091-X ↗
5. Characterization of water sorption, solubility and filler particles of light-cured composite resins10.1590/S0103-64402009000400009 ↗
6. Effect of stepped light intensity on polymerization force and conversion in a photoactivated composite10.1111/j.1708-8240.2000.tb00195.x ↗
7. Stiffness increase during the setting of dental composite resins10.1177/00220345870660120301 ↗
8. Contraction stress related to degree of conversion and reaction kinetics10.1177/0810114 ↗
9. Alternatives in polymerization contraction stress management10.1177/154411130401500306 ↗
10. Factors involved in the development of polymerization shrinkage stress in resin-composites: a systematic review10.1016/j.dental.2005.04.018 ↗
11. Polymerization shrinkage of posterior composite resins and its possible influence on postoperative sensitivity
12. Setting stresses in composites for two different curing modes10.1016/0109-5641(93)90095-8 ↗
13. The effect of resin formulation on the degree of conversion and mechanical properties of dental restorative resins10.1002/jbm.820200111 ↗
14. Resin composite--state of the art10.1016/j.dental.2010.10.020 ↗
15. Academy of Dental Materials guidance-Resin composites: Part II-Technique sensitivity (handling, polymerization, dimensional changes)10.1016/j.dental.2017.08.188 ↗
16. Monomer conversion, microhardness, internal marginal adaptation, and shrinkage stress of bulk-fill resin composites10.1016/j.dental.2015.10.001 ↗
17. Effect of a polymerization inhibitor on the chemomechanical properties and consistency of experimental resin composites10.1590/0103-6440202204242 ↗
18. The effect of cure rate on the mechanical properties of dental resins10.1016/S0109-5641(01)00010-0 ↗
19. Optimizing light-cured composite through variations in camphorquinone and butylhydroxytoluene concentrations10.1590/1807-3107BOR-2016.vol30.0066 ↗
20. The use of an elastomeric methacrylate monomer (Exothane 24) to reduce the polymerization shrinkage stress and improve the two-body wear resistance of bulk fill composites10.1016/j.dental.2021.12.017 ↗
21. A method for calculating the compliance of bonded-interfaces under shrinkage: validation for Class I cavities10.1016/j.dental.2014.05.032 ↗
22. Reduced light energy density decreases post-gel contraction while maintaining degree of conversion in composites10.1016/S0300-5712(97)00048-1 ↗
23. Cross-link density evaluation through softening tests: effect of ethanol concentration10.1016/j.dental.2007.03.010 ↗
24. Dimethacrylate network formation and polymer property evolution as determined by the selection of monomers and curing conditions10.1016/j.dental.2011.09.005 ↗
25. Correlation between polymerization shrinkage stress and C-factor depends upon cavity compliance10.1016/j.dental.2015.11.003 ↗
26. Digital image correlation in dental materials and related research: a review10.1016/j.dental.2021.02.024 ↗