Effect of rapid cooling on residual stress and surface fracture toughness of dental zirconia
Source abstract
Abstract
Short-time sintering of dental zirconia not only improves manufacturing efficiency of zirconia prosthetics, but also enables an attractive situation in which prosthetic treatment can be completed within a single visit. Although many studies have clarified the effects of heating rate and dwell time on the properties of dental zirconia during short-time sintering, there are only a few studies on rapid cooling. In this study, we investigated the effect of cooling rate on dental zirconia. It was found that the cooling rate had no effect on the three-point flexural strength, but a fast cooling rate improved fracture toughness at the material surface. Raman piezo-spectroscopy showed that a compressive stress layer formed in the neighborhood of the zirconia surface and that its thickness increased with increasing cooling rate. From the above results, it was concluded that the compressive stress layer formed on the surface by rapid cooling improved the apparent fracture toughness at the material surface.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Relationships between fracture toughness, Y2O3 fraction and phases content in modern dental Yttria-doped zirconias10.1016/j.jeurceramsoc.2021.08.003 ↗
2. Flexural strength and failure modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
3. Wear of ceramic-based dental materials10.1016/j.jmbbm.2019.01.009 ↗
4. Computation of residual stresses in quenched Al2O310.1111/j.1151-2916.1972.tb11219.x ↗
5. Crack opening profiles of indentation cracks in normal and anomalous glasses10.1016/j.actamat.2003.09.014 ↗
6. Bio-lubrication phenomena affect residual stresses and phases of zirconia implants
7. Mechanical properties, aging stability and translucency of speed-sintered zirconia for chairside restorations10.1016/j.dental.2020.04.026 ↗
8. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
9. Crack tip fracture toughness of base glasses for dental restoration glass-ceramics using crack opening displacements10.1016/j.jmbbm.2011.04.016 ↗
10. Fracture toughness determinations by indentation10.1111/j.1151-2916.1976.tb10991.x ↗
11. Stresses and stress intensity factor from COD of Vickers indentation cracks10.1023/B:JMSC.0000017792.25386.1d ↗
12. Crack opening displacements of Vickers indentation cracks10.1016/j.engfracmech.2004.07.003 ↗
13. Residual stress and flexural strength of thermally conditioned 96% alumina rods10.1111/j.1151-2916.1968.tb11885.x ↗
14. Effect of surface damage on the strength of Al2O3 ceramics with compressive Surface stresses10.1111/j.1151-2916.1973.tb12343.x ↗
15. Indentation fracture response and damage resistance of Al2O3‐ZrO2 composites strengthened by transformation‐induced residual stresses10.1111/j.1151-2916.1988.tb05818.x ↗
16. Residual compressive surface stress increases the bending strength of dental zirconia10.1016/j.dental.2016.12.007 ↗
17. Thermal conditioning of polycrystalline alumina ceramics10.1111/j.1151-2916.1964.tb14629.x ↗
18. Irwin · 1957
19. Impact of high-speed sintering on translucency, phase content, grain sizes, and flexural strength of 3Y-TZP and 4Y-TZP zirconia materials10.1016/j.prosdent.2019.02.005 ↗
20. Effect of a rapid-cooling protocol on the optical and mechanical properties of dental monolithic zirconia containing 3–5 mol% Y2O310.3390/ma13081923 ↗
21. Kirchner · 2014
22. Strengthening alumina by quenching in various media10.1063/1.1659670 ↗
23. Strengthening of hot‐pressed Al2O3 by quenching10.1111/j.1151-2916.1973.tb12342.x ↗
24. Toughening of layered ceramic composites with residual surface compression10.1111/j.1151-2916.1996.tb07883.x ↗
25. Indentation fracture: principles and applications10.1007/BF00823224 ↗
26. Strength and translucency of zirconia after high-speed sintering10.1111/jerd.12524 ↗
27. Rapid‐sintered dental zirconia for chair‐side one‐visit application10.1111/ijac.13228 ↗
28. Apparent fracture toughness of Si3N4-based laminates with residual compressive or tensile stresses in surface layers10.1016/j.actamat.2004.09.022 ↗
29. Grain boundary segregation-induced phase transformation in yttria-stabilized tetragonal zirconia polycrystal10.2109/jcersj.114.230 ↗
30. Isothermal sintering effects on phase separation and grain growth in yttria-stabilized tetragonal zirconia polycrystal10.1111/j.1551-2916.2008.02861.x ↗
31. Surface toughness of silicon nitride bioceramics: II, Comparison with commercial oxide materials10.1016/j.jmbbm.2015.08.044 ↗
32. Phase stability in plasma-sprayed, partially stabilized zirconia-yttria
33. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
34. Evaluation of the effect of high-speed sintering and specimen thickness on the properties of 5 mol% yttria-stabilized dental zirconia sintered bodies10.3390/ma15165685 ↗
35. Evaluation of the effect of high-speed sintering on the mechanical and crystallographic properties of dental zirconia sintered bodies10.1016/j.jeurceramsoc.2022.10.044 ↗
36. Strength distributions of a quench‐strengthened aluminosilicate ceramic10.1111/j.1151-2916.1988.tb05757.x ↗
37. Raman spectroscopic analysis of phase-transformation and stress patterns in zirconia hip joints10.1117/1.1647547 ↗
38. Surface toughness of silicon nitride bioceramics: I, Raman spectroscopy-assisted micromechanics10.1016/j.jmbbm.2015.09.036 ↗
39. Fracture toughness of ceramics by the Vickers indentation crack length method: a critical review
40. Microhardness and fracture toughness of dental materials by indentation method
41. Computation of the stress intensity factor and COD for submicron sized indentation cracks10.2109/jcersj.114.1044 ↗
42. Mechanical and electrical properties of polymer-derived Si–C–N ceramics reinforced by octadecylamine–Modified single-wall carbon nanotubes10.1016/j.compscitech.2011.02.013 ↗
43. Full-contour zirconia fixed partial dentures as chairside applications: a case report
44. Strengthening of ceramics with quenching residual stress10.2472/jsms.39.590 ↗
45. A systematic review on the accuracy of zirconia crowns and fixed dental prostheses10.1080/26415275.2019.1708202 ↗
46. Wear behavior and microstructural characterization of translucent multilayer zirconia10.1016/j.dental.2020.08.015 ↗
47. Superplasticity of yttria-stabilized tetragonal ZrO2 polycrystals10.1111/j.1551-2916.1986.tb00026.x ↗
48. Phase separation and hydrothermal degradation of 3 mol% Y2O3-ZrO2 ceramics10.2109/jcersj.113.530 ↗
49. Synchrotron X-ray study of the crystal structure and hydrothermal degradation of yttria-stabilized tetragonal zirconia polycrystal10.1111/j.1551-2916.2007.02191.x ↗
50. Load-bearing capacity of lithium disilicate and ultra-translucent zirconias10.1016/j.jmbbm.2018.08.023 ↗
51. Comparative evaluation of the fracture strength of monolithic crowns fabricated from different all-ceramic CAD/CAM materials (an in vitro study)10.13005/bpj/1538 ↗