Influence of an internal firing of feldspathic porcelain before or after sintering on adaptation of high-translucent zirconia laminate veneers
Source abstract
Abstract
The aim of the present study was to evaluate the influence of two different internal surface treatments, namely, the firing of feldspathic porcelain before or after zirconia sintering, on the marginal and internal adaptation of laminate veneers (LVs) made of high-translucent zirconia. A total of 33 zirconia LVs were fabricated using a CAD/CAM system and divided into three groups based on the internal surface treatment method: the pre-firing (PRE) group involved firing feldspathic porcelain before zirconia sintering, the post-firing (POS) group involved firing feldspathic porcelain after zirconia sintering, and the no treatment (NT) group involved no application of feldspathic porcelain. The adaptation of the LVs was measured using a silicone replica technique. Data were analyzed using the Kruskal-Wallis and Steel-Dwass tests (α = .05). The POS group showed significantly higher marginal discrepancy values than the PRE group across all sites. The internal space values of the PRE groups were significantly lower than those of the NT group at all sites. The internal firing of feldspathic porcelain before zirconia sintering resulted in better marginal adaptation of the high-translucent zirconia LVs than the internal firing of feldspathic porcelain after zirconia sintering. The internal firing of feldspathic porcelain before zirconia sintering can achieve uniform internal adaptation of high-translucent zirconia LVs.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Internal adaptation, marginal accuracy and microleakage of a pressable versus a machinable ceramic laminate veneers10.1016/j.jdent.2012.04.019 ↗
2. Long-term survival and complication rates of porcelain laminate veneers in clinical studies: a systematic review10.3390/jcm10051074 ↗
3. Survival rates for porcelain laminate veneers: a systematic review
4. Anterior veneer restorations - an evidence-based minimal-intervention perspective
5. Retrospective evaluation of the clinical performance and longevity of porcelain laminate veneers 7 to 14 years after cementation10.1016/j.prosdent.2018.09.007 ↗
6. Evaluation of marginal and internal fit of a CAD/CAM monolithic zirconia-reinforced lithium silicate porcelain laminate veneer system10.1111/jopr.13438 ↗
7. Marginal fit of gold inlay castings10.1016/0022-3913(66)90082-5 ↗
8. Digital evaluation of marginal and internal fit of single-crown fixed dental prostheses10.1111/eos.12576 ↗
9. Marginal and internal fit of pre-sintered Co-Cr and zirconia 3-unit fixed dental prostheses as measured using microcomputed tomography10.1016/j.prosdent.2018.01.006 ↗
10. Comparison of the marginal adaptation of zirconium dioxide crowns in preparations with two different finish lines10.1111/j.1532-849X.2011.00831.x ↗
11. Improved bonding of zirconia substructures to resin using a "glaze-on" technique10.1016/j.jdent.2011.12.011 ↗
12. Shear bond strength between an indirect composite layering material and feldspathic porcelain-coated zirconia ceramics10.1007/s00784-011-0641-9 ↗
13. A review on translucent zirconia
14. Randomized clinical trial on indirect resin composite and ceramic laminate veneers: up to 10-year findings10.1016/j.jdent.2019.06.001 ↗
15. Effect of firing procedures and layering thickness of porcelain on internal adaptation of zirconia cantilever resin-bonded fixed dental prostheses10.2186/jpr.JPR_D_21_00055 ↗
16. Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics10.4012/dmj.28.446 ↗
17. Influence of the veneering process on the marginal fit of zirconia fixed dental prostheses10.1111/j.1365-2842.2009.02053.x ↗
18. Clinical marginal and internal gaps of Procera AllCeram crowns10.1111/j.1365-2842.2005.01458.x ↗
19. Effect of preparation design on marginal and internal adaptation of translucent zirconia laminate veneers10.1111/eos.12574 ↗
20. Precision of fit: the procera AllCeram crown10.1016/S0022-3913(98)70002-2 ↗
21. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
22. The estimation of cement film thickness by an in vivo technique10.1038/sj.bdj.4802708 ↗
23. Influence of film thickness on joint bend strength of a ceramic/resin composite joint10.1016/S0109-5641(96)80030-3 ↗
24. Shear bond strength between different materials bonded with two resin cements10.1111/j.1741-2358.2011.00565.x ↗
25. Marginal adaptation of three-unit fixed partial dentures constructed from pressed ceramic systems10.1038/sj.bdj.4811390 ↗
26. Evaluation of resin bond strength to yttria-stabilized tetragonal zirconia and framework marginal fit: comparison of different surface conditionings10.2341/12-269-L ↗
27. Clinical evaluation comparing the fit of all-ceramic crowns obtained from silicone and digital intraoral impressions10.1007/s00784-015-1590-5 ↗