Should the load-to-fracture test for CAD/CAM monolithic molar crowns be standardized and how? A systematic review and finite element analysis
Source abstract
Abstract
The load-to-fracture test is widely used to evaluate crowns made of new CAD/CAM materials, even though its validity in predicting clinical performances is often questioned. Despite its limitations, the test is useful in assessing the load-bearing capacity of crowns subjected to accidental overloads and setting up step-stress regimes for fatigue testing. This study combined a systematic review (SR) and finite element analysis (FEA) to assess whether the test should be standardized and how. The SR evaluated load-to-fracture studies of monolithic CAD/CAM molar crowns published in Q1 and Q2 journals. Findings from 85 studies highlighted the lack of standardization in test methods, particularly regarding loading head type and die material. This variability led to a wide dispersion of fracture load results, limiting the utility of the load-to-fracture test. The FEA evaluated the influence of loading head type and die material on tensile stress distribution in lithium disilicate (LD) and polymer-infiltrated ceramic network (PICN) crowns. Eight in vitro conditions were simulated, varying the loading head (4 mm and 10 mm spheres, inverse V-shaped device, opposing teeth) and die material (stiff, E = 207 GPa; non-stiff, E = 13 GPa). The FEA confirmed that the stress distribution and peak tensile stress in LD and PICN crowns depend significantly on these factors as well as the crown material properties, with the peak stress variation from LD to PICN ranging from -4 % to 237 %. Using larger-diameter spheres with a die material approximating dentin in stiffness resulted in stress distributions more representative of clinical conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. The fracture strength of endocrowns manufactured from different hybrid blocks under axial and lateral forces10.1007/s00784-020-03495-y ↗
2. Fatigue failure load of molars with thin-Walled prosthetic crowns made of various materials: a 3D-FEA theoretical study10.2147/CCIDE.S286826 ↗
3. Fracture resistance and failure mode of monolithic zirconia, veneered zirconia, and metal-ceramic full-coverage restorations: a comparative in vitro study10.11607/ijp.8171 ↗
4. Comparative evaluation of fracture resistance and failure modes in endodontically treated molars restored with zirconia endocrown and onlays10.3897/folmed.65.e75621 ↗
5. Fatigue analysis of computer‐aided design/computer‐aided manufacturing resin‐based composite vs. lithium disilicate glass‐ceramic10.1111/eos.12278 ↗
6. Fracture toughness of chairside CAD/CAM materials – alternative loading approach for compact tension test10.1016/j.dental.2016.03.003 ↗
7. Survivability and fracture resistance of monolithic and multi-yttria-layered zirconia crowns as a function of yttria content: a mastication simulation study10.1111/jerd.12907 ↗
8. The influence of ferrule on the marginal gap and fracture resistance of zirconia endocrowns10.11607/ijp.8060 ↗
9. Fracture resistance of CAD-CAM monolithic ceramic and veneered zirconia molar crowns after aging in a mastication simulator10.1016/j.prosdent.2017.05.003 ↗
10. Scanning electron microscopy assessment of the load-bearing capacity of cad/cam-fabricated molar crowns10.1590/1807-3107bor-2020.vol34.0035 ↗
11. Zirconia-reinforced lithium silicate crowns: effect of thickness on survival and failure mode10.1016/j.dental.2019.04.007 ↗
12. In vitro performance of full-contour zirconia single crowns10.1016/j.dental.2011.11.024 ↗
13. Biomechanical behavior of molars restored with direct and indirect restorations in combination with deep margin elevation10.1016/j.jmbbm.2024.106459 ↗
14. Fracture resistance of additively or subtractively manufactured resin-based definitive crowns: effect of restorative material, resin cement, and cyclic loading10.1016/j.dental.2024.05.020 ↗
15. A comparative strength study of metal ceramic and all-ceramic esthetic materials: modulus of rupture10.1016/0022-3913(89)90184-4 ↗
16. Fatigue resistance of CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2013.09.020 ↗
17. Chen · 1994
18. Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns10.1016/S0022-3913(99)70036-3 ↗
19. Load-bearing capacity of various CAD/CAM monolithic molar crowns under recommended occlusal thickness and reduced occlusal thickness conditions10.4047/jap.2017.9.6.423 ↗
20. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
21. Post-fatigue fracture resistance of lithium disilicate and polymer-infiltrated ceramic network indirect restorations over endodontically-treated molars with different preparation designs: an in-vitro study10.3390/polym14235084 ↗
22. Effect of intracoronal depth of teeth restored with endocrowns on fracture resistance: in vitro and 3-dimensional finite element analysis10.1016/j.joen.2018.04.008 ↗
23. Mechanical behavior of endocrowns fabricated with different CAD-CAM ceramic systems10.1016/j.prosdent.2019.11.008 ↗
24. Characterization of a polymer-infiltrated ceramic-network material10.1016/j.dental.2014.02.019 ↗
25. How and when does fabrication damage adversely affect the clinical performance of ceramic restorations?10.1016/j.dental.2012.07.001 ↗
26. Fracture resistance and failure modes of endocrowns manufactured with different CAD/CAM materials under axial and lateral loading10.1111/jerd.12486 ↗
27. Polymer infiltrated ceramic network structures for resistance to fatigue fracture and wear10.1016/j.dental.2016.08.216 ↗
28. Influence of fatigue loading on fracture resistance of endodontically treated teeth restored with endocrowns10.2186/jpr.JPOR_2019_485 ↗
29. Marginal gap distance and cyclic fatigue loading for different all-ceramic endocrowns
30. Flexural resistance of heat-pressed and CAD-CAM lithium disilicate with different translucencies10.1016/j.dental.2016.10.005 ↗
31. Post-fatigue fracture and marginal behavior of endodontically treated teeth: partial crown vs. Full crown vs. Endocrown vs. Fiber-reinforced resin composite10.3390/ma14247733 ↗
32. The influence of aging on the fracture load of milled monolithic crowns10.1186/s12903-022-02529-z ↗
33. Fracture resistance of computer‐aided design/computer‐aided manufacturing‐generated composite resin‐based molar crowns10.1111/eos.12173 ↗
34. Contact damage as a failure mode during in vitro testing10.1111/j.1532-849X.1996.tb00281.x ↗
35. Material characteristics of a novel shrinkage-free ZrSiO4 ceramic for the fabrication of posterior crowns10.1016/j.dental.2006.06.015 ↗
36. Fracture strength and marginal and internal adaptation of lithium disilicate and hybrid ceramic endocrowns and non-retentive overlays for endodontically treated molar teeth10.1186/s12903-024-05327-x ↗
37. Influence of different surface finishing procedures of strength-gradient multilayered zirconia crowns on two-body wear and fracture load: lithium silicate or leucite glazing versus polishing?10.1016/j.jmbbm.2023.106307 ↗
38. Failure load effect of molar axial wall height with CAD/CAM ceramic crowns with moderate occlusal convergence10.1111/jerd.12366 ↗
39. Effect of cementation techniques on fracture load of monolithic zirconia crowns
40. The effect of preparation design on the fracture resistance and adaptation of the CEREC ceramic endocrowns10.1002/cre2.726 ↗
41. Effect of supporting dies' mechanical properties on fracture behavior of monolithic zirconia molar crowns10.4012/dmj.2021-090 ↗
42. Influence of margin designs on crack initiation of high translucency monolithic zirconia crowns10.1111/jopr.13269 ↗
43. Comparison of full and partial coverage crowns with CAD/CAM leucite reinforced ceramic blocks on fracture resistance and fractographic analysis10.4012/dmj.2021-253 ↗
44. Fracture resistance of zirconia surveyed crowns with four different occlusal rest seat designs
45. Fracture characteristics and translucency of multilayer monolithic zirconia crowns of various thicknesses10.1016/j.jdent.2024.105023 ↗
46. Fracture analysis of monolithic CAD‐CAM crowns10.1111/jerd.12462 ↗
47. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
48. The slippery slope – critical perspectives on in vitro research methodologies10.1016/j.dental.2011.09.001 ↗
49. Fracture resistance of monolithic zirconia crowns depending on different marginal thicknesses10.3390/ma15144861 ↗
50. Fracture resistance of all-ceramic crowns based on different preparation designs for restoring endodontically treated molars10.1111/jerd.12410 ↗
51. Mechanical properties of dental luting cements10.1016/S0022-3913(99)70216-7 ↗
52. Microstructural evolution and physical behavior of a lithium disilicate glass–ceramic10.1016/j.dental.2015.05.003 ↗
53. Fractographic analysis of lithium silicate crown failures during sintering10.1177/2050313X19838962 ↗
54. Speed-sintering and the mechanical properties of 3-5 mol% Y(2)O(3)-stabilized zirconias10.1007/s10266-023-00796-y ↗
55. Comparison between novel strength-gradient and color-gradient multilayered zirconia using conventional and high-speed sintering10.1016/j.jmbbm.2020.103977 ↗
56. Internal adaptation and mechanical properties of CAD/CAM glass fiber post-cores in molars: an in vitro study10.1016/j.jdent.2023.104685 ↗
57. Influence of the preparation design and artificial aging on the fracture resistance of monolithic zirconia crowns10.4047/jap.2016.8.1.30 ↗
58. Clinical evaluation of monolithic zirconia crowns: a failure analysis of clinically obtained cases from a 3.5-year study10.2186/jpr.JPOR_2019_643 ↗
59. Effect of two self‐adhesive cements on marginal adaptation and strength of esthetic ceramic CAD/CAM molar crowns10.1111/j.1532-849X.2009.00461.x ↗
60. Fracture resistance and 3D finite element analysis of machined ceramic crowns bonded to endodontically treated molars with two planes versus flat occlusal preparation designs: an in vitro study10.12688/f1000research.19455.2 ↗
61. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
62. The influence of low-temperature degradation and cyclic loading on the fracture resistance of monolithic zirconia molar crowns10.1016/j.jmbbm.2015.03.007 ↗
63. Critical considerations on load-to-failure test for monolithic zirconia molar crowns10.1016/j.jmbbm.2018.07.034 ↗
64. Fracture load and survival of anatomically representative monolithic lithium disilicate crowns with reduced tooth preparation and ceramic thickness10.4047/jap.2017.9.6.416 ↗
65. In vitro simulation of periodontal ligament in fatigue testing of dental crowns10.1055/s-0040-1713953 ↗
66. Nelson · 2010 · 401
67. Clinically relevant fracture testing of all-ceramic crowns10.1016/j.dental.2013.04.026 ↗
68. Fractographic analyses of all-ceramic crowns: a study of 27 clinically fractured crowns10.1016/j.dental.2013.03.018 ↗
69. Simulation of clinical fractures for three different all-ceramic crowns10.1111/eos.12128 ↗
70. Fractographic features of glass‐ceramic and zirconia‐based dental restorations fractured during clinical function10.1111/eos.12127 ↗
71. Load at fracture of monolithic and bilayered zirconia crowns with and without a cervical zirconia collar10.1016/j.prosdent.2015.11.017 ↗
72. Fracture strength testing of crowns made of CAD/CAM composite resins10.1016/j.jpor.2017.10.003 ↗
73. Fracture strength of CAD/CAM posterior ceramic crowns after manual enhancement of occlusal morphology
74. Fracture resistance and microleakage of endocrowns utilizing three CAD-CAM blocks10.2341/13-143-L ↗
75. Influence of cementation on in vitro performance, marginal adaptation and fracture resistance of CAD/CAM-fabricated ZLS molar crowns10.1016/j.dental.2015.08.154 ↗
76. In vitro performance and fracture resistance of novel CAD/CAM ceramic molar crowns loaded on implants and human teeth10.4047/jap.2018.10.4.300 ↗
77. Monolithic zirconia crowns: effect of thickness reduction on fatigue behavior and failure load10.4047/jap.2021.13.5.269 ↗
78. Flexural strength and modulus of elasticity of different types of resin-based composites10.1590/S1806-83242007000100003 ↗
79. In vitro performance and fracture resistance of CAD/CAM-fabricated implant supported molar crowns10.1007/s00784-016-1898-9 ↗
80. In-vitro performance of CAD/CAM crowns with insufficient preparation design10.1016/j.jmbbm.2018.10.002 ↗
81. Fracture force of CAD/CAM resin composite crowns after in vitro aging10.1007/s00784-019-03099-1 ↗
82. Stability and wear of zirconia crowns with micro-layering10.1016/j.jdent.2023.104560 ↗
83. In-vitro performance of subtractively and additively manufactured resin-based molar crowns10.1016/j.jmbbm.2023.105806 ↗
84. Evaluation of marginal/internal fit and fracture load of monolithic zirconia and zirconia lithium silicate (ZLS) CAD/CAM crown systems10.3390/ma14216346 ↗
85. Marginal adaptation and fracture strength of endocrowns manufactured with different restorative materials: SEM and mechanical evaluation10.1002/jemt.23586 ↗
86. Comparison of retention and fracture load of endocrowns made from zirconia and zirconium lithium silicate after aging: an in vitro study10.1186/s12903-022-02072-x ↗
87. Mechanical strength and subcritical crack growth under wet cyclic loading of glass-infiltrated dental ceramics10.1016/j.dental.2010.01.007 ↗
88. Marginal discrepancy and fracture load of thermomechanically fatigued crowns fabricated with different CAD‐CAM techniques10.1111/jopr.13612 ↗
89. ADM guidance—ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
90. Impact of the occlusal contact pattern and occlusal adjustment on the wear and stability of crowns10.1016/j.jdent.2022.104364 ↗
91. Monolithic zirconia dental crowns. Internal fit, margin quality, fracture mode and load at fracture10.1016/j.dental.2017.06.009 ↗
92. New material perspective for endocrown restorations: effects on mechanical performance and fracture behavior10.1590/1807-3107bor-2019.vol33.0012 ↗
93. Failure loads of heat-pressed versus milled lithium disilicate endocrowns10.1007/s00784-022-04728-y ↗
94. Features of fracture of prosthetic tooth-endocrown constructions by means of acoustic emission analysis10.1016/j.dental.2018.01.023 ↗
95. Acoustic properties of fracture of dental restorative materials and endocrown restorations under quasi-static loading10.1016/j.dental.2020.03.014 ↗
96. Fractographic analysis of 35 clinically fractured bi-layered and monolithic zirconia crowns10.1016/j.jdent.2022.104271 ↗
97. Fracture strength of minimally prepared all-ceramic CEREC crowns after simulating 5 years of service10.1016/j.dental.2013.03.019 ↗
98. In vitro analysis of the fracture resistance of CAD–CAM monolithic zirconia molar crowns with different occlusal thickness10.1016/j.jmbbm.2016.04.014 ↗
99. Standardization · 2015
100. Marginal adaptation and fracture resistance of milled and 3D-printed CAD/CAM hybrid dental crown materials with various occlusal thicknesses10.2186/jpr.JPR_D_23_00089 ↗