journal article·2016-07

Manufacturing of high-strength Ni-free Co–Cr–Mo alloy rods via cold swaging

Kenta Yamanaka, Manami Mori, Kazuo Yoshida, Koji Kuramoto, Akihiko Chiba

Publisher page

Abstract

The strengthening of biomedical metallic materials is crucial to increasing component durability in biomedical applications. In this study, we employ cold swaging as a strengthening method for Ni-free Co-Cr-Mo alloy rods and examine its effect on the resultant microstructures and mechanical properties. N is added to the alloy to improve the cold deformability, and a maximum reduction in area (r) of 42.6% is successfully obtained via cold swaging. The rod strength and ductility increase and decrease, respectively, with increasing cold-swaging reduction r. Further, the 0.2% proof stress at r=42.6% eventually reaches 1900MPa, which is superior to that obtained for the other strengthening methods proposed to date. Such significant strengthening resulting from the cold-swaging process may be derived from extremely large work hardening due to a strain-induced γ (fcc)→ε (hcp) martensitic transformation, with the resultant intersecting ε-martensite plates causing local strain accumulation at the interfaces. The lattice defects (dislocations/stacking faults) inside the ε phase also likely contribute to the overall strength. However, excessive application of strain during the cold-swaging process results in a severe loss in ductility. The feasibility of cold swaging for the manufacture of high-strength Co-Cr-Mo alloy rods is discussed.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Mechanical properties of forged low Ni and C-Containing Co−Cr−Mo biomedical implant alloy10.4028/www.scientific.net/MSF.475-479.2317 ↗
2. Nickel essentiality, toxicity, and carcinogenicity10.1016/S1040-8428(01)00214-1 ↗
3. Disegi · 1999
4. Ultrastrong Mg alloy via nano-spaced stacking faults10.1080/21663831.2013.765927 ↗
5. Physics and model of strengthening by parallel stacking faults10.1063/1.4822323 ↗
6. Kocks · 2000
7. Grain refinement of biomedical Co–27Cr–5Mo–0.16N alloy by reverse transformation10.1016/j.matlet.2009.10.001 ↗
8. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
9. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
10. Nano-sized twins induce high rate sensitivity of flow stress in pure copper10.1016/j.actamat.2005.01.031 ↗
11. Deformation induced FCC to HCP transformation in a Co−27Cr−5Mo−0.05C alloy10.1016/j.msea.2010.12.024 ↗
12. Fatigue and life prediction for cobalt–chromium stents: a fracture mechanics analysis10.1016/j.biomaterials.2005.10.012 ↗
13. Deformation mode in biomedical Co–27% Cr–5% Mo alloy consisting of a single hexagonal close-packed structure10.1016/j.scriptamat.2010.08.006 ↗
14. Evolution of cold-rolled microstructures of biomedical Co−Cr−Mo alloys with and without N doping10.1016/j.msea.2010.09.002 ↗
15. Microstructures and mechanical properties of biomedical Co−29Cr−6Mo−0.14N alloys processed by hot rolling10.1007/s11661-012-1156-y ↗
16. Cold-rolling behavior of biomedical Ni-free Co−Cr−Mo alloys: role of strain-induced ε martensite and its intersecting phenomena10.1016/j.jmbbm.2015.10.021 ↗
17. Texture evolution and mechanical anisotropy of biomedical hot-rolled Co–Cr–Mo alloy10.1016/j.jmbbm.2015.06.034 ↗
18. Strengthening of biomedical Co–Cr–Mo alloy by multipass “low-strain-per-pass” thermomechanical processing10.1016/j.actbio.2015.09.016 ↗
19. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
20. Effects of heat treatment and hot forging on microstructure and mechanical properties of Co−Cr−Mo alloy for surgical implants10.2320/matertrans.MRA2007274 ↗
21. Deformation behavior of low-carbon Co−Cr−Mo alloys for low-friction implant applications10.1002/(SICI)1097-4636(199607)31:3<409::AID-JBM16>3.0.CO;2-D ↗
22. The effect of contouring on fatigue strength of spinal rods: is it okay to Re-bend and which materials are best?10.1016/j.jspd.2013.08.004 ↗
23. Assessment of symptomatic rod fracture after posterior instrumented fusion for adult spinal deformity10.1227/NEU.0b013e3182672aab ↗
24. Strengthening an austenitic Fe–Mn steel using nanotwinned austenitic grains10.1016/j.actamat.2012.03.035 ↗
25. Dental alloys
26. Ultrafine grain refinement of biomedical Co−29Cr−6Mo alloy during conventional hot-compression deformation10.1007/s11661-009-9879-0 ↗
27. Mechanical properties of as-forged Ni-free Co−29Cr−6Mo alloys with ultrafine-grained microstructure10.1016/j.msea.2011.04.027 ↗
28. Enhanced mechanical properties of as-forged Co–Cr–Mo−N alloys with ultrafine-grained structures10.1007/s11661-012-1288-0 ↗
29. Origin of significant grain refinement in Co−Cr−Mo alloys without severe plastic deformation10.1007/s11661-012-1303-5 ↗
30. Effects of nitrogen addition on microstructure and mechanical behavior of biomedical Co−Cr−Mo alloys10.1016/j.jmbbm.2013.10.006 ↗
31. Analysis of the fracture mechanism of Ti−6Al−4V alloy rods that failed clinically after spinal instrumentation surgery10.1097/BRS.0000000000000881 ↗
32. Strength and ductility of 316L austenitic stainless steel strengthened by nano-scale twin bundles10.1016/j.actamat.2011.11.009 ↗
33. Growing spine study group, Growing rod fractures: risk factors and opportunities for prevention10.1097/BRS.0b013e31822a982f ↗
34. Rods in spinal surgery: a review of the literature10.1016/j.spinee.2013.04.022 ↗