Step-stress vs. staircase fatigue tests to evaluate the effect of intaglio adjustment on the fatigue behavior of simplified lithium disilicate glass-ceramic restorations
Source abstract
Abstract
The aim of the study was to compare the outcomes for the fatigue mechanical behavior of bonded simplified lithium disilicate restorations, with and without an internal adjustment by grinding with diamond bur in running two fatigue tests: Staircase and Step-stress testing approaches. Ceramic discs (IPS e.max CAD) were prepared (Ø = 10 mm; thickness = 1.0 mm), submitted to an in-lab simulation of CAD/CAM milling (#60 SiC paper) and allocated into 2 groups according to the internal adjustment by grinding of the cementation surface: no adjustment (CTRL); or grinding with a coarse diamond bur (GR). Adhesive cementation (Multilink N) was performed onto epoxy resin discs (Ø = 10 mm; thickness = 2 mm) after ceramic/epoxy surface treatments. The cemented assemblies of each group were randomly assigned into 2 subgroups considering two fatigue tests (n = 15): Staircase - SC (250,000 cycles; 20 Hz), or Step-stress - SS (10,000 cycles per step; 20 Hz). Roughness, topographic and fractographic analyses were additionally performed. Statistical analyses were carried out using the Dixon and Mood method for Staircase data, and Kaplan-Meier and Mantel-Cox (log-rank) tests for Step-stress data. Ceramic restorations having its intaglio surface ground (GR group: SC test = 306.67 N; SS test = 646.67 N) presented lower fatigue failure load (FFL) values than the CTRL group (SC test = 879.28 N; SS test = 1090.00 N), regardless of the fatigue testing approach. The percentage of mean FFL decrease comparing the CTRL to GR group was higher for SC (65.1%) than the SS (40.7%) approach. However, a different total number of cycles was applied for each method. Both fatigue tests were able to detect the negative effect of internal adjustments of lithium disilicate glass-ceramic simplified restorations on their mechanical behavior. Therefore, both methods can be applied for similar evaluations (fatigue testing for ceramic restorations).
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Fatigue resistance of Y-TZP/porcelain crowns is not influenced by the conditioning of the intaglio surface10.2341/14-166-L ↗
2. Fatigue of restorative materials10.1177/10454411010120040501 ↗
3. Reliability and failure behavior of CAD-on fixed partial dentures10.1016/j.dental.2016.01.013 ↗
4. Mechanical fatigue degradation of ceramics versus resin composites for dental restorations10.1016/j.dental.2014.01.003 ↗
5. A critical perspective on mechanical testing of implants and prostheses10.1177/0022034515624445 ↗
6. The contact mechanics of fractal surfaces10.1038/nmat855 ↗
7. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
8. Fatigue Testing Procedures and Statistical Interpretations of Data
9. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
10. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
11. Mar. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
12. A method for obtaining and analyzing sensitivity data10.1080/01621459.1948.10483254 ↗
13. Crack propagation in ceramic materials under cyclic loading conditions
14. Size and shape of the human first permanent molar: a Fourier analysis of the occlusal and equatorial outlines10.1002/(SICI)1096-8644(199903)108:3<281::AID-AJPA4>3.0.CO;2-# ↗
15. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
16. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
17. A review of the strength properties of dental ceramics10.1016/0022-3913(92)90602-7 ↗
18. ISO 4287 · 1997
19. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
20. Ceramics 101: what Is This Stuff Anyway?
21. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
22. Fracture surface analysis of dental ceramics: clinically failed restorations
23. Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2015.04.014 ↗
24. Influence of surface finishing on fracture load and failure mode of glass ceramic crowns10.1016/j.prosdent.2016.12.012 ↗
25. Comparison of fatigue resistance and failure modes between metal-ceramic and all-ceramic crowns by cyclic loading in water10.1016/j.jdent.2014.08.013 ↗
26. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
27. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
28. Hydrofluoric acid concentrations: effect on the cyclic load-to-failure of machined lithium disilicate restorations10.1016/j.dental.2018.06.028 ↗
29. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
30. A critical evaluation of fatigue studies for restorative materials in Dentistry10.1007/s40496-016-0097-8 ↗
31. Influence of external and internal surface roughness modifications on ceramic flexural strength10.1016/j.prosdent.2014.04.003 ↗
32. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
33. Fatigue resistance of CAD/CAM resin composite molar crowns10.1016/j.dental.2015.12.005 ↗
34. Surface and intra-pulpal temperature rises during tooth bleaching: an in vitro study10.1038/sj.bdj.4812558 ↗
35. Suresh · 1998
36. Determining the slow crack growth parameter and Weibull two parameter estimates of bilaminate disks by constant displacement-rate flexural testing10.1016/S0109-5641(03)00068-X ↗
37. Fracture surface characterization of clinically failed all-ceramic crowns10.1177/00220345940730120601 ↗
38. Fatigue performance of adhesively cemented glass-, hybrid- and resin-ceramic materials for CAD/CAM monolithic restorations10.1016/j.dental.2019.01.013 ↗
39. Effects of two grading techniques of zirconia material on the fatigue limit of full-contour 3-unit fixed dental prostheses10.1016/j.dental.2016.12.010 ↗
40. Stress fatigue: basic principles and prosthodontic implications