journal article·2016-01

Evaluation of the shear bond strength of dental porcelain and the low magnetic susceptibility Zr–14Nb alloy

Yuka Kajima, Atsushi Takaichi, Tohru Yasue, Hisashi Doi, Hidekazu Takahashi, Takao Hanawa, Noriyuki Wakabayashi

Publisher page

Abstract

The aim of this study was to investigate the bond strength of dental porcelain and the preheated Zr-14Nb alloy, and compare this strength with that of titanium. White oxide layers, which were predominantly composed of monoclinic zirconia, were formed on the preheated sample groups, and exhibited a greater roughness than the control samples. At the metal-ceramic interface, a greater Nb diffusion range was observed than in the control samples. The bond strengths of the samples subjected to 20min preheating treatment were the lowest (33.6 ± 3.2 MPa), which may be ascribed to the formation of a brittle thick oxide layer under excessive heat treatment. The samples subjected to this heat treatment for 5 min exhibited the highest mean bond strength (43.7 ± 5.9 MPa), which was significantly higher than that of titanium (35.3 ± 3.5 MPa). Thus, the Zr-14Nb alloy is a promising candidate for fixed dental prosthesis, as long as the appropriate treatment conditions are adopted.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Oxide adherence and porcelain bonding to titanium and Ti–6Al–4V alloy10.1177/00220345900690060101 ↗
2. Effect of surface roughness on the texture and oxidation behavior of Zircaloy-4 cladding tube10.1016/j.apsusc.2013.08.137 ↗
3. Adherence controlling elements in ceramic–metal systems. I. Precious alloys10.1177/00220345770560090301 ↗
4. Adherence controlling elements in ceramic–metal systems. II. Nonprecious alloys10.1177/00220345770560090401 ↗
5. Bonding mechanism evidence in a ceramic—nonprecious alloy system10.1002/jbm.820110506 ↗
6. Oxidation properties of Zr–Nb alloys at 973–1273K in air
7. The effect of zinc levels in a gold-based alloy on porcelain-metal bonding10.1016/j.dental.2012.02.003 ↗
8. Influence of pulse sequence parameters at 1.5T and 3.0T on MRI artefacts produced by metal–ceramic restorations
9. Artifacts in brain magnetic resonance imaging due to metallic dental objects
10. Effect of oxidation on ceramometal bond strength10.1016/0022-3913(82)90243-8 ↗
11. Designs of bond strength tests for metal-ceramic complexes: review of the literature10.1016/S0022-3913(96)90244-9 ↗
12. Comparative microstructural study of the diffusion zone between NiCr alloy and different dental ceramics10.1177/154405910208100509 ↗
13. Optimization of bond strength between gold alloy and porcelain through a composite interlayer obtained by powder metallurgy10.1016/j.msea.2010.10.054 ↗
14. Microstructure, hardness, corrosion resistance and porcelain shear bond strength comparison between cast and hot pressed CoCrMo alloy for metal–ceramic dental restorations10.1016/j.jmbbm.2012.03.015 ↗
15. Experimental evaluation of the bond strength between a CoCrMo dental alloy and porcelain through a composite metal–ceramic graded transition interlayer10.1016/j.jmbbm.2012.04.019 ↗
16. Clinical values of (18) F-FDG PET/CT in oral cavity cancer with dental artifacts on CT or MRI10.1002/jso.23691 ↗
17. Three-dimensional quantification of susceptibility artifacts from various metals in magnetic resonance images10.1016/j.actbio.2013.05.017 ↗
18. ISO 9693 Metal–Ceramic Dental Restorative Systems, 1999. Geneva: International Organization for Standardization.
19. Physico-mechanical properties and prosthodontic applications of Co–Cr dental alloys: a review of the literature10.4047/jap.2014.6.2.138 ↗
20. Thermodynamic evaluation of the Nb–O–Zr system10.1016/j.jnucmat.2006.10.008 ↗
21. Surface characteristics and castability of Zr–14Nb alloy dental castings10.4012/dmj.2014-117 ↗
22. Oxidation effects on porcelain-titanium interface reactions and bond strength10.4012/dmj.9.91 ↗
23. Microstructure and mechanical properties of as-cast Zr–Nb alloys10.1016/j.actbio.2011.07.020 ↗
24. Effect of cold rolling on the magnetic susceptibility of Zr–14Nb alloy10.1016/j.actbio.2012.10.046 ↗
25. Fusing of dental ceramics to titanium10.1177/00220345010800030101 ↗
26. Effect of pretreatments on the metal–ceramic bonding strength of a Pd–Ag alloy10.1016/j.jdent.2013.11.020 ↗
27. Quantification of susceptibility artifacts produced on high-field magnetic resonance images by various biomaterials used for neurosurgical implants. Technical note10.3171/jns.2002.97.6.1472 ↗
28. Effect of preoxidation of titanium on the titanium–ceramic bonding
29. Electrochemical studies on zirconium and its biocompatible alloys Ti–50Zr at.% and Zr–2.5Nb wt.% in simulated physiologic media10.1002/jbm.a.30352 ↗
30. Early laser-welded titanium frameworks supported by implants in the edentulous mandible: a 15-year comparative follow-up study10.1111/j.1708-8208.2008.00119.x ↗
31. Laser-welded titanium frameworks supported by implants in the partially edentulous mandible: a 10-year comparative follow-up study10.1111/j.1708-8208.2007.00073.x ↗
32. A systematic review of the survival and complication rates of implant-supported fixed dental prostheses (FDPs) after a mean observation period of at least 5 years10.1111/j.1600-0501.2012.02546.x ↗
33. Artifacts from dental casting alloys in magnetic resonance imaging10.1177/154405910308200806 ↗
34. Mechanical and chemical analyses across dental porcelain fused to CP titanium or Ti6Al4V10.1016/j.msec.2013.12.030 ↗
35. Effects of phase constitution on magnetic susceptibility and mechanical properties of Zr-rich Zr–Mo alloys10.1016/j.actbio.2011.07.005 ↗
36. Influence of the processing route of porcelain/Ti–6Al–4V interfaces on shear bond strength10.1016/j.jmbbm.2013.02.003 ↗
37. Retrospective analysis of prosthetic complications of implant-supported fixed partial dentures after an observation period of 5 to 10 years10.11607/jomi.2999 ↗
38. Evaluation of interface characterization and adhesion of glass ceramics to commercially pure titanium and gold alloy after thermal- and mechanical-loading10.1016/j.dental.2008.07.002 ↗
39. Titanium for prosthodontic applications: a review of the literature
40. Computational modeling of elastic constants as a function of temperature and composition in Zr–Nb alloys10.1016/j.calphad.2014.11.003 ↗
41. Complication and failure rates with implant-supported fixed dental prostheses and single crowns: a 10-year retrospective study10.1111/cid.12066 ↗
42. The influence of Goldbonder and pre-heat treatment on the adhesion of titanium alloy and porcelain10.1111/j.1365-2842.2004.01408.x ↗
43. Comparison of the bond compatibility of titanium and a NiCr alloy to dental porcelain10.1016/S0300-5712(98)00045-1 ↗
44. Formation of white oxide layer on Zr–14Nb alloy using thermal treatment10.4012/dmj.2013-323 ↗
45. Initial hemocompatibility studies of titanium and zirconium alloys: prekallikrein activation, fibrinogen adsorption, and their correlation with surface electrochemical properties10.1002/(SICI)1097-4636(199609)32:1<77::AID-JBM9>3.0.CO;2-M ↗
46. Effect of titanium preoxidation on wrought pure titanium to ceramic bond strength10.1016/S0022-3913(13)60025-6 ↗
47. Microstructure, corrosion behavior and cytotoxicity of Zr–Nb alloys for biomedical application10.1016/j.msec.2012.02.002 ↗
48. Bond strength and interfacial characterization of eight low fusing porcelains to cp Ti10.1016/j.dental.2009.11.004 ↗