A comparative study of the mechanical behaviour of thermally oxidised commercially pure titanium and zirconium
Source abstract
Abstract
The objective of this study is to compare the mechanical behaviour of thermally oxidised commercially pure titanium (CP-Ti) and commercially pure zirconium (CP-Zr). For this purpose, these two bio-metals were thermally oxidised under the same condition (650°C for 6h) and the oxidised specimens were characterised using various analytical and experimental techniques, including oxygen uptake analysis, layer thickness and hardness measurements, scratch tests, dry sliding friction and wear tests and tribocorrosion tests in Ringer's solution. The results show that under the present thermal oxidation condition, 4 times more oxygen is introduced into CP-Zr than into CP-Ti and the oxide layer produced on CP-Zr is nearly 6 times thicker than that on CP-Ti. Thermally oxidised CP-Zr possesses a higher hardness, a deeper hardening depth and better scratch resistance than thermally oxidised CP-Ti. Under dry sliding and tribocorrosion conditions, thermally oxidised CP-Zr also possesses much better resistance to material removal and a higher load bearing capacity than thermally oxidised CP-Ti. Thus, thermally oxidised Zr possesses much better mechanical behaviour than thermally oxidised Ti.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced materials and composites · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Effect of oxidation time on the tribological behaviour of thermally oxidized commercially pure zirconium under dry sliding conditions10.1016/j.surfcoat.2016.11.070 ↗
2. Sliding wear resistance of oxide layers formed on a titanium surface during thermal oxidation10.1016/j.wear.2016.03.007 ↗
3. Unlubricated sliding friction and wear characteristics of thermally oxidized commercially pure titanium10.1016/j.wear.2013.09.020 ↗
4. Realising the potential of duplex surface engineering10.1016/S0301-679X(98)00015-2 ↗
5. Surface characterization and mechanical property evaluation of thermally oxidized Ti-6Al-4V10.1016/j.matchar.2008.12.014 ↗
6. Bloyce, A., 1998. Surface engineering of titanium alloys for wear protection. Proc. IMechE Part J: J. Eng. Tribol., 212, pp. 467–476.10.1243/1350650981542263 ↗
7. Surface modification of titanium alloys for combined improvements in corrosion and wear resistance10.1016/S0257-8972(98)00580-5 ↗
8. Titanium and zirconium based alloys modified by intensive plastic deformation and nitrogen ion implantation for biocompatible implants10.1016/j.jmbbm.2011.05.034 ↗
9. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
10. Corrosion-wear mechanisms of hard coated austenitic 316L stainless steel10.1016/S0043-1648(03)00559-3 ↗
11. Designer surfaces for titanium components
12. Abrasion resistance of oxidized zirconium in comparison with CoCrMo and titanium nitride coatings for artificial knee joints10.1002/jbm.b.31581 ↗
13. Biocompatibility of Ti-alloys for long-term implantation10.1016/j.jmbbm.2012.11.014 ↗
14. Oxidized zirconium: a potentially longer lasting hip implant10.1016/j.matdes.2004.08.014 ↗
15. Effect of thermal oxidation on corrosion and corrosion-wear behaviour of a Ti-6Al-4V alloy10.1016/j.biomaterials.2003.10.009 ↗
16. Improved wear resistance of zirconium by enhanced oxide films10.1016/0040-6090(84)90205-0 ↗
17. A model for stresses, crack generation and facture toughness calculation in scratched TiN-coated steel surfaces10.1016/S0043-1648(02)00297-1 ↗
18. Hunter, G., Asgian, C.M., Hines, G.I., 2002. Methods of Surface Hardening Zirconium Alloys and Resulting Products. United States Patent, US 6447550.
19. Oxidized zirconium femoral component for TKA: a follow-up note of a previous report at a minimum 10 years10.1016/j.knee.2014.04.005 ↗
20. Ceramic conversion treatment of zirconium alloys to combat wear10.1179/026708409X12450792800079 ↗
21. Modelling the tribo-corrosion interaction in aqueous sliding conditions10.1016/S0301-679X(02)00058-0 ↗
22. Thick rutile layer on titanium for tribological applications10.1016/j.triboint.2005.08.004 ↗
23. Thermal oxidation of Ti6Al4V alloy: Microstructural and electrochemical characterization10.1016/j.matchemphys.2009.09.007 ↗
24. Electrochemical methods in tribocorrosion: a critical appraisal10.1016/S0013-4686(01)00679-X ↗
25. Bioinertness and fracture toughness evaluation of the monoclinic zirconia surface film of OxiniumTM femoral head by Raman and cathodoluminescence spectroscopy10.1016/j.jmbbm.2013.10.026 ↗
26. Thermal oxidation of medical Ti6Al4V blasted with ceramic particles: effects on the microstructure, residual stresses and mechanical properties10.1016/j.jmbbm.2015.09.032 ↗
27. Oxidation of zirconium in air10.2320/matertrans1960.3.203 ↗
28. Triboelectrochemical techniques and interpretation methods in tribocorrosion: a comparative evaluation10.1016/j.triboint.2007.11.003 ↗
29. Recent metallic materials for biomedical applications10.1007/s11661-002-0109-2 ↗
30. Tribological evaluation of oxidized zirconium using an articular cartilage counterface: a novel material for potential use in hemiarthroplasty10.1016/S0142-9612(96)00152-4 ↗
31. Physical characterization of a new composition of oxidized zirconium-2.5 wt% niobium produced using a two step process for biomedical applications10.1016/j.apsusc.2011.02.014 ↗
32. An electron microscope study of breakaway oxidation of zirconium at 623 K10.1016/0022-3115(80)90232-9 ↗
33. Electrochemical techniques for studying tribocorrosion processes10.1016/S0043-1648(03)00556-8 ↗
34. Thermal oxidation behaviour and tribological properties of textured TC4 surface: Influence of thermal oxidation temperature and time10.1016/j.triboint.2015.10.013 ↗
35. Tribocorrosion behaviour of AISI 304 stainless steel in 0.5 M NaCl solution10.1016/j.matchemphys.2011.03.063 ↗
36. Breakaway phenomena in the oxidation of zirconium at 850 and 950 °C10.1016/S0010-938X(65)90471-3 ↗
37. Influence of thermal oxidation temperature on the microstructural and tribological behavior of Ti6Al4V alloy10.1016/j.surfcoat.2014.01.004 ↗
38. The improvement of wettability, biotribological behavior and corrosion resistance of titanium alloy pretreated by thermal oxidation10.1016/j.triboint.2014.06.008 ↗
39. A model for compressive coating stresses in the scratch adhesion test10.1016/S0257-8972(01)01130-6 ↗