journal article·2017-11Open access

Quantifying the mode II critical strain energy release rate of borate bioactive glass coatings on Ti6Al4V substrates

A. Matinmanesh, Y. Li, O. Clarkin, P. Zalzal, E.H. Schemitsch, M.R. Towler, M. Papini

Abstract

Bioactive glasses have been used as coatings for biomedical implants because they can be formulated to promote osseointegration, antibacterial behavior, bone formation, and tissue healing through the incorporation and subsequent release of certain ions. However, shear loading on coated implants has been reported to cause the delamination and loosening of such coatings. This work uses a recently developed fracture mechanics testing methodology to quantify the critical strain energy release rate under nearly pure mode II conditions, GIIC, of a series of borate-based glass coating/Ti6Al4V alloy substrate systems. Incorporating increasing amounts of SrCO3 in the glass composition was found to increase the GIIC almost twofold, from 25.3 to 46.9J/m2. The magnitude and distribution of residual stresses in the coating were quantified, and it was found that the residual stresses in all cases distributed uniformly over the cross section of the coating. The crack was driven towards, but not into, the glass/Ti6Al4V substrate interface due to the shear loading. This implied that the interface had a higher fracture toughness than the coating itself.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (87)

Show source-provided references
1. Fracture R-curve of a toughened epoxy adhesive as a function of irreversible degradation10.1016/j.msea.2010.04.099 ↗
2. Prediction of environmental degradation of closed adhesive joints using data from open-faced specimens10.1016/j.compstruct.2011.09.017 ↗
3. Characterization and prediction of fracture properties in hygrothermally degraded adhesive joints: an open-faced approach10.1080/01694243.2012.730028 ↗
4. American Society of Mechanical Engineers, 2015. ASME - STANDARDS - Surface Texture (Surface Roughness, Waviness, and Lay) [Internet]. 2009 [cited Dec 7]. Available from: 〈https://www.asme.org/products/codes-standards/b461-2009-surface-texture-surface-roughness〉.
5. Anderson · 2005 · 640
6. A critical evaluation of indentation techniques for measuring fracture toughness: I, Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
7. ASTM, 2015. C1624 Standard Test Method for Adhesion Strength and Mechanical Failure Modes of Ceramic Coatings by Quantitative Single Point ScratchTesting. A.S.T.M International.
8. ASTM International, 2012. ASTM D3433-99 Standard Test Method for Fracture Strength in Cleavage of Adhesives in Bonded Metal Joints. In. Available from: 〈http://www.skygeek.com/j-b-weld-8265-cold-weld-compound.html〉.
9. ASTM International, 2015. ASTM F1147 Tension Testing for Calcium Phosphate and Metallic Coatings. In 2011 [cited December 7]. Available from: 〈http://www.testresources.net/applications/standards/astm/astm-f1147-tension-testing-for-calcium-phosphate-and-metallic-coatings〉.
10. ASTM International, 2017. ASTM E228 Standard Test Method for Linear Thermal Expansion of Solid Materials with a Push-Rod Dilatometer. In 2016 [cited Mar20]. Available from: 〈https://compass.astm.org/download/E228.15223.pdf〉.
11. Mode II stress-intensity factors for cracked wood beams10.1016/0013-7944(77)90029-7 ↗
12. Coefficient of thermal expansion of bioactive glasses: available literature data and analytical equation estimates10.1016/j.ceramint.2011.05.048 ↗
13. Measurement of adhesion for thermally sprayed materials10.1163/156856193X00088 ↗
14. Indentation method for determining the macroscopic fracture energy of brittle bimaterial interfaces10.1111/j.1151-2916.1992.tb08195.x ↗
15. The determination of the mode II adhesive fracture resistance, GIIC, of structural adhesive joints: an effective crack length approach10.1016/j.engfracmech.2004.08.007 ↗
16. Bioactive glass–ceramic coated titanium implants prepared by electrophoretic deposition10.1016/j.msec.2012.06.013 ↗
17. Influence of substrate surface topography on the critical normal force in scratch adhesion testing of TiN-coated steels10.1016/0257-8972(92)90046-D ↗
18. Biomaterial developments for bone tissue engineering10.1016/S0142-9612(00)00102-2 ↗
19. Residual stresses and cracking in brittle solids bonded with a thin ductile layer10.1016/0001-6160(88)90305-7 ↗
20. Mode II interlaminar fracture of graphite/epoxy and graphite/PEEK10.1177/073168448600500302 ↗
21. A review of the methods for the evaluation of coating-substrate adhesion10.1016/0921-5093(91)90482-3 ↗
22. Experimental coating defects in hydroxylapatite-coated implants10.1097/00003086-199104000-00033 ↗
23. Slightly curved or kinked cracks10.1007/BF00012619 ↗
24. Antibacterial coatings for medical devices based on glass polyalkenoate cement chemistry10.1007/s10856-008-3519-x ↗
25. Biofilm inhibitory coatings formulated from glass polyalkenoate cement chemistry: an evaluation of their adhesive nature10.1007/s10853-009-3344-8 ↗
26. Zinc and silver glass polyalkenoate cements: an evaluation of their antibacterial nature
27. The response of Pseudomonas aeruginosa biofilm to the presence of a glass polyalkenoate cement formulated from a silver containing glass10.1007/s10853-010-4945-y ↗
28. Transformation of borate glasses into biologically useful materials
29. Plasma sprayed coatings of hydroxylapatite10.1002/jbm.820211203 ↗
30. Donachie · 2000 · 390
31. Effects of non-planarity on the mixed mode fracture resistance of bimaterial iiinterfaces10.1016/0001-6160(89)90017-5 ↗
32. On crack path selection and the interface fracture energy in bimaterial systems10.1016/0001-6160(89)90197-1 ↗
33. Mixed-mode fracture characterization of adhesive joints10.1016/0266-3538(94)90052-3 ↗
34. Residual stresses and stress intensity factors for vickers indentation cracks in glass derived from COD measurements10.1002/adem.200400121 ↗
35. Crack path selection in a brittle adhesive layer10.1016/0020-7683(91)90069-R ↗
36. Friedrich · 2012 · 686
37. Bonding of bone to apatite-coated implants10.1302/0301-620X.70B1.2828374 ↗
38. Methods for determining the mode I and mode II fracture toughness of glass using thermal stresses10.1115/1.2903301 ↗
39. Glass-based coatings for titanium implant alloys10.1002/(SICI)1097-4636(19990915)46:4<549::AID-JBM13>3.0.CO;2-M ↗
40. Bioactive glass coatings with hydroxyapatite and Bioglass particles on Ti-based implants. 1. Processing10.1016/S0142-9612(99)00131-3 ↗
41. Novel bioactive functionally graded coatings on Ti6Al4V10.1002/1521-4095(200006)12:12<894::AID-ADMA894>3.0.CO;2-4 ↗
42. Bioactive glass coatings with hydroxyapatite and Bioglass particles on Ti-based implants. 1. Processing10.1016/S0142-9612(99)00131-3 ↗
43. Thermal analysis of amorphous phases in hydroxyapatite coatings10.1111/j.1151-2916.1998.tb02301.x ↗
44. Reaction of sodium calcium borate glasses to form hydroxyapatite10.1007/s10856-007-3053-2 ↗
45. Comparison of bone–implant interface shear strength of solid hydroxyapatite and hydroxyapatite-coated titanium implants10.1002/jbm.820270502 ↗
46. Hench · 1993 · 406
47. Impact of doping on the mechanical properties of acicular mullite10.1016/j.jeurceramsoc.2013.02.006 ↗
48. Kinetics and mechanisms of the conversion of silicate (45S5), borate, and borosilicate glasses to hydroxyapatite in dilute phosphate solutions10.1007/s10856-006-9220-z ↗
49. Hutchinson J.W., Suo Z., 1991. Mixed Mode Cracking in Layered Materials. In: Wu JWH and TY, editor. Advances in Applied Mechanics [Internet]. Elsevier [cited 2015 Dec 23]. p. 63–191. Available from: 〈http://www.sciencedirect.com/science/article/pii/S0065215608701649〉.10.1016/S0065-2156(08)70164-9 ↗
50. Analysis of stresses and strains near the end of a crack traversing a plate10.1115/1.4011547 ↗
51. JB Weld epoxies [Internet]. Available from: 〈www.JBweld.com〉.
52. Novel bioactive materials with different mechanical properties10.1016/S0142-9612(03)00044-9 ↗
53. Indentation techniques for evaluating the fracture toughness of biomaterials and hard tissues10.1016/j.jmbbm.2008.10.008 ↗
54. Behavior of indentation cracks near free surfaces and interfaces10.1007/BF00047064 ↗
55. Elastic/plastic indentation damage in ceramics: the median/radial crack system10.1111/j.1151-2916.1980.tb10768.x ↗
56. Characteristics of plasma-sprayed bioactive glass coatings on Ti-6A1–4V alloy: an in vitro study10.1016/0257-8972(95)02463-8 ↗
57. Scratch test for coating/substrate systems – A literature review10.1179/cmq.2007.46.2.155 ↗
58. Characterization and fracture property of different strontium-containing borate-based glass coatings for Ti6Al4V substrates10.1016/j.jnoncrysol.2016.12.010 ↗
59. Bioactive borate glass scaffold for bone tissue engineering10.1016/j.jnoncrysol.2007.10.003 ↗
60. Structure and properties of hydroxyapatite-bioactive glass composites plasma sprayed on Ti6Al4V10.1007/BF00122397 ↗
61. Bioactive glass coatings for orthopedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
62. Plasma-sprayed hydroxyapatite+titania composite bond coat for hydroxyapatite coating on titanium substrate10.1016/j.biomaterials.2003.10.092 ↗
63. Quantitative evaluation of the adhesion of bioactive glasses onto Ti6Al4V substrates10.1016/j.matdes.2016.02.086 ↗
64. Equivalent crack based analyses of ENF and ELS tests10.1016/j.engfracmech.2007.03.005 ↗
65. O’Brien, T.K., Murri, G.B., Salpekar, S.A., 1989. Interlaminar Shear Fracture Toughness and Fatigue Thresholds for Composite Materias. ASTM International; Composite materials: Fatigue and fracture, second volume.10.1520/STP10418S ↗
66. Bioactive borate glass coatings for titanium alloys10.1007/s10856-008-3419-0 ↗
67. Measurement of mechanical properties by ultra-low load indentation10.1016/S0921-5093(98)00724-2 ↗
68. Protter · 1988 · 990
69. Silica-based and borate-based, titania-containing bioactive coatings characterization: critical strain energy release rate, residual stresses, hardness, and thermal expansion10.3390/jfb7040032 ↗
71. Elastic modulus and fracture toughness of ternary PbO-ZnO-B2O3 glasses10.1111/j.1151-2916.1982.tb10369.x ↗
72. Silva · 2012 · 558
73. Elastic properties of substituted-45S5 bioactive glasses and glass ceramics
74. Major damage mechanisms during scratch and wear testing of hard coatings on hard substrates10.1016/0040-6090(89)90524-5 ↗
75. Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings: a review10.1002/jbm.1056 ↗
76. Prestandardization study on mode II interlaminar fracture toughness test for cfrp in japan10.1016/0010-4361(95)93669-B ↗
77. The effect of surface macrotexture and hydroxylapatite coating on the mechanical strengths and histologic profiles of titanium implant materials10.1002/jbm.820211205 ↗
78. Mechanical properties of bioactive glasses, glass-ceramics and composites10.1243/0954411981533908 ↗
79. The shear strength and the failure mode of plasma-sprayed hydroxyapatite coating to bone: the effect of coating thickness10.1002/jbm.820271012 ↗
80. Changes in phases and crystallinity of plasma-sprayed hydroxyapatite coatings under heat treatment: a quantitative study10.1002/jbm.820291204 ↗
81. Use of end-loaded-split (ELS) test to study stable fracture behaviour of composites under mode II loading10.1016/S0263-8223(96)00066-9 ↗
82. Elastic moduli and behaviors of metallic glasses10.1016/j.jnoncrysol.2005.03.024 ↗
83. Hardness and elastic properties of Bi2O3-based glasses10.1023/A:1017973830342 ↗
84. Welsch · 1993 · 1206
85. Measurement of adhesive joint fracture properties as a function of environmental degradation10.1016/S0143-7496(98)00028-1 ↗
86. Evaluation of Ti implants coated with Ag-containing borate bioactive glass for simultaneous eradication of infection and fracture fixation in a rabbit tibial model10.1557/jmr.2012.375 ↗
87. An experimental investigation of residual stresses in an epoxy–steel laminate10.1016/j.ijadhadh.2005.07.006 ↗