Aim To evaluate wear and marginal quality of resin composite restorations over eight years of clinical service in vivo. Methods 30 patients received 68 resin composite restorations (36 Grandio, 32 Tetric Ceram) in the course of a prospective clinical trial. 3-D evaluation of 36 selected teeth involving 144 epoxy replicas was carried out using a special 3-D scanning device with an accuracy of U1=2.5+L/350 μm; U3=3+L/300 μm. In vivo replicas were sputter-coated with gold and examined under a SEM at 200× magnification. Marginal integrity between resin composite and enamel was expressed as a percentage of the entire judgeable margin length. Results During the clinical 8-year observation period, wear significantly increased in the restored areas as well as in OCAs. RBCs under investigation showed no significant differences regarding wear (p>0.05). Localization of the restorations (premolar vs. molar or upper vs. lower) did not show a significant influence on wear rates (p>0.05). Clinically, by SEM, and by 3-D scanning distinct changes of worn contours on enamel and RBC were visible. Quantitative margin analysis revealed a change of perfect margins (58% at baseline vs. 14% at 8 years), positive step formations (15% at baseline vs. 10% at 8 years), and negative step formations (20% at baseline vs. 71% at 8 years) over time (p<0.001). Regarding the portion of gap-free margins (baseline vs. 2 years) and total margin length (baseline to 8 years), Grandio showed lower values (Mann-Whitney U-test; p<0.05). The portion of negative step formations was lower for Tetric Ceram at baseline (Mann-Whitney-U test; p<0.05). Conclusions After eight years of clinical service, neither wear nor marginal quality was a critical factor for estimation and survival of extended posterior resin composite restorations.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Marginal quality of posterior microhybrid resin composite restorations applied using two polymerisation protocols: 5-year randomised split mouth trial10.1016/j.jdent.2013.02.009 ↗
2. Localized and generalized simulated wear of resin composites10.2341/13-155-L ↗
3. Wear rates of resin composites10.2341/12-112-L ↗
4. Comparison of laboratory and clinical wear rates of resin composites
5. Correlation of clinical performance with ‘in vitro tests’ of restorative dental materials that use polymer-based matrices10.1016/j.dental.2011.08.594 ↗
6. Protection hypothesis for composite wear10.1016/0109-5641(92)90105-L ↗
7. Confirmation of Leinfelder clinical wear standards10.1016/0109-5641(94)90016-7 ↗
8. Evaluation of composite wear with a new multi-mode oral wear simulator10.1016/S0109-5641(96)80026-1 ↗
9. Factors effecting dental composite wear in vitro10.1002/(SICI)1097-4636(199724)38:4<303::AID-JBM2>3.0.CO;2-S ↗
10. Wear properties of a novel resin composite compared to human enamel and other restorative materials10.2341/13-108-L ↗
11. Wear of a dental composite in an artificial oral environment: a clinical correlation10.1002/jbm.b.32801 ↗
12. Resin-based composite performance: are there some things we can׳t predict?10.1016/j.dental.2012.06.013 ↗
13. In vitro evaluation of the marginal degradation of dental composites under simulated occlusal loading10.1016/S0109-5641(99)00045-7 ↗
14. Marginal integrity: is the clinical performance of bonded restorations predictable in vitro?
15. Selective enamel etching reconsidered: better than etch-and-rinse and self-etch?
16. Luting of ceramic inlays in vitro: marginal quality of self-etch and etch-and-rinse adhesives versus self-etch cements10.1016/j.dental.2007.04.003 ↗
17. Nanohybrid vs. fine hybrid composite in extended class II cavities: 8-year results10.1007/s00784-013-0957-8 ↗
18. Self-etch vs etch-and-rinse adhesives: effect of thermo-mechanical fatigue loading on marginal quality of bonded resin composite restorations10.1016/j.dental.2004.07.005 ↗
19. Fatigue behavior of dental resin composites: flexural fatigue in vitro versus 6 years in vivo10.1002/jbm.b.32651 ↗
20. Abrasive wear and surface roughness of contemporary dental composite resin10.4012/dmj.2013-339 ↗
21. Systematic reviews: I. The correlation between laboratory tests on marginal quality and bond strength. II. The correlation between marginal quality and clinical outcome
22. Clinical relevance of tests on bond strength, microleakage and marginal adaptation10.1016/j.dental.2012.07.158 ↗
23. Round robin test: wear of nine dental restorative materials in six different wear simulators – supplement to the round robin test of 200510.1016/j.dental.2010.09.003 ↗
24. Marginal adaptation in vitro and clinical outcome of Class V restorations10.1016/j.dental.2008.11.004 ↗
25. FDI World Dental Federation: clinical criteria for the evaluation of direct and indirect restorations-update and clinical examples10.1007/s00784-010-0432-8 ↗
26. Hickel · J. Adhes. Dent. · 2007 · 9 · S121
27. Texture of composite resins exposed to two- and three-body wear in vitro10.5005/jp-journals-10024-1521 ↗
28. A regression analysis of filler particle content to predict composite wear10.1016/S0022-3913(97)70208-7 ↗
29. Two- and three-body wear of composite resins10.1016/j.dental.2012.09.008 ↗
30. Antagonist enamel wears more than ceramic inlays10.1177/154405910608501206 ↗
31. Are resin composites suitable replacements for amalgam? A study of two-body wear
32. In vitro wear device for determining posterior composite wear10.14219/jada.archive.1999.0406 ↗
33. Chewing pressure vs. wear of composites and opposing enamel cusps10.1177/00220345920710081201 ↗
34. Buonocore memorial lecture. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition
35. The effect of 1% metronidazole gel in routine maintenance of persistent furcation involvement in human beings10.1902/jop.1989.60.12.699 ↗
36. Age of failed restorations: a deceptive longevity parameter10.1016/j.jdent.2010.12.008 ↗
37. 12-year survival of composite vs. amalgam restorations10.1177/0022034510376071 ↗
38. A retrospective clinical study on longevity of posterior composite and amalgam restorations10.1016/j.dental.2005.11.036 ↗
39. Longevity of posterior composite restorations: a systematic review and meta-analysis10.1177/0022034514544217 ↗
40. Internal corrosion in dental composite wear10.1002/1097-4636(2000)53:4<371::AID-JBM11>3.0.CO;2-N ↗
41. The effects of alcoholic beverages on composite wear10.1016/S0109-5641(99)00088-3 ↗
42. The effect of water on polymer matrix and composite wear10.1016/0109-5641(94)90015-9 ↗
43. Effects of filler size, water, and alcohol on hardness and laboratory wear of dental composites10.1080/00016350410005555 ↗
44. Pooling of long term clinical wear data for posterior composites
45. Wear of dental resin composites: insights into underlying processes and assessment methods – a review10.1002/jbm.b.10563 ↗
46. Clinical recipe for durable dental bonding: why and how?
47. An accurate and simple method for the measurement of dental composite wear10.1111/j.1365-2842.1996.tb00884.x ↗
48. Visual versus mechanical wear measurement of dental composite resin10.1111/j.1365-2842.1996.tb00885.x ↗