journal article·2019-03

Crack initiation from a clinically relevant notch in a highly-crosslinked UHMWPE subjected to static and cyclic loading

Abhi Sirimamilla, Clare M. Rimnac

Publisher page

Abstract

Crosslinked Ultra High Molecular Weight Polyethylene (UHMWPE), which is used as a bearing material in total joint replacement components, is subjected to static and cyclic loads in vivo. Resistance to crack initiation from a notch as a function of static and cyclic loads is not well understood for crosslinked UHMWPE. This study estimated the resistance of crosslinked UHMWPE (crosslinked with 100 kGy gamma radiation and remelted to extinguish free radicals) to crack initiation for a clinically relevant notch under both static and cyclic loading conditions. For cyclic loading, four frequencies were applied with a sine waveform and two frequencies were applied with a square waveform to independently estimate the effect of frequency and rate of loading on crack initiation. Crack initiation time and cycles to crack initiation were determined. Crack initiation time for fatigue loading conditions was substantially lower compared to static loading conditions. Crack initiation time decreased with an increase in test frequency. A square wave resulted in shorter crack initiation time compared to a sine wave. The results suggest that crosslinked UHMWPE is more resistant to crack initiation from a notch under static loading conditions compared to fatigue loading conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Orthopedic Infections and Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Notch fatigue of ultrahigh molecular weight polyethylene (UHMWPE) used in total joint replacements10.1016/j.jmbbm.2016.02.014 ↗
2. The porous-coated anatomic total hip prosthesis: failure of the metal-backed acetabular component10.2106/00004623-199605000-00016 ↗
3. ASTM, 2001. E1820-01. Standard Test Method for Measurement of Fracture Toughness.
4. Total hip arthroplasty using highly cross-linked polyethylene in patients younger than 50 years with minimum 10-year follow-up10.1016/j.arth.2012.12.005 ↗
5. Study of fatigue resistance of chemical and radiation crosslinked medical grade ultrahigh molecular weight polyethylene10.1002/(SICI)1097-4636(19990915)46:4<573::AID-JBM16>3.0.CO;2-A ↗
6. Compression and tension fatigue resistance of medical grade ultra high molecular weight polyethylene: the effect of morphology, sterilization, aging and temperature10.1016/S0032-3861(99)00199-8 ↗
7. The Effect of conformity, thickness, and material on stresses in ultrahigh molecular-weight components for total joint replacement10.2106/00004623-198668070-00010 ↗
8. Catastrophic failure of the polyethylene liner of uncemented acetabular components10.1302/0301-620X.76B4.8027143 ↗
9. Cracking and impingement in ultra-high-molecular-weight polyethylene acetabular liners10.1016/j.arth.2005.05.001 ↗
10. Effects of loading history on fatigue crack-growth in high-density polyethylene and toughened poly(Methyl Methacrylate)10.1002/pen.760270203 ↗
11. Fracture of the polyethylene tibial post in a NexGen posterior-stabilized knee prosthesis10.1016/j.arth.2004.04.013 ↗
12. Mechanisms of failure of modular prostheses10.1097/00003086-199212000-00017 ↗
13. Fatigue crack propagation behavior of ultrahigh molecular weight polyethylene10.1002/jor.1100020202 ↗
14. Norman E. Dowling., 2012. Mechanical Behavior of Materials (4th edition). ISBN-13: 978-0131395060.
15. A prospective, randomized study of cross-linked and non-cross-linked polyethylene for total hip arthroplasty at 10-year follow-up10.1016/j.arth.2012.03.048 ↗
16. Peak stress intensity dictates fatigue crack propagation in UHMWPE10.1016/j.polymer.2007.04.006 ↗
17. Crack propagation resistance is similar under static and cyclic loading in crosslinked UHMWPE: a pilot study10.1007/s11999-010-1712-y ↗
18. Clinical fracture of cross-linked UHMWPE acetabular liners10.1016/j.biomaterials.2009.07.013 ↗
19. The John Charnley Award: highly crosslinked polyethylene in total hip arthroplasty decreases long-term wear: a double-blind randomized trial10.1007/s11999-014-3735-2 ↗
20. Grellmann · 2001
21. Does vitamin E-stabilized ultrahigh-molecular-weight polyethylene address concerns of cross-linked polyethylene in total knee arthroplasty?10.1016/j.arth.2011.03.024 ↗
22. Recurrent dislocation after revision total hip replacement with a large prosthetic femoral head. A case report10.2106/00004623-200404000-00025 ↗
23. Highly crosslinked polyethylene does not reduce aseptic loosening in cemented THA 10-year findings of a randomized study., Clinical10.1007/s11999-012-2400-x ↗
24. Catastrophic failure of an acetabular total hip arthroplasty component mimicking a posterior dislocation10.1016/j.artd.2016.09.010 ↗
25. Krista Parran, V.N., Rimnac, C., 2016. Crack initiation resistance from a Blunt Notch in a hindered phenol antioxidant UHMWPE. In: Proceedings of the ORS Annual Meeting.
26. Kurtz · 2015
27. Thermomechanical behavior of virgin and highly crosslinked ultra-high molecular weight polyethylene used in total joint replacements10.1016/S0142-9612(02)00102-3 ↗
28. Polyethylene wear and rim fracture in total disc arthroplasty10.1016/j.spinee.2006.05.012 ↗
29. Lach, R., Estimation of the resistance against stable crack initiation and unstable crack propagation using R-curnes and stability assessment diagrams in ductile polymeric ABS-materials. In: Proceedings of the 13th European Conference on Fracture (ECF 13), San Sebastian, Spain, pp. 1–8.
30. Dislocation after total hip arthroplasty: risk factors and treatment options10.3944/AOTT.2013.2978 ↗
31. Matlab Corporation. Needham Massachusetts.
32. Fracture of the polyethylene tibial post in a posterior cruciate-substituting total knee arthroplasty mimicking patellar clunk syndrome: a report of 5 cases10.1016/S0883-5403(03)00333-4 ↗
33. Comparative fatigue behavior and toughness of remelted and annealed highly crosslinked polyethylenes10.1002/jbm.b.30807 ↗
34. A rational analytical theory of fatigue
35. Pelvic muscle and acetabular contact forces during gait10.1016/S0021-9290(97)00041-9 ↗
36. Mechanical failures in total hip replacement requiring reoperation10.2106/00004623-197961010-00006 ↗
37. Thermomechanical aspects of dynamic crack initiation10.1023/A:1018616917384 ↗
38. Measurements of Ultra High Molecular-Weight Polyethylene10.1002/pen.760282403 ↗
39. Fatigue of polymers10.1007/BF02265215 ↗
40. Peak stress intensity factor governs crack propagation velocity in crosslinked ultrahigh-molecular-weight polyethylene10.1002/jbm.b.32850 ↗
41. Application of viscoelastic fracture model and non-uniform crack initiation at clinically relevant notches in crosslinked UHMWPE10.1016/j.jmbbm.2012.07.008 ↗
42. Viscoplastic crack initiation and propagation in crosslinked UHMWPE from clinically relevant notches up to 0.5mm radius10.1016/j.jmbbm.2017.08.030 ↗
43. Notched stress-strain behavior of a conventional and a sequentially annealed highly crosslinked UHMWPE10.1016/j.biomaterials.2008.08.010 ↗
44. Rim cracking of the cross-linked longevity polyethylene acetabular liner after total hip arthroplasty10.2106/00004623-200710000-00016 ↗
45. Evaluation of J-initiation fracture toughness of ultra high molecular weight polyethylene used in total joint replacements10.1016/j.polymertesting.2008.03.007 ↗
46. Static fracture resistance of ultra high molecular weight polyethylene using the single specimen normalization method10.1016/j.polymertesting.2007.11.010 ↗
47. Williams · 1984
48. Anomalous fracture behaviour in polyethylenes under fatigue and constant load10.1007/BF01151528 ↗
49. The relative influences of molecular structure on brittle fracture by fatigue and under constant load in polyethylenes10.1002/pen.10606 ↗