Effect of microwave crystallization on the wear resistance of reinforced glass-ceramics
Source abstract
Abstract
This study compared the wear resistance of different reinforced glass-ceramics crystalized by conventional or microwave firing. The wear rate of three ceramics [one lithium disilicate ceramic (LD): IPS e.max CAD - Ivoclar Vivadent; and two zirconia reinforced lithium silicates: Suprinity - VITA Zahnfabrik (ZLS1) and Celtra Duo - Dentsply (ZLS2)] crystallized by conventional (c) or microwave (mw) firing protocols were collected according to the contact- [two-body (n = 20/gr)] and contact-free wear tests [three-body (n = 20/gr)]. After wear tests performed on ACTA wear machine, mean surface roughness (Ra) and Scanning Electron Microscopy (SEM) analyzes were performed to evaluate the surface alterations. The wear and roughness data (in μm) were evaluated using two-way ANOVA and Tukey post-hoc test (α = 0.05). Two-body wear test revealed that ZLS1 (1.30 ± 1.79)A showed higher wear rate than LD (0.79 ± 2.15)B and ZLS2 (0.85 ± 0.94)B, regardless the crystallization approach. For three-body test, conventional crystallization (0.62 ± 0.4)A showed higher wear rates than microwave (0.22 ± 0.71)B; while the type of ceramic was not significant. The crystallization protocol (p < 0.001) and ceramic material (p = 0.001) affected the surface roughness in the three-body; whereas the two-body test, only the crystallization protocol (p = 0.046). SEM analysis showed a similar and smother surface morphology for LD and ZLS2 compared to ZLS1. Conventional crystallization showed materials more prone to wear than the microwave, in the presence of food bolus. Therefore, the microwave crystallization can be suggested as an alternative to improve the evaluated glass-ceramics wear resistance.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental Implant Techniques and Outcomes · Dental materials and restorations · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Microwave processing of ceramics10.1016/S1359-0286(98)80011-9 ↗
2. Applying microwave technology to sintering dental zirconia10.1016/S0022-3913(12)60181-4 ↗
3. Influence of heat‐treatment protocols on mechanical behavior of lithium silicate dental ceramics10.1111/ijac.13257 ↗
4. Assessment of wear facets produced by the ACTA wear machine10.1016/j.jdent.2015.12.003 ↗
5. Wear properties of a novel resin composite compared to human enamel and other restorative materials10.2341/13-108-L ↗
6. Monolithic ceramics: effect of finishing techniques on surface properties, bacterial adhesion and cell viability10.2341/17-011-L ↗
7. Three-body wear effect on different CAD/CAM ceramics staining durability10.1016/j.jmbbm.2019.103579 ↗
8. Occlusal wear simulation with the ACTA wear machine10.1016/0300-5712(94)90167-8 ↗
9. The influence of surface roughness on porcelain strength10.1016/S0109-5641(00)00030-0 ↗
10. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
11. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
12. Wear resistance of a pressable low-fusing ceramic opposed by dental alloys10.1016/j.jmbbm.2013.12.018 ↗
13. The effects of enamel wear on the metal-porcelain interface10.1016/0022-3913(83)90198-1 ↗
14. Two-body wear of resin and ceramic denture teeth in comparison to human enamel10.1016/j.dental.2007.04.012 ↗
15. Erosion caused by gastroesophageal reflux: diagnostic considerations10.1111/j.1532-849X.1997.tb00108.x ↗
16. Effect of microstructure on the mechanical properties of lithium disilicate glass-ceramics10.1016/j.jmbbm.2018.02.032 ↗
17. Round robin test: wear of nine dental restorative materials in six different wear simulators - supplement to the round robin test of 200510.1016/j.dental.2010.09.003 ↗
18. Wear of three dental composites under different testing conditions10.1046/j.1365-2842.2002.00878.x ↗
19. Enamel wear caused by three different restorative materials10.1016/S0022-3913(05)80319-1 ↗
20. International Organization for Standardization · 2001
21. An in vitro investigation into the wear effects of selected restorative materials on dentine10.1111/j.1365-2842.1995.tb00784.x ↗
22. Effect of surface roughness of porcelain on adhesion of bacteria and their synthesizing glucans10.1067/mpr.2000.107442 ↗
23. Comparison of the optical properties of pre-colored dental monolithic zirconia ceramics sintered in a conventional furnace versus a microwave oven10.4047/jap.2017.9.5.394 ↗
24. Effects of the sintering conditions of dental zirconia ceramics on the grain size and translucency10.4047/jap.2013.5.2.161 ↗
25. Quantitative in vivo wear of human enamel10.1177/00220345890680120601 ↗
26. Wear, strength, modulus and hardness of CAD/CAM restorative materials10.1016/j.dental.2016.08.222 ↗
27. Wear resistance and abrasiveness of CAD-CAM monolithic materials10.1016/j.prosdent.2018.05.011 ↗
28. Crystallization of lithium disilicate glass using microwave processing10.1111/j.1551-2916.2011.04936.x ↗
29. Fracture toughness of yttria-stabilized zirconia sintered in conventional and microwave ovens10.1016/S0022-3913(13)60037-2 ↗
30. Sinterização de cerâmicas em microondas. Parte I: aspectos fundamentais10.1590/S0366-69132007000100002 ↗
31. In vitro investigation of the wear of human enamel by dental porcelain10.1016/S0022-3913(99)70280-5 ↗
32. Wear characteristics of current aesthetic dental restorative CAD/CAM materials: two-body wear, gloss retention, roughness and Martens hardness10.1016/j.jmbbm.2013.01.003 ↗
33. Microwave versus conventional sintering: a review of fundamentals, advantages and applications10.1016/j.jallcom.2010.01.068 ↗
34. Etiology and treatment of occlusal pathosis and associated facial pain10.1016/0022-3913(81)90340-1 ↗
35. Wear of direct resin composites and teeth: considerations for oral rehabilitation10.1111/eos.12600 ↗
36. Contact- and contact-free wear between various resin composites10.1016/j.dental.2014.11.007 ↗
37. Effect of zirconia polycrystal and stainless steel on the wear of resin composites, dentin and enamel10.1016/j.jmbbm.2018.12.024 ↗
38. Strength and fracture origins of a feldspathic porcelain10.1016/j.dental.2011.12.005 ↗
39. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
40. Multifunctional uses of a novel ceramic-lithium disilicate10.1111/j.1708-8240.2010.00362.x ↗
41. Simplified treatment of severe dental erosion with ultrathin CAD-CAM composite occlusal veneers and anterior bilaminar veneers10.1016/j.prosdent.2016.02.013 ↗
42. Abrasion of human enamel by different dental ceramics in vitro10.1177/00220345910700031301 ↗
43. Wear of opposing teeth by posterior composite resins–evaluation of newly developed wear test methods10.4012/dmj.2008-031 ↗
44. Mechanical properties of lithium metasilicate after short-term thermal treatments10.1016/j.jmbbm.2019.06.011 ↗
45. The prevalence, etiology and management of tooth wear in the United Kingdom10.1016/S0022-3913(97)70043-X ↗
46. The effect of zirconia sintering temperature on flexural strength, grain size, and contrast ratio10.1007/s00784-012-0692-6 ↗
47. Three generations of zirconia: from veneered to monolithic. Part II
48. Wear of resin denture teeth by two-body contact10.1016/j.dental.2005.03.009 ↗
49. Macro- and microtopographical examination and quantification of CAD-CAM composite resin 2- and 3-body wear10.1016/j.prosdent.2017.11.014 ↗
50. Self-etching primers vs acid conditioning: impact on bond strength between ceramics and resin cement10.2341/16-348-L ↗
51. Reinforced glass-ceramics: parametric inspection of three-dimensional wear and volumetric loss after chewing simulation10.1590/0103-6440201902699 ↗
52. Durability of staining and glazing on a hybrid ceramics after the three-body wear10.1016/j.jmbbm.2020.103856 ↗
53. Early and long-term wear of 'fast-set' conventional glass-ionomer cements10.1016/j.dental.2004.09.007 ↗