Is the application of a silane-based coupling agent necessary to stabilize the fatigue performance of bonded simplified lithium disilicate restorations?
Source abstract
Abstract
This study evaluated the influence of ceramic surface conditioning and storage regimen (baseline vs. aging) on the fatigue performance of simplified lithium disilicate glass-ceramic restorations. A total of 90 ceramic discs (Ø= 10 mm; thickness= 1.0 mm) were allocated into 6 groups (n= 15), considering 2 factors: "ceramic surface treatment" - CA (only silane-based coupling agent, Monobond N), HF (5% hydrofluoric acid etching), or HF+CA (5% HF acid etching plus silane-based coupling agent); and "storage regimen" - baseline (24 hours - 5 days of distilled water at 37 °C), or long-term aging (180 days of distilled water at 37 °C + 25,000 thermal cycles). After intaglio ceramic conditioning, adhesive bonding (Multilink N) was performed onto epoxy resin discs (Ø= 10 mm; thickness= 2.5 mm) and the bonded sets were subjected to step-stress fatigue tests (initial load: 200 N; step-size: 50 N; 10,000 cycles per step; 20 Hz). Fatigue data were analyzed using Kaplan-Meier and Weibull statistical analyses. Fractography and topography analyses were also conducted. The fatigue findings demonstrated that the performance among groups for both baseline and aging conditions maintained a tendency: the CA groups had the worst behavior (baseline: 893 N/143,667 cycles; aging: 639 N/84,179 cycles), while the surface etching with HF (baseline: 1247 N/214,333 cycles; aging: 816.67 N/128,333 cycles) and HF+CA groups (baseline: 1290 N/222,333 cycles; aging: 900 N/145,000 cycles) had no statistically significant difference between them. The aging protocol reduced the performance of all groups. The groups with better fatigue performance (HF and HF+CA) did not have statistical differences regarding structural reliability (Weibull modulus). Most failures were radial cracks from the cementation interface, except for CA aging specimens, with 27% failing from debonding. The HF etching led to noteworthy surface topographical alterations. Micromechanical interlocking resulting from HF acid etching remained prevalent in the fatigue behavior. Thus, the silane-based coupling agent (Monobond N) does not need to be applied after HF etching in terms of fatigue behavior outcomes.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Erosion and Treatment
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. The impact of hydrofluoric acid surface treatments on the performance of a porcelain laminate restorative material10.1016/j.dental.2006.03.002 ↗
2. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach10.1016/j.dental.2016.11.015 ↗
3. Fracture load of composite resin and feldspathic all-ceramic CAD/CAM crowns10.1016/j.prosdent.2005.11.014 ↗
4. Silanated surface treatment: effects on the bond strength to lithium disilicate glass-ceramic10.1590/0103-6440201300354 ↗
5. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
6. A critical perspective on mechanical testing of implants and prostheses10.1177/0022034515624445 ↗
7. Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions10.1016/j.dental.2006.11.011 ↗
8. Effect of MDP-containing silane and adhesive used alone or in combination on the long-term bond strength and chemical interaction with lithium disilicate ceramics
9. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
10. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
11. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
12. Silane reactivity and resin bond strength to lithium disilicate ceramic surfaces10.1016/j.dental.2019.05.002 ↗
13. Degradation, fatigue, and failure of resin dental composite materials10.1177/154405910808700802 ↗
14. Long term water storage deteriorates bonding of composite resin to alumina and zirconia short communication10.2174/1874210601307010123 ↗
15. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
16. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
17. Enhanced bonding strength between lithium disilicate ceramics and resin cement by multiple surface treatments after thermal cycling10.1371/journal.pone.0220466 ↗
18. Microshear bond strength of resin cements to lithium disilicate substrates as a function of surface preparation10.2341/14-240-L ↗
19. Cements and adhesives for all-ceramic restorations
20. Does acid etching morphologically and chemically affect lithium disilicate glass ceramic surfaces?
21. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
22. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
23. Chemical adhesion rather than mechanical retention enhances resin bond durability of a dental glass-ceramic with leucite crystallites10.1088/1748-6041/5/4/044101 ↗
24. Physicochemical and morphological characterization of a glass ceramic treated with different ceramic primers and post-silanization protocols10.1016/j.dental.2019.05.003 ↗
25. In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: effect on the fatigue behavior of the bonded ceramic10.1016/j.jmbbm.2021.104604 ↗
26. Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic10.1002/jbm.b.33619 ↗
27. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
28. Adhesion to a lithium disilicate glass ceramic etched with hydrofluoric acid at distinct concentrations10.1590/0103-6440201802080 ↗
29. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
30. Two-step vs. one-step conditioning systems and adhesive interface of glass ceramic surface and resins systems10.1080/01694243.2018.1455798 ↗
31. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
32. Editorial: the VALUE and remaining NEED of bond-strength testing
33. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
34. Influence of surface treatment of contaminated lithium disilicate and leucite glass ceramics on surface free energy and bond strength of universal adhesives10.4012/dmj.2015-123 ↗