Objectives To evaluate the biaxial flexural strength (BFS), surface roughness (Ra) and micro tensile bond strength (μTBS) of two CAD/CAM materials after different surface treatments. Materials and methods For μTBS, 64 human molars were used and 32 blocks of resin composite (RC-Lava Ultimate) and polymer-infiltrated ceramic (PIC -Vita Enamic). The blocks and teeth were distributed into 16 groups according to the factors "surface treatment" (HF: 10% hydrofluoric acid; APA: Al2O3 sandblasting; SC: silicate-Al2O3 sandblasting; MEP: Monobond Etch and Prime) and "thermal cycling" (TC). After cementation, the blocks were sectioned into 1 mm2 bars. Half of the specimens were thermocycled and submitted to μTBS test. For BFS, RC and PIC discs were made and distributed according to the surface treatments and after mechanical cycling, submitted to BFS test. Roughness, EDS, SEM, and Weibull analyses were also performed. Data were analyzed by (1 or 2-way) ANOVA and Tukey test (α = 0.05). Results For RC, SC and HF after TC showed significantly higher μTBS values. For PIC HF after TC showed higher μTBS than the other groups. For RC, the BFS was higher for MEP than Al2O3 and SC. For PIC, none of the surface treatments influenced BFS. Conclusion The highest μTBS for RC was obtained with SC followed by silanization and for PIC, HF followed by silanization. The RC showed lower strength after Al2O3 blasting. For PIC all surface treatments resulted in similar BFS.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Effect of different resin cements and surface treatments on the shear bond strength of ceramic-glass polymer materials10.1016/j.prosdent.2017.12.016 ↗
2. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach10.1016/j.dental.2016.11.015 ↗
3. Fracture toughness of chairside CAD/CAM materials – alternative loading approach for compact tension test10.1016/j.dental.2016.03.003 ↗
4. Influence of ceramic thickness and light-curing time on long-term μTBS between silica based ceramic and human dentin10.1080/01694243.2016.1274134 ↗
5. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
6. Analysis of tensile bond strengths using Weibull statistics10.1016/j.biomaterials.2004.01.060 ↗
7. Micro-shear bond strength of different resin cements to ceramic/glass-polymer CAD-CAM block materials10.1016/j.jpor.2016.02.003 ↗
8. Influence on fracture resistance of molars with MOD cavities
9. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
10. Bonding to CAD-CAM composites: an interfacial fracture toughness approach10.1177/0022034517728714 ↗
11. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
12. Bond strength of novel CAD/CAM restorative materials to self-adhesive resin cement: the effect of surface treatments
13. Effect of surface treatments on the bonding strength of self-adhesive resin cements to zirconia ceramics
14. Influence of pretreatment methods on the adhesion of composite and polymer infiltrated ceramic CAD-CAM blocks
15. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
16. Effect of surface treatments on shear bond strength of resin composite bonded to CAD/CAM resin-ceramic hybrid materials10.4047/jap.2016.8.4.259 ↗
17. International organization for standardization · 2008
18. Evaluation of the effect of different surface treatments on luting CAD/CAM composite resin overlay workpieces
19. Stress distribution difference between Lava Ultimate full crowns and IPS e.max CAD full crowns on a natural tooth and on tooth-shaped implant abutments10.1007/s10266-016-0276-z ↗
20. Effect of different surface treatments on the biaxial flexure strength, Weibull characteristics, roughness, and surface topography of bonded CAD/CAM silica-based ceramics10.1016/j.dental.2020.11.009 ↗
21. Microtensile bond strength of composite cement to novel CAD/CAM materials as a function of surface treatment and aging10.2341/15-263-L ↗
22. Effect of different surface treatment techniques on the repair strength of indirect composites
23. A 3-year clinical evaluation of endodontically treated posterior teeth restored with two different materials using the CEREC AC chair-side system10.1016/j.prosdent.2017.04.022 ↗
24. Effect of resin cement type on the microtensile bond strength to lithium disilicate ceramic and dentin using different test assemblies
25. Can different etching protocols change the properties of a hybrid ceramic?
26. Bonding effectiveness of tooth-colored materials to resin cement provided by self-etching silane primer after short- and long-term storage10.1016/j.prosdent.2018.12.018 ↗
27. Lithium disilicate restorations fatigue testing parameters: a systematic review10.1111/jopr.12376 ↗
28. Evaluation of the surface characteristics of dental cad/cam materials after different surface treatments10.3390/ma13040981 ↗
29. Microtensile bond strength and micromorphologic analysis of surface-treated resin nanoceramics10.4047/jap.2016.8.4.275 ↗
30. The microtensile bond test: a review
31. Bonding effectiveness of luting composites to different CAD/CAM materials
32. Evaluation of the surface roughness and accelerated aging of CAD/CAM materials10.11607/ijp.6556 ↗
33. The impact of hydrofluoric acid etching followed by unfilled resin on the biaxial strength of a glass-ceramic10.1016/j.dental.2013.08.210 ↗
34. Influence of acid-etching and ceramic primers on the repair of a glass ceramic
35. The influence of storage time and cutting speed on microtensile bond strength
36. Moisture spectrum of demineralized dentin for adhesive systems with different solvent bases
37. Adhesive bonding to polymer infiltrated ceramic10.4012/dmj.2015-271 ↗
38. Polymer-infiltrated ceramic CAD/CAM inlays and partial coverage restorations: 3-year results of a prospective clinical study over 5 years10.1007/s00784-017-2293-x ↗
39. Monolithic polymer-infiltrated ceramic network CAD/CAM single crowns: three-year mid-term results of a prospective clinical study10.11607/ijp.6548 ↗
40. Adhesive bonding to hybrid materials: an overview of materials and recommendations
41. Roughness, surface energy, and superficial damages of CAD/CAM materials after surface treatment10.1007/s00784-018-2365-6 ↗
42. Two-year performance of CAD/CAM fabricated resin composite inlay restorations: a randomized controlled clinical trial10.1111/jerd.12534 ↗
43. Effect of hydrofluoric acid concentration and etching time on resin-bond strength to different glass ceramics10.1590/1807-3107bor-2019.vol33.0041 ↗
44. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
45. The effect of surface treatments on the mechanical and optical behaviors of CAD/CAM restorative materials