journal article·2018-02Open access

Evaluating the critical strain energy release rate of bioactive glass coatings on Ti6Al4V substrates after degradation

A. Matinmanesh, Y. Li, A. Nouhi, P. Zalzal, E.H. Schemitsch, M.R. Towler, M. Papini

Abstract

It has been reported that the adhesion of bioactive glass coatings to Ti6Al4V reduces after degradation, however, this effect has not been quantified. This paper uses bilayer double cantilever (DCB) specimens to determine GIC and GIIC, the critical mode I and mode II strain energy release rates, respectively, of bioactive coating/Ti6Al4V substrate systems degraded to different extents. Three borate-based bioactive glass coatings with increasing amounts of incorporated SrO (0, 15 and 25mol%) were enamelled onto Ti6Al4V substrates and then immersed in de-ionized water for 2, 6 and 24h. The weight loss of each glass composition was measured and it was found that the dissolution rate significantly decreased with increasing SrO content. The extent of dissolution was consistent with the hypothesis that the compressive residual stress tends to reduce the dissolution rate of bioactive glasses. After drying, the bilayer DCB specimens were created and subjected to nearly mode I and mode II fracture tests. The toughest coating/substrate system (one composed of the glass containing 25mol% SrO) lost 80% and 85% of its GIC and GIIC, respectively, in less than 24h of degradation. The drop in GIC and GIIC occurred even more rapidly for other coating/substrate systems. Therefore, degradation of borate bioactive glass coatings is inversely related to their fracture toughness when coated onto Ti6A4V substrates. Finally, roughening the substrate was found to be inconsequential in increasing the toughness of the system as the fracture toughness was limited by the cohesive toughness of the glass itself.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Dental materials and restorations · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. Fracture R-curve of a toughened epoxy adhesive as a function of irreversible degradation. Mater10.1016/j.msea.2010.04.099 ↗
2. Hygrothermal degradation of two rubber-toughened epoxy adhesives: Application of open-faced fracture tests10.1016/j.ijadhadh.2010.10.001 ↗
3. Crack path selection in the fracture of fresh and degraded epoxy adhesive joints10.1016/j.engfracmech.2011.03.020 ↗
4. Prediction of environmental degradation of closed adhesive joints using data from open-faced specimens10.1016/j.compstruct.2011.09.017 ↗
5. American Society of Mechanical Engineers · 2009
6. American Society of Mechanical Engineers. ASME - STANDARDS - Surface Texture (Surface Roughness, Waviness, and Lay). (ASME, 2009). ASTM D3433-99 Standard Test Method for Fracture Strength in Cleavage of Adhesives in Bonded Metal Joints. in (2012).
7. Anderson · 2005
8. Effect of Surface Roughness on the Performance of Adhesive Joints Under Static and Cyclic Loading10.1080/00218464.2010.482430 ↗
9. The role of titanium ions on structural, dielectric and optical properties of Li2O–MgO–B2O3 glass system10.1016/j.matchemphys.2004.05.045 ↗
10. Differentiation of preosteoblasts using a delivery system with BMPs and bioactive glass microspheres10.1007/s10856-006-0687-4 ↗
11. Healing of critical-size segmental defects in rat femora using strong porous bioactive glass scaffolds10.1016/j.msec.2014.06.022 ↗
12. Effect of borate glass composition on its conversion to hydroxyapatite and on the proliferation of MC3T3-E1 cells10.1002/jbm.a.31679 ↗
13. Residual Stresses and Cracking in Brittle Solids Bonded with a Thin Ductile Layer10.1016/0001-6160(88)90305-7 ↗
14. Mode II Interlaminar Fracture of Graphite/Epoxy and Graphite/PEEK10.1177/073168448600500302 ↗
15. In vivo behaviour of hydroxyapatite coatings on titanium implants: a quantitative study in the rabbit10.1016/S0142-9612(01)00392-1 ↗
16. Mixed-mode fatigue behavior of degraded toughened epoxy adhesive joints10.1016/j.ijadhadh.2010.11.007 ↗
17. Bioactive material template for in vitro, synthesis of bone10.1002/jbm.820290311 ↗
18. Macromolecular crowding: obvious but underappreciated10.1016/S0968-0004(01)01938-7 ↗
19. Effects of non-planarity on the mixed mode fracture resistance of bimaterial interfaces10.1016/0001-6160(89)90017-5 ↗
20. Molecular mechanisms of mesenchymal stem cell differentiation towards osteoblasts10.4252/wjsc.v5.i4.136 ↗
21. Mixed-mode fracture characterization of adhesive joints10.1016/0266-3538(94)90052-3 ↗
22. Friedrich · 2012
23. Bonding of bone to apatite-coated implants10.1302/0301-620X.70B1.2828374 ↗
24. Dissolution response of hydroxyapatite coatings to residual stresses10.1002/1097-4636(20010615)55:4<596::AID-JBM1053>3.0.CO;2-Y ↗
25. Third-generation biomedical materials10.1126/science.1067404 ↗
26. Cementless Hydroxyapatite coated hip prostheses10.1155/2015/386461 ↗
27. Sol–gel derived mesoporous 58S bioactive glass coatings on AZ31 magnesium alloy and in vitro degradation behavior10.1016/j.surfcoat.2013.12.026 ↗
28. Kinetics and mechanisms of the conversion of silicate (45S5), borate, and borosilicate glasses to hydroxyapatite in dilute phosphate solutions10.1007/s10856-006-9220-z ↗
29. Effects of strontium-doped bioactive glass on the differentiation of cultured osteogenic cells10.22203/eCM.v021a11 ↗
30. Review of bioactive glass: from Hench to hybrids10.1016/j.actbio.2012.08.023 ↗
31. In vivo tensile testing of fluorapatite and hydroxylapatite plasma-sprayed coatings10.1002/jbm.820280506 ↗
32. Material fundamentals and clinical performance of plasma-sprayed hydroxyapatite coatings: a review10.1002/jbm.1056 ↗
33. New strontium-based bioactive glasses: physicochemical reactivity and delivering capability of biologically active dissolution products10.1039/b822214b ↗
34. Plasma bone-specific alkaline phosphatase as an indicator of osteoblastic activity10.1302/0301-620X.75B2.8444951 ↗
35. Indentation-induced residual stresses in 45S5 bioglass and the stress effect on the material dissolution10.1016/j.engfracmech.2008.06.024 ↗
36. Investigating the influence of Na+ and Sr2+ on the structure and solubility of SiO2-TiO2-CaO-Na2O/SrO bioactive glass10.1007/s10856-015-5415-5 ↗
37. Antibacterial and osteo-stimulatory effects of a borate-based glass series doped with strontium ions10.1177/0885328216672088 ↗
38. Characterization and fracture property of different strontium-containing borate-based glass coatings for Ti6Al4V substrates10.1016/j.jnoncrysol.2016.12.010 ↗
39. Investigating the surface reactivity of SiO2-TiO2-CaO-Na2O/SrO bioceramics as a function of structure and incubation time in simulated body fluid10.1007/s10856-014-5229-x ↗
40. Networks and hubs for the transcriptional control of osteoblastogenesis10.1007/s11154-006-9001-5 ↗
41. Conversion of borate-based glass scaffold to hydroxyapatite in a dilute phosphate solution10.1088/1748-6041/5/1/015005 ↗
42. Bioactive glass coatings for orthopedic metallic implants10.1016/S0955-2219(03)00303-0 ↗
43. Plasma-sprayed hydroxyapatite+titania composite bond coat for hydroxyapatite coating on titanium substrate10.1016/j.biomaterials.2003.10.092 ↗
44. The effect of mesenchymal stem cell differentiation in monolayer and 3D culture10.1016/j.biomaterials.2005.01.006 ↗
45. Quantitative evaluation of the adhesion of bioactive glasses onto Ti6Al4V substrates10.1016/j.matdes.2016.02.086 ↗
46. Quantifying the mode II critical strain energy release rate of borate bioactive glass coatings on Ti6Al4V substrates10.1016/j.jmbbm.2017.07.030 ↗
47. Studies on influence of aluminium ions on the bioactivity of B2O3–SiO2–P2O5–Na2O–CaO glass system by means of spectroscopic studies10.1016/j.apsusc.2013.09.055 ↗
48. Comparative investigation on the adhesion of hydroxyapatite coating on Ti–6Al–4V implant: a review paper10.1016/j.ijadhadh.2013.09.030 ↗
49. Effect of modifier ions on fluorescence and absorption of Eu3+ in alkali and alkaline earth silicate glasses10.1016/0022-3093(94)90324-7 ↗
50. Thermal Expansion of Hydroxyapatite-β-Tricalcium Phosphate Ceramics
51. The novel zinc finger-containing transcription factor osterix is required for osteoblast differentiation and bone formation10.1016/S0092-8674(01)00622-5 ↗
52. Dissolution of bioactive glasses: the effects of crystallinity coupled with stress10.1007/s11837-009-0132-5 ↗
53. O’Brien, T. K., Murri, G. B. & Salpekar, S. A. Interlaminar Shear Fracture Toughness and Fatigue Thresholds for Composite Materias. ASTM Int. Composite materials: Fatigue and fracture, second volume, (1989).10.1520/STP10418S ↗
54. Materials characterisation and cytotoxic assessment of strontium-substituted bioactive glasses for bone regeneration.10.1039/c0jm01139h ↗
55. Evaluation of titanium plasma-sprayed and plasma-sprayed hydroxyapatite implants in vivo10.1016/j.biomaterials.2003.11.053 ↗
56. The effect of hydroxyapatite coating on bone growth into porous titanium alloy implants10.1302/0301-620X.71B2.2925737 ↗
57. Strontium borate glass: potential biomaterial for bone regeneration10.1098/rsif.2009.0504 ↗
58. Fatigue behaviour of a glass coating on Ti6AL4V for biomedical applications10.17533/udea.redin.343446 ↗
59. Bioactive borate glass coatings for titanium alloys10.1007/s10856-008-3419-0 ↗
60. Study of the effect of substrate roughness on adhesive joints by SEM image analysis10.1163/156856106777144345 ↗
61. Silica-Based and Borate-Based, Titania-Containing Bioactive Coatings Characterization: Critical Strain Energy Release Rate, Residual Stresses, Hardness, and Thermal Expansion10.3390/jfb7040032 ↗
62. Dietary boron supplementation enhances the effects of estrogen on bone mineral balance in ovariectomized rats10.1385/BTER:81:1:29 ↗
63. Sodium migration pathways in multicomponent silicate glasses, 2010. Car–Parrinello molecular dynamics simulations. J. Chem. Phys. 133, 014701.10.1063/1.3456712 ↗
64. Bone morphogenetic protein-2 stimulates alkaline phosphatase activity and collagen synthesis in cultured osteoblastic cells, MC3T3-E110.1016/0006-291X(91)90490-X ↗
65. Prestandardization study on mode II interlaminar fracture toughness test for cfrp in japan10.1016/0010-4361(95)93669-B ↗
66. Modeling the Water−Bioglass Interface by Ab Initio Molecular Dynamics Simulations10.1021/am900198t ↗
67. Surface Signatures of Bioactivity: MD Simulations of 45S and 65S Silicate Glasses10.1021/la902548f ↗
68. Stimulation of bone formation by dietary boron in an orthopedically expanded suture in rabbits10.2319/112708-604.1 ↗
69. Use of end-loaded-split (ELS) test to study stable fracture behaviour of composites under mode II loading10.1016/S0263-8223(96)00066-9 ↗
70. Fabrication of CaO–NaO–SiO2/TiO2 scaffolds for surgical applications10.1007/s10856-012-4746-8 ↗
71. Measurement of adhesive joint fracture properties as a function of environmental degradation10.1016/S0143-7496(98)00028-1 ↗
72. Evaluation of Ti implants coated with Ag-containing borate bioactive glass for simultaneous eradication of infection and fracture fixation in a rabbit tibial model10.1557/jmr.2012.375 ↗
73. Bond degradation at the plasma‐sprayed HAcoating/Ti‐6AI‐4V alloy interface: an in vitro study10.1007/BF00120268 ↗
74. Measurements of residual stresses in plasma-sprayed hydroxyapatite coatings on titanium alloy10.1016/j.surfcoat.2004.02.038 ↗
75. Structure and properties of alkaline earth borate glasses
76. An experimental investigation of residual stresses in an epoxy–steel laminate10.1016/j.ijadhadh.2005.07.006 ↗
77. Effects of materials parameters on mineralization and degradation of sol-gel bioactive glasses with 3D-ordered macroporous structures10.1002/jbm.a.10093 ↗