Impact of try-in paste removal on the fatigue behavior of bonded lithium disilicate ceramics
Source abstract
Abstract
This in vitro study assessed the effectiveness of three cleaning protocols (air-water spray, 37% phosphoric acid, or Ivoclean) on lithium disilicate restorations' fatigue behavior after try-in paste application, compared to a clean condition. Lithium disilicate discs (IPS e.max CAD, Ivoclar) with Ø-= 12 mm and 1 mm thickness were prepared from prefabricated CAD-CAM blocks, polished, subjected to CAD-CAM milling topography simulation and crystallization. After, etching with 5% hydrofluoric acid and the application of try-in paste (Variolink try-in paste shade white; load of 2.5 N for 5 min) was performed. Discs that received try-in paste were divided into three groups according to the removal protocol: SPRAY - air-water spray for 30 s; HPO - active application of 37% phosphoric acid for 60 s; IVOC - application of Ivoclean for 20 s. Control group (CTRL group) did not receive the try-in paste application. Half of the specimens (n= 15) were tested in the baseline condition (24 h up to 7 days), and the others underwent 25,000 thermal cycles (5 - 55 °C) + 210 days of distilled water storage (37 °C). Additional specimens (n= 3) underwent monotonic testing (1 mm/min). Fatigue testing involved a cyclic fatigue approach (20 Hz, initial load = 100 N - 5000 cycles, step size = 50 N - 10,000 cycles) until a visible crack appeared. Fractographic and topographic analyses were performed. Fatigue data were statistically analyzed with two-way ANOVA, Kaplan-Meier log-rank (Mantel-Cox), and independent t-test (α= 0.05). In the baseline condition, the IVOC group resulted in a superior fatigue behavior compared to the CTRL and SPRAY groups, but similar to the HPO group. The HPO and SPRAY presented a similar fatigue behavior to the CTRL group. It was noticed a decrease in fatigue behavior after aging, which resulted in all the cleaning protocols leading to similar fatigue behavior compared to the CTRL group. On the SPRAY group surface, try-in pastes remnants were noticed. In summary, despite a detrimental impact at baseline conditions, all tested cleaning protocols seem proper to remove the try-in paste from the ceramic's surface in the long-term evaluation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. The effect of try-in paste and resin cement shade on colour properties of dental veneers
2. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach10.1016/j.dental.2016.11.015 ↗
3. Fatigue testing of biomaterials and their interfaces10.1016/j.dental.2017.01.012 ↗
4. Clinical performance of pressable glass‐ceramic veneers after 5, 10, 15, and 20 years: a retrospective case series study10.1111/jerd.12496 ↗
5. Can cleansing regimens effectively eliminate saliva contamination from lithium disilicate ceramic surface?
6. Does adhesive luting reinforce the mechanical properties of dental ceramics used as restorative materials? A systematic review and meta-analysis
7. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
8. Influence of the color of composite resin foundation and luting cement on the final color of lithium disilicate ceramic systems10.1016/j.prosdent.2016.05.016 ↗
9. Silane reactivity and resin bond strength to lithium disilicate ceramic surfaces10.1016/j.dental.2019.05.002 ↗
10. Evaluation of cleaning methods on lithium disilicate glass ceramic surfaces after organic contamination10.2341/20-176-L ↗
11. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
12. Active and passive application of the phosphoric acid on the bond strength of lithium disilicate10.1590/0103-6440201600428 ↗
13. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
14. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
15. The effect of storage conditions, contamination modes and cleaning procedures on the resin bond strength to lithium disilicate ceramic
16. Effect of surface cleaning regimen on glass ceramic bond strength10.3390/molecules24030389 ↗
17. Ceramic dental biomaterials and CAD/CAM technology: state of the art10.1016/j.jpor.2014.07.003 ↗
18. Malament · J. Prosthet. Dent · 2021 · 126 · 53310.1016/j.prosdent.2020.08.013 ↗
19. Effect of different surface treatment protocols on the bond strength between lithium disilicate and resin cements
20. Influence of fit-checking material and cleaning protocols on the bond strength of lithium disilicate glass-ceramics10.2341/22-036-L ↗
21. Treatment of surface contamination of lithium disilicate ceramic before adhesive luting
22. A review of adhesion science10.1016/j.dental.2009.11.157 ↗
23. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
24. Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: a systematic review and meta-analysis
25. The VALUE and remaining NEED of bond-strength testing
26. Physicochemical and morphological characterization of a glass ceramic treated with different ceramic primers and post-silanization protocols10.1016/j.dental.2019.05.003 ↗
27. Predictable bonding of adhesive indirect restorations: factors for success10.1038/s41415-021-3336-x ↗
28. Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a review10.1007/s00784-011-0636-6 ↗
29. Surface conditioning protocol for the adhesion of resin-based cements to base and noble alloys: how to condition and why?
30. Spectrophotometric analysis of clinical factors related to the color of ceramic restorations: a pilot study
31. Microstructural considerations for novel lithium disilicate glass ceramics: a review10.1111/jerd.12864 ↗
32. In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: effect on the fatigue behavior of the bonded ceramic10.1016/j.jmbbm.2021.104604 ↗
33. Evaluation paste removal method and bond strength between resin cement and lithium disilicate ceramic: an in vitro study
34. Effect of “Try-in” paste removal method on bond strength to lithium disilicate ceramic10.1016/j.jdent.2011.09.011 ↗
35. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
36. Substrate rigidity effect on CAD/CAM restorations at different thicknesses
37. Strength-limiting damage in lithium silicate glass-ceramics associated with CAD–CAM10.1016/j.dental.2018.11.004 ↗
38. Laboratory processing methods and bonding to glass ceramics: systematic review10.1016/j.ijadhadh.2023.103572 ↗
39. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
40. A brief review on fatigue test of ceramic and some related matters in Dentistry10.1016/j.jmbbm.2022.105607 ↗
41. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
42. Wachtman · 1972
43. Chairside CAD/CAM materials. Part 3: cyclic fatigue parameters and lifetime predictions10.1016/j.dental.2018.03.024 ↗
44. Comparison of bond strength to three restorative materials after contamination and the use of two cleaning agents
45. Influence of surface treatment of contaminated lithium disilicate and leucite glass ceramics on surface free energy and bond strength of universal adhesives10.4012/dmj.2015-123 ↗
46. Influence of cleaning methods on the bond strength of resin cement to saliva-contaminated lithium disilicate ceramic10.1007/s00784-019-03074-w ↗
47. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗