Effect of occlusal adjustment and subsequent repolishing on the surface roughness and volumetric wear of different types of glazed monolithic zirconia after chewing simulation
Source abstract
Abstract
The objective was to evaluate the effect of material (four monolithic zirconia) and surface condition [glazed (G) versus polished after simulation of occlusal adjustment (GAP)] on roughness and volumetric wear (VW) of dental zirconia after chewing simulation (CS). Zirconia specimens (ZS) were fabricated with an approximate diameter of 12.0 mm and a thickness of 1.0 mm. The four types of monolithic zirconia utilized were Prettau 4 Anterior (PA), Lava Plus (LP), Cercon hT (hT), and Cercon xT (xT). All specimens were coated with a thin and uniform layer of Prettau Plus glaze. Additionally, half of the ZS underwent a simulation of occlusal adjustment followed by clinical polishing. The sliding wear test was performed using a chewing simulator set at 30 N, 2 Hz, and 500,000 cycles, employing steatite specimens (SS) to simulate opposing dentition. ZS and SS underwent topographic analysis through optical profilometry to assess volumetric wear (VW) and surface roughness. The average roughness values (μm) of the zirconia ranged from 0.38h (PA-G before CS) to 2.55a (PA-GAP after CS), while for the antagonist the values ranged from 1.3b (LP-G before CS) to 2.6a (PA-GAP after CS). The VW values (mm3) of the ZS ranged from 0.7b (LP-G) to 2.5a (LP-GAP), while for the antagonist the values ranged from 0.17a (xT-GAP) to 0.33a (LP-G). The CS increased the roughness of all materials tested, regardless of the surface condition. The glazed condition showed lower roughness than the glazed/occlusal adjustment/polishing condition before the CS for three zirconia (PA, LP and xT) and after the CS for all materials. The surface condition did not significantly influence volumetric wear (VW) for three materials (PA, hT, and xT); however, for the Lava Plus (LP) group, the glazed condition resulted in reduced VW. The VW of the SS was unaffected by the material type or surface condition. In summary, zirconia specimens that underwent occlusal adjustment followed by repolishing demonstrated increased surface roughness compared to the glazed ones, while their wear behavior varied depending on the type of zirconia used.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Three-body wear associated with three ceramics and enamel10.1016/S0022-3913(99)70037-5 ↗
2. Enamel wear against monolithic zirconia restorations: a meta-analysis and systematic review of in vitro studies10.1111/jerd.12823 ↗
3. In vitro wear of a zirconium-reinforced lithium silicate ceramic against different restorative materials10.1016/j.jmbbm.2019.103403 ↗
4. The wear performance of glazed and polished full contour zirconia10.1590/0103-6440201902801 ↗
5. Classification and properties of dental zirconia as implant fixtures and superstructures10.3390/ma14174879 ↗
6. Suitability of 3D printed pieces of nanocrystalline zirconia for dental applications10.1016/j.dental.2020.01.006 ↗
7. A state-of-the-art review on the wear of the occlusal surfaces of natural teeth and prosthetic crowns10.3390/ma13163525 ↗
8. Grinding and polishing of the inner surface of monolithic simplified restorations made of zirconia polycrystals and lithium disilicate glass-ceramic: effects on the load-bearing capacity under fatigue of the bonded restorations10.1016/j.jmbbm.2021.104833 ↗
9. Effect of surface treatments on wear and surface properties of different CAD-CAM materials and their enamel antagonists10.1016/j.prosdent.2021.06.023 ↗
10. Grinding damage assessment on four high-strength ceramics10.1016/j.dental.2015.11.028 ↗
11. Recent advances in dental zirconia: 15 years of material and processing evolution10.1016/j.dental.2024.02.026 ↗
12. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
13. Clinical and laboratory surface finishing procedures for zirconia on opposing human enamel wear: a laboratory study10.1016/j.jmbbm.2015.06.007 ↗
14. Effect of dental restorative materials surface roughness on the in vitro biofilm formation of Streptococcus mutans biofilm
15. Effect of external staining on the optical properties and surface roughness of monolithic zirconia of different thicknesses10.1016/j.prosdent.2021.08.014 ↗
16. Effect of feldspar porcelain coating upon the wear behavior of zirconia dental crowns10.1016/j.wear.2012.10.016 ↗
17. A new classification system for all-ceramic and ceramic-like restorative materials10.11607/ijp.4244 ↗
18. Fatigue performance of distinct CAD/CAM dental ceramics
19. The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging10.1016/j.prosdent.2018.12.013 ↗
20. Wear of dental materials: clinical significance and laboratory wear simulation methods -A review10.4012/dmj.2018-140 ↗
21. Evaluation of various polishing systems and the phase transformation of monolithic zirconia10.1016/j.prosdent.2016.01.021 ↗
22. The wear of polished and glazed zirconia against enamel10.1016/S0022-3913(13)60005-0 ↗
23. Non-biological and biological risk indicators for tooth wear outcomes in adults10.1159/000527091 ↗
24. Effect of the number of coloring liquid applications on the optical properties of monolithic zirconia10.1016/j.dental.2014.04.008 ↗
25. Effects of surface treatments on the translucency, opalescence, and surface texture of dental monolithic zirconia ceramics10.1016/j.prosdent.2015.11.020 ↗
26. Fatigue and wear of human tooth enamel: a review10.1016/j.jmbbm.2022.105574 ↗
27. Wear resistance and abrasiveness of CAD-CAM monolithic materials10.1016/j.prosdent.2018.05.011 ↗
28. Low temperature degradation -aging- of zirconia: a critical review of the relevant aspects in dentistry10.1016/j.dental.2010.04.006 ↗
29. Effects of different finishing/polishing protocols and systems for monolithic zirconia on surface topography, phase transformation, and biofilm formation10.4047/jap.2019.11.2.81 ↗
30. Two-body wear test of enamel against laboratory polished and clinically adjusted zirconia
31. Wear of monolithic zirconia against different CAD-CAM and indirect restorative materials10.1016/j.prosdent.2021.03.023 ↗
32. Polish of interface areas between zirconia, silicate-ceramic, and composite with diamond-containing systems10.4047/jap.2018.10.4.315 ↗
33. Wear performance of substructure ceramics and veneering porcelains10.1016/j.dental.2011.04.001 ↗
34. Experimental comparison on dental BioTribological pairs zirconia/zirconia and zirconia/natural tooth by using a reciprocating tribometer10.1007/s10916-019-1230-8 ↗
35. A study on the wear of enamel caused by monolithic zirconia and the subsequent phase transformation compared to two other ceramic systems10.4103/0972-4052.194940 ↗
36. 10-year randomized trial (RCT) of zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.jdent.2018.05.015 ↗
37. Comparative study of the wear of the pair human teeth/Vita Enamic (R) vs commonly used dental ceramics through chewing simulation10.1016/j.jmbbm.2018.08.029 ↗
38. Comparative evaluation of enamel wear against monolithic zirconia and layered zirconia after polishing and glazing: an in vitro study10.4103/jips.jips_503_21 ↗
39. Comparison of translucency and opalescence among different dental monolithic ceramics10.1016/j.prosdent.2021.04.030 ↗
40. Effect of pigmentation techniques on the fatigue mechanical behavior of a translucent zirconia for monolithic restorations10.1016/j.jmbbm.2022.105362 ↗
41. A randomized clinical trial comparing zirconia and metal-ceramic three-unit posterior fixed partial dentures: a 5-year follow-up
42. Color in zirconia-based restorations and related factors: a literature review
43. Quantitative analysis on the wear of monolithic zirconia crowns on antagonist teeth10.1186/s12903-021-01452-z ↗
44. Wear behavior and microstructural characterization of translucent multilayer zirconia10.1016/j.dental.2020.08.015 ↗
45. A two-body frictional wear test10.1177/00220345940730091001 ↗
46. Influence of different surface treatments on two-body wear and fracture load of monolithic CAD/CAM ceramics10.1007/s00784-019-03173-8 ↗
47. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
48. Fatigue strength of yttria-stabilized zirconia polycrystals: effects of grinding, polishing, glazing, and heat treatment10.1016/j.jmbbm.2017.06.016 ↗