This aim of this study is to determine the elastoplastic properties of Ni-free Al3FeSi2 intermetallic coatings grown on medical stainless steel under different experimental conditions. Elastoplastic properties are defined by the plasticity index (PI), which correlates the hardness and the Young's modulus. Special emphasis is devoted to correlate the PI with the wear resistance under sliding contact, determined by scratch testing, and fracture toughness, determined by using a novel method based on successive impacts with small loads. With regard to the substrate, the developed coatings are harder and exhibit a lower Young's reduced modulus, irrespective of the experimental conditions. It has been shown that preheating of the samples prior to hot dipping and immersion influences the type and volume fraction of precipitates, which in turn also affect the nanomechanical properties. The higher the preheating temperature is, the greater the Young's reduced modulus is. For a given preheating condition, an increase of the immersion time yields a decrease in hardness. Although apparent friction coefficients of coated specimens are smaller than those obtained on AISI 316 LVM, they increase when using preheating or higher immersion times during processing, which correlates with the PI. The presence of precipitates produces an increase in fracture toughness, with values greater than those presented by samples processed on melted AlSi alloys with lower Si content (12 wt%). Therefore, these intermetallic coatings could be considered "hard but tough", suitable to enhance the wear resistance, especially when using short periods of immersion.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Surface Treatment and Residual Stress · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
2. Corrosion behaviour and biocompatibility of novel Ni-free intermetallic coating growth on austenitic steel by hot dipping in an Al–12.6wt% Si alloy
3. Corrosion behaviour and biocompatibility of a novel Ni- free intermetallic coating growth on austenitic steel by hot dipping in an Al–12.6% Si alloy
4. Beake · Diam. Relat. Mater. · 2002 · 11 · 160610.1016/S0925-9635(02)00107-3 ↗
5. Investigating the fracture resistance and adhesion of DLC films with micro-impact testing10.1016/S0925-9635(02)00107-3 ↗
6. Evaluating the fracture properties and fatigue wear of tetrahedral amorphous carbon films on silicon by nano-impact testing10.1016/S0257-8972(03)00934-4 ↗
7. Evaluating the fracture properties and fatigue wear of tetrahedral amorphous carbon films on silicon by nano-impact testing10.1016/S0257-8972(03)00934-4 ↗
8. Breustch · 2005
9. Failures modes in scratch adhesión testing10.1016/0257-8972(91)90188-3 ↗
10. Life expectancy of modular Ti6Al4V hip implants: influence of stress and environment10.1016/j.jmbbm.2011.06.018 ↗
11. Analysis of sharp-tip-indentation load-depth curve for contact area determination taking into account pile up and sink-in effects10.1557/JMR.2004.0419 ↗
12. Proliferation/differentiation of osteoblastic human alveolar bone cell cultures in the presence of stainless steel corrosion products10.1023/A:1008975507654 ↗
13. Dobbs · 1978 · vol. 684 · 245
14. Characterization and cytotoxicity of ions released from stainless steel and nickel–titanium orthodontic alloys10.1016/j.ajodo.2003.09.009 ↗
15. Enderle · 2005
16. Calcium phosphate coating on titanium induced by phosphating
17. A method to assess the fracture toughness of intermetallic coatings by ultramicroindentation techniques: applicability to coated medical stainless steel10.1016/j.actamat.2012.12.009 ↗
18. Frutos · J. Alloys Compd. · 2015
19. Development of hard intermetallic coatings on austenitic stainless steel by hot dipping in an Al–Si alloy10.1016/j.surfcoat.2009.03.015 ↗
20. Nanomechanical properties of novel intermetallic coatings developed on austenitic stainless steels by siliconisation in liquid phase10.1016/j.intermet.2010.10.001 ↗
21. Characterization of the elastic-plastic behavior of intermetallic coatings growth on medical stainless steel by instrumented ultramicroindentation10.1016/j.jmbbm.2012.08.008 ↗
22. Deformation and failure mechanism of nano-composite coatings under nano-indentation10.1016/j.surfcoat.2005.10.010 ↗
23. Nano and microcrystal coatings and their high-temperature applications10.1002/1521-4095(200107)13:12/13<1001::AID-ADMA1001>3.0.CO;2-V ↗
24. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
25. Corrosion and its importance in selection of materials for biomedical applications
26. Friction in hip prostheses10.1016/S0142-9612(97)00034-3 ↗
27. Harding · Mater. Res. Soc. Symp. Proc. · 1995 · 356 · 66310.1557/PROC-356-663 ↗
28. Metal release rate from AISI 316L stainless steel and pure FE, CR and Ni into a sysnthetic biological medium – a comparison10.1039/b805075a ↗
29. Corrosion-resistant alloys in chloride solutions; materials for surgical implants
30. Fretting in orthopaedic implants: a review10.1016/0043-1648(94)90272-0 ↗
31. Fretting fatigue crack analysis in Ti-6Al-4V10.1016/j.ijfatigue.2005.07.008 ↗
32. Fretting corrosión behaviour of thermally oxidized CP-Ti in Ringer׳s solution10.1016/j.corsci.2009.10.029 ↗
33. 2006
34. 2009 · vol. 1
35. Surface modifications of surgical implants
36. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimized tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
37. Design criteria for wear-resistant nanostructured and glassy-metal coatings
38. Frictional component of the indentation size effect in low hardness testing10.1557/JMR.1993.1028 ↗
39. Titanium alloys in total joint replacement—a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
40. Development in vapour deposited ceramic coatings for tribological applications
41. Structure–property relationships in single and dual phase nanocrystalline hard coatings10.1016/S0257-8972(03)00576-0 ↗
42. A review on nickel-free nitrogen containing austenitic stainless steels for biomedical applications10.1016/j.msec.2013.06.002 ↗
43. Sol–gel derived hydrosyapatite coatings on titanium substrate10.1023/A:1004738900778 ↗
44. Hard and superhard nanocomposite coatings10.1016/S0257-8972(99)00586-1 ↗
45. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
46. 2003 · 1
47. A metal-induced apoptosis: mechanisms10.1016/j.mrfmmm.2003.07.015 ↗
48. Ion reléase from orthodontic appliances10.1016/S0300-5712(98)00073-6 ↗
49. Durability of metallic implant materials
50. Development of nitrogen-containing nickel free austenitic stainless steels for metallic biomaterials−review10.1016/j.msec.2004.08.030 ↗
51. Sutow · 1981 · vol. I · 45
52. Metal allergy to stainless steel wire after coronary artery bypass grafting10.1007/s100470300011 ↗
53. The use of titanium for medical applications in the USA10.1016/0921-5093(96)10243-4 ↗