Changes of residual stresses on the surface of leucite-reinforced ceramic restoration luted with resin composite cements during aging in water
Source abstract
Abstract
The objective of this study was to compare the changes in the residual stresses present on the surface of leucite-reinforced dental ceramic restorations luted with a self-adhesive and a conventional resin composite cement during aging in water. Ring specimens made of a leucite-reinforced ceramics were luted to ceramic cylinders using a self-adhesive (Panavia SA Luting Plus) or a conventional resin composite cement (Panavia V5) in dual-cure or self-cure mode. Residual stresses on the ring surface were measured using indentation fracture method at 1 h, 1, 3, 7, 14 and 28 days of the 37 °C water immersion. Water sorption, water solubility and elastic modulus of the cements were also measured. Compressive stress was generated on the surface of the ceramic rings by the polymerization of the resin composite cements, and the stresses appeared to decrease over time by water sorption of the cements. The dual-cured conventional resin composite cement remained compressive stresses on the ceramic surface, while only the self-cured self-adhesive cement, which demonstrated the greatest water sorption, generated tensile stresses during the four weeks of aging in water. The elastic moduli of cements did not significantly change through the immersion, suggesting that the stresses were less affected by the modulus. To prevent the generation of tensile stresses on the leucite-reinforced ceramic restoration, self-adhesive cements exhibiting small water sorption should be clinically selected.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Toughness measurement in direct resin composites using quantitative fractographic analysis10.25241/stomaeduj.2018.5(1).art.1 ↗
2. Polymerization contraction stress in dual-cure cements and its effect on interfacial integrity of bonded inlays10.1016/S0300-5712(02)00047-7 ↗
3. Maximising the fracture resistance of dentine-bonded all-ceramic crowns10.1016/S0300-5712(98)00050-5 ↗
4. Should resin cements be used for every cementation?10.14219/jada.archive.2007.0271 ↗
5. Determination of hardness to elastic modulus ratios using Knoop indentation measurements and a model based onloading and reloading half-cycles10.1007/BF01114301 ↗
6. Hardness
7. Relaxation of polymerization contraction shear stress by hygroscopic expansion10.1177/00220345900690010501 ↗
8. Developing a more complete understanding of stresses produced in dental composites during polymerization10.1016/j.dental.2004.10.004 ↗
9. Hygroscopic and hydrolytic effects in dental polymer networks10.1016/j.dental.2005.05.005 ↗
10. Polymerization stress – is it clinically meaningful?10.1016/j.dental.2015.06.020 ↗
11. Self-adhesive resin cements – chemistry, properties and clinical considerations10.1111/j.1365-2842.2010.02148.x ↗
12. Fracture toughness of dental ceramics: comparison of bending and indentation method10.1016/S0109-5641(01)00005-7 ↗
13. Favorable residual stress induction by resin-cementation on dental porcelain10.1016/j.dental.2017.07.018 ↗
14. Kinetics of polymerization and contraction stress development in self-adhesive resin cements10.1016/j.dental.2012.06.003 ↗
15. Evidence of chemical bonding to hydroxyapatite by phosphoric acid esters10.1016/j.biomaterials.2005.01.035 ↗
16. Comparison of two heat-pressed all-ceramic dental materials10.1016/S0109-5641(00)00031-2 ↗
17. Direct posterior esthetic restorations
18. Effect of curing mode on the micro-mechanical properties of dual-cured self-adhesive resin cements10.1007/s00784-011-0527-x ↗
19. Deformation of a dental ceramic following adhesive cementation10.1177/0022034509354049 ↗
20. Effect of resin hydrophilicity on water sorption and changes in modulus of elasticity10.1016/j.biomaterials.2005.04.052 ↗
21. Comparison of polymerization contraction stresses of between self- and light-curing composites10.1016/S0300-5712(98)00065-7 ↗
22. Contraction stress of composite resin build-up procedures for pulpless molars
23. Letter to the editor10.1177/00220345900690031701 ↗
24. Dental cements for luting and bonding restorations: self-adhesive resin cements
25. A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation Measurements10.1111/j.1151-2916.1982.tb10357.x ↗
26. Evaluation of ISO 4049: water sorption and water solubility of resin cements10.1111/eos.12339 ↗
27. Analysis of chemical interaction of 4-MET with hydroxyapatite using XPS10.4012/dmj.25.645 ↗
28. Water aging reverses residual stresses in hydrophilic dental composites10.1177/0022034513513905 ↗
29. Water sorption and water solubility of self-etching and self-adhesive resin cements10.1016/j.prosdent.2015.06.002 ↗
30. An in situ evaluation of the polymerization shrinkage, degree of conversion, and bond strength of resin cements used for luting fiber posts10.1016/j.prosdent.2016.02.019 ↗
31. Crack formation of all-ceramic crowns dependent on different core build-up and luting materials10.1016/S0300-5712(98)00049-9 ↗
32. Residual stress measurement for engineering ceramics by indentation fracture method
33. Dental resin cements – the influence of water sorption on contraction stress changes and hydroscopic expansion10.3390/ma11060973 ↗
34. Effective expansion: balance between shrinkage and hygroscopic expansion10.1177/0022034516633450 ↗
35. Residual stresses in bilayer dental ceramics10.1016/j.biomaterials.2004.08.025 ↗
36. Can hygroscopic expansion compensate polymerization shrinkage? Part I. Deformation of restored teeth10.1016/j.dental.2010.09.007 ↗
37. Composite inlay system: material properties and design
38. Calculation of contraction stresses in dental composites by analysis of crack propagation in the matrix surrounding a cavity10.1016/j.dental.2008.10.008 ↗
39. Polymerization stress of dental resin composite continues to develop 12 hours after irradiation10.1111/jerd.12091 ↗
40. Contraction stresses in direct and indirect composite restorations compared by crack analysis
41. Finite element stress analysis of indirect restorations prepared in cavity bases10.4012/dmj.26.274 ↗