Impact of multiple firings on fracture load of veneered zirconia restorations
Source abstract
Abstract
Objectives This investigation evaluated the impact of multiple firings during the veneering process of anterior all-ceramic restorations on the fracture load (FL) of zirconia crowns veneered with different ceramics (ZRT, ZRO, HFZ, STR). Methods All-ceramic crowns with anatomically reduced zirconia frameworks were prepared using four different veneering ceramics (N = 192/n = 48 per veneering ceramic). The crowns were fired 2 and 10 times. Half of them were thermocycled (5000 cycles, 5 °C/55 °C, 20s). FL using Voss shear test was measured. Data was analyzed using ANOVA with partial eta squared and post-hoc Scheffé-test as well as t-test and Weibull analysis. Results Regarding FL, greatest differences were among the number of firings (p<0.001, ηp2 = 0.369). FL was not influenced by the interaction of both number of firings and aging level (p = 0.231) and the interaction of number of firings and veneering ceramic (p = 0.222). Differences were found comparing FL values of ZRT and STR (p<0.001) and of HFZ and STR (p<0.001). No differences occurred among the veneering ceramics after 2 (p = 0.430) and after 10 firings (p = 0.057) in respect to initial FL. For all initially tested veneering ceramics, FL showed higher values after 10 firings (p≤0.001-0.014). When aged, ZRO, HFZ, and STR also provided higher FL values after 10 firings (p≤0.001). For ZRT, FL values differed between initial and aged testing after 2 firings (p = 0.001) with aged specimens providing higher FL values. After 10 firings, none of the veneering ceramics showed differences regarding FL values between initial and aged testing. Weibull modulus was higher for ZRT specimens after 10 firings when tested initially (m = 10.1) and for aged ZRT specimens after 2 firings (m = 11.1). Failures occurred either with chipping of the veneer or total fracture. Significance Veneered zirconia restorations tested presented higher FL after 10 firings compared to 2 firings. Aging via thermocycling showed a positive effect on the FL.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Reconstructive Facial Surgery Techniques · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Maximum bite force following unilateral fixed prosthetic treatment: a within-subject comparison to the dentate side10.1159/000370214 ↗
2. Effects of multiple firings on the microstructure of zirconia and veneering ceramics10.4012/dmj.2015-429 ↗
3. Efficiency of Er: YAG laser in veneers debonding with two materials & thicknesses – an in vitro study10.21608/mjd.2021.223399 ↗
4. Residual stresses in porcelain-veneered zirconia prostheses10.1016/j.dental.2012.04.019 ↗
5. Effect of number of firings on the color and translucency of ceramic core materials with veneer ceramic of different thicknesses10.1016/j.prosdent.2017.02.011 ↗
6. Thermal-induced residual stresses affect the lifetime of zirconia–veneer crowns10.1016/j.dental.2012.11.015 ↗
7. Evaluation of thermal compatibility between core and veneer dental ceramics using shear bond strength test and contact angle measurement10.1016/j.dental.2010.03.019 ↗
8. The effect of porcelain thickness and surface liner application on the fracture behavior of a ceramic system10.1016/j.dental.2011.05.009 ↗
9. Analysis of thermal distributions in veneered zirconia and metal restorations during firing10.1016/j.dental.2013.08.212 ↗
10. Influence of thermal gradients on stress state of veneered restorations10.1016/j.dental.2014.02.020 ↗
11. Two regression methods for estimation of a two-parameter Weibull distribution for reliability of dental materials10.1016/j.dental.2014.11.014 ↗
12. Probability of fracture of all-ceramic crowns
13. Sintering of dental porcelain: effect of time and temperature on appearance and porosity10.1016/S0109-5641(01)00038-0 ↗
14. Effect of thermal misfit between different veneering ceramics and zirconia frameworks on in vitro fracture load of single crowns10.4012/dmj.26.766 ↗
15. Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites10.1016/j.dental.2008.09.003 ↗
16. Effect of core design and veneering technique on damage and reliability of Y-TZP-supported crowns10.1016/j.dental.2012.11.012 ↗
17. Survival of zirconia-and metal-supported fixed dental prostheses: a systematic review
18. Impact of multiple firings on thermal properties and bond strength of veneered zirconia restorations10.1016/j.jmbbm.2022.105134 ↗
19. Thermal dimensional behavior of dental ceramics10.1016/j.biomaterials.2003.09.027 ↗
20. Role of coefficient of thermal expansion on bond strength of ceramic veneered yttrium-stabilized zirconia
21. Fracture of brittle solids (Cambridge solid state science series)10.1115/1.3424125 ↗
22. Current status of zirconia restoration10.1016/j.jpor.2013.09.001 ↗
23. In vitro evaluation of shear bond strength of veneering ceramics to zirconia10.4012/dmj.2009-065 ↗
24. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: multiple-unit FDPs10.1016/j.dental.2015.02.013 ↗
25. A systematic review of the survival and complication rates of zirconia-ceramic and metal-ceramic single crowns10.1111/clr.13306 ↗
26. Influence of substructure design, veneer application technique, and firing regime on the in vitro performance of molar zirconia crowns10.1016/j.dental.2013.04.011 ↗
27. Fracture toughness of veneering ceramics for fused to metal (PFM) and zirconia dental restorative materials10.6028/jres.115.024 ↗
28. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
29. Effect of firing protocols on cohesive failure of all-ceramic crowns10.1016/j.jdent.2010.08.014 ↗
30. Influence of core-veneer thickness ratio on the fracture load and failure mode of zirconia crowns10.1111/jopr.12601 ↗
31. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
32. The use of slow heating and slow cooling regimens to strengthen porcelain fused to zirconia10.1016/S0022-3913(12)60050-X ↗
33. Effects of multiple firings on the mechanical properties and microstructure of veneering ceramics for zirconia frameworks10.1016/j.jdent.2012.01.014 ↗
34. Influences of multiple firings and aging on surface roughness, strength and hardness of veneering ceramics for zirconia frameworks10.1016/j.jdent.2015.06.006 ↗
35. Thermal gradients and residual stresses in veneered Y-TZP frameworks10.1016/j.dental.2011.08.001 ↗
36. Zirconia-porcelain bonding: effect of multiple firings on microtensile bond strength
37. The effect of ceramic thickness and number of firings on the color of ceramic systems: an in vitro study10.1016/j.prosdent.2006.11.002 ↗
38. Effect of repeated firings on flexural strength of veneered zirconia10.1016/j.dental.2015.04.012 ↗
39. Stability of metal-ceramic crowns (die Festigkeit metallkeramischer Kronen)