journal article·2022-02

Adhesion of bioactive glass-based adhesive to bone

Varinder Pal Singh Sidhu, Faizan Bilwani, Mark R. Towler, Marcello Papini

Publisher page

Abstract

Understanding the failure modes and the fracture resistance is critical in evaluating the performance of an adhesive for sternal fixation. In this paper, a fracture mechanics testing methodology was used to assess the adhesion of a bioactive glass-based adhesive to bovine bone in terms of a measured mode I critical strain energy release rate (GIC). Reinforced double cantilever beam (DCB) samples were observed to produce repeatable values of GIC. The measured GIC was found to increase significantly from 5.41 to 12.60 J/m2 with an increase in adhesive thickness from 390 to 990 μm because of the constraint from the two adherends regulating the plastic zone size ahead of the crack. The specimens failed cohesively in all cases demonstrating that there was good adhesion to bone, a condition necessary to restrict micromotion and thus provide rigid sternal fixation when used along with sternal wires. It was also found that when the bone was flooded with liquid during adhesive application a much lower GIC of between 0.69 and 1.15 J/m2 was measured. Overall, the results demonstrate that the fracture mechanics approach can be used to provide a quantitative measure of the adhesion of the bioactive glass-based adhesive to the bone and that the adhesive should only be applied to clean bone in a dry environment.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Surgical Sutures and Adhesives · Orthopedic Surgery and Rehabilitation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (81)

Show source-provided references
1. The role of poly(acrylic acid) in conventional glass polyalkenoate cements10.1515/polyeng-2015-0079 ↗
2. A novel tantalum-containing bioglass. Part II. Development of a bioadhesive for sternal fixation and repair10.1016/j.msec.2016.10.024 ↗
3. Fracture R-curve of a toughened epoxy adhesive as a function of irreversible degradation10.1016/j.msea.2010.04.099 ↗
4. Fracture R-curve characterization of toughened epoxy adhesives10.1016/j.engfracmech.2009.10.009 ↗
5. Evolution of crack path and fracture surface with degradation in rubber-toughened epoxy adhesive joints: application to open-faced specimens10.1016/j.ijadhadh.2011.04.007 ↗
6. Anderson · 2005
7. The effect of zinc on microbial growth
8. Effect of adhesive thickness on fatigue and fracture of toughened epoxy joints – Part II: analysis and finite element modeling10.1016/j.engfracmech.2010.07.006 ↗
9. The fracture of epoxy- and elastomer-modified epoxy polymers in bulk and as adhesives10.1002/app.1975.070190917 ↗
10. Standardized methodology for in vitro assessment of bone-to-bone adhesion strength10.1016/j.ijadhadh.2017.03.014 ↗
11. Comparison of an experimental bone cement with surgical Simplex® P, Spineplex® and Cortoss10.1007/s10856-007-3363-4 ↗
12. Compressive and diametral tensile strength of glass ionomer cements10.1590/S1678-77572004000400017 ↗
13. Broek · 1986
14. The divalent strontium salt S12911 enhances bone cell replication and bone formation in vitro10.1016/8756-3282(96)00080-4 ↗
15. Influence of layer thickness on cohesive properties of an epoxy-based adhesive—an experimental study10.1080/00218464.2010.498718 ↗
16. Strontium ranelate promotes osteoblastic cell replication through at least two different mechanisms10.1016/j.bone.2008.02.010 ↗
17. A review of the methods for the evaluation of coating-substrate adhesion10.1016/0921-5093(91)90482-3 ↗
18. A review on the mechanical methods for evaluating coating adhesion10.1007/s00707-013-0979-y ↗
19. Glass-ionomer dental restoratives10.1016/S0079-6700(01)00006-5 ↗
20. da Silva · 2012
21. L. F. M. da Silva, A. Öchsner, and R. D. Adams, Handbook of Adhesion Technology. .
22. Julian's re-introduction of Milton's operation10.1016/0003-4975(92)90293-D ↗
23. Novel polyalkenoate (glass-ionomer) dental cements based on zinc silicate glasses10.1016/0142-9612(94)90055-8 ↗
24. Darvel · 2009
25. Modified DCB and CLS specimens for mixed-mode fatigue testing of adhesively bonded thin sheets10.1016/j.ijadhadh.2010.04.002 ↗
26. Entangled polymers10.1063/1.2915700 ↗
27. Full-spectrum cardiac surgery through a minimal incision: mini-sternotomy (lower half) technique10.1016/S0003-4975(97)01368-4 ↗
28. The expansile properties of kryptonite relating to cranioplasty10.1097/SCS.0000000000000508 ↗
29. Kryptonite bone cement prevents pathologic sternal displacement10.1016/j.athoracsur.2010.05.009 ↗
30. Fracture load predictions for adhesive joints10.1016/0266-3538(94)90091-4 ↗
31. Studies on the free volume and the volume expansion behavior of amorphous polymers10.1016/S0969-806X(00)00211-5 ↗
32. Hutchinson · 1991 · 63
33. Failure of a ductile adhesive layer constrained by hard adherends10.1115/1.482769 ↗
34. The median sternal incision in intracardiac surgery with extracorporeal circulation; a general evaluation of its use in heart surgery
35. Infected median sternotomy wound. Successful treatment by muscle flaps10.1097/00000658-198006000-00012 ↗
36. S. M. Kenny, “Bone cements and fillers: a review,” J. Mater. Sci. Mater. Med., vol. 14, no. 11.10.1023/A:1026394530192 ↗
37. Bone cements and fillers: a review10.1023/A:1026394530192 ↗
38. Strength of the cement-bone interface10.1097/00003086-198203000-00043 ↗
39. Mechanical strength of poly(methyl methacrylate) cement-human bone interfaces10.1002/jbm.820170305 ↗
40. Experimental verification of the linear relationship between stress and the reciprocal of the peak barkhausen voltage in ASTM A36 steel10.1109/TMAG.2012.2234728 ↗
41. Effect of bond thickness on the fracture toughness of adhesive joints10.1115/1.1631433 ↗
42. Disruption and infection of median sternotomy: a comprehensive review10.1016/S1010-7940(02)00124-0 ↗
43. Interfacial fracture toughness between bovine cortical bone and cements10.1016/S0142-9612(02)00464-7 ↗
44. Stimulatory effect of zinc on deoxyribonucleic acid synthesis in bone growth of newborn rats: enhancement with zinc and insulin-like growth factor-I10.1007/s00223-001-2010-1 ↗
45. Penetration and shear strength of cement-bone interfaces in vivo10.1097/00003086-199301000-00041 ↗
46. Tensile strength of the cement-bone interface depends on the amount of bone interdigitated with PMMA cement10.1016/S0021-9290(96)00164-9 ↗
47. Mechanical strength of the cement–bone interface is greater in shear than in tension10.1016/S0021-9290(99)00107-4 ↗
48. On experimental methods to investigate the effect of layer thickness on the fracture behavior of adhesively bonded joints10.1016/j.ijadhadh.2011.08.004 ↗
49. Quantitative evaluation of the adhesion of bioactive glasses onto Ti6Al4V substrates10.1016/j.matdes.2016.02.086 ↗
50. Mechanical analysis of midline sternotomy wound closure10.1016/S0022-5223(99)70251-5 ↗
51. Novel adhesives for sternal fixation and stabilization: a biomechanical analysis10.1016/j.clinbiomech.2019.01.007 ↗
52. Novel adhesives for distal radius fixation: a biomechanical analysis10.1016/j.jmbbm.2018.09.011 ↗
53. Bone cement, thermal injury and the radiolucent zone10.3109/17453678408992403 ↗
54. Moore · 2001 · vol. 28
55. R-curve behavior of Cu–Sn3.0Ag0.5Cu solder joints: effect of mode ratio and microstructure10.1016/j.msea.2009.08.046 ↗
56. Reliability of PMMA bone cement fixation: fracture and fatigue crack-growth behaviour10.1023/A:1018574109544 ↗
57. Clinical outcomes of noninfectious sternal dehiscence after median sternotomy10.1016/j.athoracsur.2006.04.058 ↗
58. Wound complications after median sternotomy: a study of 61 patients from a consecutive series of 9,279
59. Neurotoxic effects of aluminium among foundry workers and alzheimer's disease10.1016/S0161-813X(02)00097-9 ↗
60. Clinical, immunological, anti-inflammatory and antioxidant roles of zinc10.1016/j.exger.2007.10.013 ↗
61. Potential risk of sternal wires10.1016/j.ejcts.2003.11.043 ↗
62. Measurement of adhesion of sternal wires to a novel bioactive glass-based adhesive10.3390/jfb10030037 ↗
63. Primary sternal plating in high-risk patients prevents mediastinitis10.1016/j.ejcts.2004.04.038 ↗
64. Historical review of porous-coated implants10.1016/S0883-5403(87)80024-4 ↗
65. Standard test method for fracture strength in cleavage of adhesives in bonded metal joints
66. Interfacial fracture toughness of synthetic bone-cement interface10.4028/www.scientific.net/KEM.312.251 ↗
67. M. J. Tyas and M. F. Burrow, “Adhesive restorative materials: a review.,” Aust. Dent. J., vol. 49, no. 3, pp. 112-121; quiz 154, Sep. 2004, doi: 10.1111/j.1834-7819.2004.tb00059.x.10.1111/j.1834-7819.2004.tb00059.x ↗
68. Bioactive glass-containing cranial implants: an overview10.1007/s10853-017-0888-x ↗
69. Bio-adhesion evaluation of a chitosan-based bone bio-adhesive10.1016/j.ijadhadh.2019.04.009 ↗
70. Glass polyalkenoate (glass-ionomer) cements: a review10.1016/0300-5712(86)90030-8 ↗
71. Interfacial fracture toughness of tissue-biomaterial systems10.1002/(SICI)1097-4636(199721)38:1<1::AID-JBM1>3.0.CO;2-V ↗
72. Testing of bone-biomaterial interfacial bonding strength: a comparison of different techniques10.1002/(SICI)1097-4636(199623)33:3<133::AID-JBM2>3.0.CO;2-R ↗
73. Dimensional changes of resin/ionomer restoratives in aqueous and neutral media10.1016/S0109-5641(99)00098-6 ↗
74. Dental silicate cements: IX. Decomposition of the powder10.1177/00220345700490013301 ↗
75. The glass-ionomer cement, a new translucent dental filling material10.1002/jctb.5020211101 ↗
76. Wilson · 1993
77. The processing, mechanical properties and bioactivity of strontium based glass polyalkenoate cements10.1007/s10856-007-3287-z ↗
78. Nanostructure and elastic modulus of single trabecula in bovine cancellous bone10.1016/j.jbiomech.2014.09.009 ↗
79. Percutaneous upper extremity fracture fixation using a novel glass-based adhesive10.1016/j.jor.2018.01.033 ↗
80. Fracture toughness and crack resistance curves of acrylic bone cements10.1002/jbm.b.34537 ↗
81. British Standards Specification for Dental Glass Ionomer Cement BS