Conventional-, bulk-fill- or flowable-resin composites as prosthetic core build-up: Influence on the load-bearing capacity under fatigue of bonded leucite-reinforced glass-ceramic
Source abstract
Abstract
This study aimed to evaluate the fatigue performance of simplified ceramic restorations (leucite-reinforced glass ceramic) adhesively cemented onto substrates of different resin composites. Three options from the same commercial line were selected (Tetric N-Line, Ivoclar), classified as Conventional (CRC), Bulk-fill (BRC) and Flowable (FRC), which were used to make discs using a cylindrical metallic device (n = 19; Ø = 10 mm, thickness = 2.0 mm). A total of 57 discs (Ø = 10 mm, thickness = 1.0 mm) were made from CAD/CAM prefabricated blocks of a leucite reinforced glass-ceramic (Empress CAD, Ivoclar) to simulate a monolithic restoration, then were randomly distributed to be bonded on 19 discs of each three different resin composite substrates (CRC; BRC; or FRC) with a dual resin cement (Multilink N; Ivoclar). The samples were subjected to a compression test with a hemispherical stainless-steel piston (Ø = 40 mm) at a monotonic regimen (n = 4; 1 mm/min loading rate and 500 kgf loading cell until fracture). The cyclic fatigue test was performed underwater at a frequency of 20 Hz (n = 15). The first step was applied using 200N for 5000 cycles, followed by increments of 50N at each step of 10,000 until failure. The outcome considered for both tests was the occurrence of radial crack. Specific statistical tests (α = 0.05) were performed for monotonic (One-way ANOVA; Tukey's test) and fatigue data (Kaplan-Meier test; Log-rank test). Fractography of fractured samples were also performed. The FRC group had the lowest failure load in both test regimes (p < 0.05; monotonic: 726.64N; fatigue: 716.67N). There were no differences between the CRC and BRC groups (p > 0.05; monotonic: 989.30 and 990.11N; fatigue: 810.00 and 833.33N, respectively). The same result was obtained considering cycles for fatigue failure (FRC < CRC=BRC). Leucite glass-ceramic bonded to substrates made of flowable resin composite behaves worse mechanically than bonding to conventional or bulk-fill resin composite substrates.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Clinical effectiveness of bulk-fill and conventional resin composite restorations: systematic review and meta-analysis10.3390/polym12081786 ↗
2. Flowable resin composites: a systematic review and clinical considerations
3. A characterization of first-generation flowable composites10.14219/jada.archive.1998.0274 ↗
4. Effect of luting materials, presence of tooth preparation, and functional loading on stress distribution on ceramic laminate veneers: a finite element analysis10.1016/j.prosdent.2020.02.005 ↗
5. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
6. Bulk-fill resin-based composite restorative materials: a review10.1038/sj.bdj.2017.214 ↗
7. Effects of flowable composite lining and operator experience on microleakage and internal voids in class II composite restorations10.1067/mpr.2001.113780 ↗
8. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
9. Effect of supporting substrate on the failure behavior of a polymer-infiltrated ceramic network material10.1016/j.prosdent.2018.08.008 ↗
10. Microstructural features of current resin composite materials10.1007/s40496-014-0029-4 ↗
11. Microleakage reduction from newer esthetic restorative materials in permanent molars
12. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
13. Effect of an adhesive interlayer on the fracture of a brittle coating on a supporting substrate10.1557/JMR.2003.0031 ↗
14. Polymerization shrinkage and elasticity of flowable composites and filled adhesives10.1016/S0109-5641(99)00022-6 ↗
15. Overview: damage in brittle layer structures from concentrated loads10.1557/JMR.2002.0440 ↗
16. Ceramic dental biomaterials and CAD/CAM technology: state of the art10.1016/j.jpor.2014.07.003 ↗
17. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics10.1111/j.1532-849X.2012.00845.x ↗
18. Strength characterization and lifetime prediction of dental ceramic materials10.1016/j.dental.2020.10.015 ↗
19. Influence of the foundation substrate on the fatigue behavior of bonded glass, zirconia polycrystals, and polymer infiltrated ceramic simplified CAD-CAM restorations10.1016/j.jmbbm.2021.104391 ↗
20. Influence of surface treatment of resin composite substrate on the load-bearing capacity under fatigue of lithium disilicate monolithic simplified restorations10.1016/j.jmbbm.2021.104792 ↗
21. Present status and future directions: the restoration of root filled teeth10.1111/iej.13796 ↗
22. All-ceramic computer-aided design and computer-aided manufacturing restorations: evolution of structures and criteria for clinical application10.5005/jp-journals-10024-2549 ↗
23. The marginal seal of class II restorations: flowable composite resin compared to injectable glass ionomer
24. Lithium disilicate glass-ceramic vs translucent zirconia polycrystals bonded to distinct substrates: fatigue failure load, number of cycles for failure, survival rates, and stress distribution10.1016/j.jmbbm.2018.12.010 ↗
25. Polymerization shrinkage, microhardness and depth of cure of Bulk-fill resin composites10.4012/dmj.2018-063 ↗
26. The fracture resistance of all-ceramic crowns on sup- porting structures with different elastic moduli
27. Load-bearing capacity under fatigue and FEA analysis of simplified ceramic restorations supported by Peek or zirconia polycrystals as foundation substrate for implant purposes10.1016/j.jmbbm.2021.104760 ↗
28. Extensive assessment of the physical, mechanical, and adhesion behavior of a low-viscosity bulk-fill composite and a traditional resin composite in tooth cavities10.2341/16-299-L ↗
29. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
30. Crack initiation modes in bilayered alumina/porcelain disks as a function of core/veneer thickness ratio and supporting substrate stiffness10.1177/00220345000790060801 ↗
31. Comparison of physical properties of three commercial composite core build-up materials10.4012/dmj.2018-038 ↗