Optimization of 3-butenoic acid-modified polyalkenoic acid for enhanced glass ionomer cement performance
Source abstract
Abstract
Objective Glass ionomer cements (GICs) suffer from mechanical limitations due to rigid intermolecular hydrogen bonding in polyalkenoic acid (PCA) that impedes ionic cross-linking during setting. This study examined how molecular weight and solution concentration of modified polyalkenoic acid (PCA) containing 3-butenoic acid (VA) spacers at 8 mol% concentration (PCA-VA-8) influence comprehensive GIC performance. Methods PCA-VA-8 polymers with varying molecular weights (5.49 × 104 to 15.57 × 104) were synthesized via free radical copolymerization of acrylic acid, itaconic acid, and 3-butenoic acid by controlling initiator dosage. Experimental GICs were prepared using different PCA-VA-8 concentrations (40-60 wt%) and powder-to-liquid ratios (3.2:1 to 4.0:1). Mechanical properties were evaluated according to ISO 9917-1:2007 standards, while water sorption, solubility, aging resistance, and fluoride release were assessed over 4-week immersion periods. Results The optimal formulation (molecular weight ≈8 × 104, 50 wt% concentration, 3.6:1 powder-to-liquid ratio) achieved enhanced mechanical properties: flexural strength 54.14 ± 5.29 MPa, flexural modulus 19.00 ± 1.06 GPa, and compressive strength 221.35 ± 17.06 MPa (p < 0.05). This formulation showed 33 %-63 % higher flexural strength than commercial Fuji IX-GIC throughout 4-week water aging while maintaining excellent dimensional stability. Water sorption was reduced by 18 %-22 % during initial weeks compared to commercial materials, with solubility remaining comparable to controls (p > 0.05). Fluoride release analysis revealed an initial burst release of 4.1 μg/mL on day 1, followed by stabilization at 0.6-0.9 μg/mL from day 4 onward. Although lower than the initial release of commercial Fuji IX-GIC (6.2 μg/mL), the sustained fluoride levels remained above the therapeutic threshold necessary for remineralization and caries prevention. Significance VA-modified PCA enhances GIC mechanical properties through improved polymer chain flexibility while maintaining clinical requirements for water resistance and fluoride release, representing a promising advancement for next-generation restorative applications.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Polymer composites and self-healing · Dental materials and restorations · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Synthesis of poly(acrylic-co-itaconic acid) through precipitation photopolymerization for glass-ionomer cements: characterization and properties of the cements10.1016/j.dental.2020.03.006 ↗
2. Characteristics of experimental resin-modified glass-ionomer cements, containing alternate monomers to HEMA10.1016/j.dental.2021.08.003 ↗
3. In vitro and ln vivo assessment of newly developed slow-release fluoride glass device10.1007/BF03262728 ↗
4. The role of poly(acrylic acid) in conventional glass polyalkenoate cements10.1515/polyeng-2015-0079 ↗
5. Solution photo-copolymerization of acrylic acid and itaconic acid: the effect of polymerization parameters on mechanical properties of glass ionomer cements10.1016/j.jmbbm.2021.105020 ↗
6. Enhancing mechanical properties of glass ionomer cements with basalt fibers10.1007/s12633-019-00312-4 ↗
7. Mechanical properties and water-aging resistance of glass ionomer cements reinforced with 3-aminopropyltriethoxysilane treated basalt fibers10.1016/j.jmbbm.2021.104369 ↗
8. Effect of incorporating silica-hydroxyapatite-silver hybrid nanoparticles into the resin-modified glass ionomer on the adhesive remnant index score and shear bond strength of orthodontic metal brackets: an in vitro study10.1016/j.ortho.2023.100761 ↗
9. Characterization of glass-ionomer cements 1. Long term hardness and compressive strength10.1016/0300-5712(76)90025-7 ↗
10. Characterization of glass-ionomer cements: 6. A study of erosion and water absorption in both neutral and acidic media10.1016/S0300-5712(80)80046-7 ↗
11. Glass-ionomer dental restoratives10.1016/S0079-6700(01)00006-5 ↗
12. Influence of poly(acrylic acid) content on the fracture behaviour of glass polyalkenoate cements10.1023/A:1004479108367 ↗
13. In vitro cytotoxicity of different dental resin-cements on human cell lines10.1007/s10856-020-06471-w ↗
14. The influence of poly(acrylic) acid number average molecular weight and concentration in solution on the compressive fracture strength and modulus of a glass-ionomer restorative10.1016/j.dental.2011.02.003 ↗
15. Antimicrobial properties of conventional restorative filling materials and advances in antimicrobial properties of composite resins and glass ionomer cements—A literature review10.1016/j.dental.2014.12.005 ↗
16. Prevention and reversal of dental caries: role of low level fluoride10.1111/j.1600-0528.1999.tb01989.x ↗
17. The influence of poly(acrylic acid) molar mass and concentration on the properties of polyalkenoate cements - part II Young's modulus and flexural strength10.1023/A:1012441727897 ↗
18. Incorporation of nanomaterials in glass ionomer cements-recent developments and future perspectives: a narrative review10.3390/nano12213827 ↗
19. Fluoride release from restorative materials and its effects on dentin demineralization10.1177/00220345990780101001 ↗
20. The preventive effect of glass ionomer cement restorations on secondary caries formation: a systematic review and meta-analysis10.1016/j.dental.2023.10.008 ↗
21. A novel glass ionomer cement with silver zeolite for restorative dentistry10.1016/j.jdent.2023.104524 ↗
22. Evaluation of bone-like apatite biomineralization on biomimetic graphene oxide/hydroxyapatite nanocomposite10.1016/j.inoche.2023.110450 ↗
23. The influence of poly(acrylic acid) molecular weight on the fracture toughness of glass-ionomer cements10.1007/BF00660982 ↗
24. ISO · 2007 · vol. 2
25. Preparation of glass ionomer cement using N-acryloyl-substituted amino acid monomers — evaluation of physical properties10.1016/S0109-5641(96)80063-7 ↗
26. Enhancement of the mechanical properties of a dental glass ionomer cement by silica/hydroxyapatite/silver nanocomposite
27. Use of allylbenzene and allyl phenyl ether as chain-transfer agents in radical polymerization10.1023/B:RJAC.0000044130.01483.f7 ↗
28. Factors influencing fluoride release in atraumatic restorative treatment (ART) materials: a review10.1016/j.jobcr.2019.06.015 ↗
29. Size and pH effect on electrical and conformational behavior of poly(acrylic acid): simulation and experiment10.1016/j.eurpolymj.2005.11.023 ↗
30. Ionogel impregnated glass ionomer cement and the effect of nanoparticle additives10.1039/D4MA00592A ↗
31. Evaluation of setting kinetics, mechanical strength, ion release, and cytotoxicity of high-strength glass ionomer cement contained elastomeric micelles10.1186/s12903-024-04468-3 ↗
32. Enhancement of glass ionomer cements through polycarboxylic acid modification with alkylenoic acid spacers10.1002/slct.202500474 ↗
33. Static and dynamic mechanical behavior of engineered cementitious composites with PP and PVA fibers
34. The effect of temperature and ionic solutes on the fluoride release and recharge of glass-ionomer cements10.1016/j.dental.2019.11.018 ↗
35. Fluoride content and recharge ability of five glassionomer dental materials10.1186/1472-6831-8-21 ↗
36. Mechanical properties of polymers: the influence of molecular weight and molecular weight distribution10.1080/15321797208068169 ↗
37. IR and NMR analyses of hardening and maturation of glass-ionomer cement10.1177/00220345960750120201 ↗
38. Matyjaszewski · 2002 · 922
39. The effect of initiator‐to‐monomer ratio on the properties of the polybutadiene‐ol synthesized by free radical solution polymerization of 1, 3‐butadiene10.1002/pi.1172 ↗
40. Synthesis of a proline-modified acrylic acid copolymer in supercritical CO2 for glass-ionomer dental cement applications10.1016/j.actbio.2009.01.037 ↗
41. Effects of N-vinylcaprolactam containing polyelectrolytes on hardness, fluoride release and water sorption of conventional glass ionomers10.1016/S0022-3913(11)60062-0 ↗
42. Effects of N-vinylcaprolactam containing polyelectrolytes on hardness, fluoride release and water sorption of conventional glass ionomers10.1016/S0022-3913(11)60062-0 ↗
43. A review of polyelectrolyte modifications in conventional glass-ionomer dental cements10.1039/c2jm14880c ↗
44. Modifications in glass ionomer cements: nano-sized fillers and bioactive nanoceramics10.3390/ijms17071134 ↗
45. Kinetic studies of water uptake and loss in glass-ionomer cements10.1007/s10856-007-3244-x ↗
46. Enhancing the mechanical properties of glass-ionomer dental cements: a review10.3390/ma13112510 ↗
47. Kinetics of ion release from a conventional glass-ionomer cement10.1007/s10856-021-06501-1 ↗
48. Evaluation of fluoride release in chitosan-modified glass ionomer cements10.1016/j.identj.2022.05.005 ↗
49. Effect of mixing method on the porosity of encapsulated glass ionomer cement10.1016/j.dental.2004.03.001 ↗
50. Odian · 2004
51. The effect of powder to liquid ratio on physical properties and fluoride release of glass ionomer cements containing pre-reacted spherical glass fillers10.4012/dmj.2019-097 ↗
52. Fluoride release from two commercially available dental fluoride gels—in vitro study10.3390/gels11020135 ↗
53. Glass-ionomer cements of improved flexural strength10.1177/00220345860650021101 ↗
54. Compressive strength and fluoride release profile of a glass ionomer cement reinforced with silver-hydroxyapatite-silica hybrid nanoparticles: an in vitro study10.1016/j.ortho.2024.100871 ↗
55. Modifications of polyalkenoic acid and its effect on glass ionomer cement10.1039/D3MA00406F ↗
56. Glass-ionomer cement restorative materials: a sticky subject?10.1111/j.1834-7819.2010.01293.x ↗
57. Evaluation of the flexural strength, water sorption, and solubility of a glass ionomer dental cement modified using phytomedicine10.3390/ma13235352 ↗
58. Standardization · 2018
59. Enhanced remineralisation ability and antibacterial properties of sol-gel glass ionomer cement modified by fluoride containing strontium-based bioactive glass or strontium-containing fluorapatite10.1016/j.dental.2024.02.014 ↗
60. Effect of powder/liquid ratio of glass ionomer cements on flexural and shear bond strengths to dentin
61. A new translucent cement for dentistry. The glass ionomer cement10.1038/sj.bdj.4802810 ↗
62. The influence of polyacid molecular weight on some properties of glass-ionomer cements10.1177/00220345890680021401 ↗
63. The influence of polyacid molecular weight on some properties of glass-ionomer cements10.1177/00220345890680021401 ↗
64. Mechanical properties and microstructures of glass-ionomer cements10.1016/S0109-5641(99)00093-7 ↗
65. Novel amino acid-constructed polyalkenoates for dental glass-ionomer restoratives10.1177/0885328206059797 ↗
66. Preparation and evaluation of a novel glass-ionomer cement with antibacterial functions10.1016/j.dental.2011.02.006 ↗
67. The measure of wear in N-vinyl pyrrolidinone (NVP) modifed glass-ionomer cements10.1002/pat.552 ↗
68. Developing a novel glass ionomer cement with enhanced mechanical and chemical properties10.1016/j.dental.2024.05.019 ↗
69. Star-shape poly(acrylic acid)-composed glass-ionomer cements: effects of MW and arm number on mechanical properties10.1002/app.33451 ↗
70. Improving the mechanical properties of conventional glass ionomer cement through using 4-Pentenoic acid modified polycarboxylic acid (PCA)10.1080/00222348.2022.2078142 ↗