Simulated oral environment affects zirconia aging and mechanical strength
Source abstract
Abstract
Background Zirconia is an emerging alternative to titanium for dental implant systems. However, zirconia surfaces can deteriorate under aqueous conditions, thereby compromising mechanical performance. The goal of this study was to assess the impact of biological exposure or aging simulating the oral cavity on the surface integrity and mechanical strength of surface-treated zirconia. Methods Partially yttria- or magnesia-stabilized zirconia specimens were polished, acid-etched, or sandblasted. Zirconia disks were exposed to mammalian cells or bacteria. Surface degradation via tetragonal-to-monoclinic phase transformation was assessed by Raman microscopy. Zirconia bars were subjected to accelerated aging by exposure to autoclave steam. Surface morphology was examined by scanning electron microscopy, and mechanical strength was measured using four-point bend test loading until failure. Results Early-colonizing oral bacteria significantly increased monoclinic content ∼5-fold on acid-etched yttria-stabilized zirconia versus control (p < 0.05). Surface monoclinic content on acid-etched zirconia increased rapidly (54.6 ± 9.3 %) after 4 h of aging before plateauing (77.0 ± 5.7 %) after 20 h. In contrast, polished or sandblasted zirconia exhibited minimal monoclinic content (∼4 %) after 4 h that gradually increased to ∼40 % by 20 h. Acid-etching treatment significantly reduced the flexural strength of zirconia (585 ± 34 MPa) while sandblasting variants were statistically similar (922 ± 52 MPa) to machined control (921 ± 74 MPa). Aging reduced the flexural strength of machined or sandblasted zirconia, which was significant (p < 0.05) for machined zirconia (782 ± 178 MPa). Conclusions Acid-etching and/or exposure to acidic environment increase zirconia susceptibility to surface degradation, impacting its surface and mechanical properties.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental Implant Techniques and Outcomes · Dental materials and restorations · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Long term fatigue behavior of zirconia based dental ceramics10.3390/ma3052975 ↗
2. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
3. Report on fractures of trilayered all-ceramic fixed dental prostheses10.1016/j.csefa.2016.10.001 ↗
4. Effect of hydrofluoric acid concentration and etching time on the adhesive and mechanical behavior of glass-ceramics: a systematic review and meta-analysis
5. Low temperature degradation of a Y-TZP dental ceramic10.1016/j.actbio.2010.09.020 ↗
6. Titanium particles in peri-implantitis: distribution, pathogenesis and prospects10.1038/s41368-023-00256-x ↗
7. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
8. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
9. Micromechanical properties and microstructure evolution of magnesia partially stabilized zirconia prepared by spark plasma sintering10.1016/j.jeurceramsoc.2022.10.021 ↗
10. Effect of accelerated aging on dental zirconia-based materials10.1016/j.jmbbm.2016.08.023 ↗
11. Flexural strength and crystalline stability of a monolithic translucent zirconia subjected to grinding, polishing and thermal challenges10.1016/j.ceramint.2020.07.114 ↗
12. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
13. Hydrofluoric acid etching of dental zirconia. Part 1: etching mechanism and surface characterization10.1016/j.jeurceramsoc.2015.09.021 ↗
14. Quantification of hydrothermal degradation in zirconia by nanoindentation10.1016/j.actamat.2008.04.050 ↗
15. Biocompatibility of magnesia-partially stabilized zirconia (Mg-PSZ) ceramics10.1007/BF00549808 ↗
16. Zirconia dental implants; the relationship between design and clinical outcome: a systematic review
17. The effect of different aging protocols on the flexural strength and phase transformations of two monolithic zirconia ceramics
18. Long-time aging in 3mol.% yttria-stabilized tetragonal zirconia polycrystals at human body temperature10.1016/j.actbio.2013.09.033 ↗
19. Effect of acid mixtures on surface properties and biaxial flexural strength of as-sintered and air-abraded zirconia10.3390/ma14092359 ↗
20. The effect of zirconia and titanium surfaces on biofilm formation and on host-derived immunological parameters10.1016/j.ijom.2021.01.021 ↗
21. Low-temperature degradation of different zirconia ceramics for dental applications10.1016/j.actbio.2011.11.016 ↗
22. The effects of dental grinding and sandblasting on ageing and fatigue behavior of dental zirconia (Y-TZP) ceramics10.1016/j.jeurceramsoc.2007.09.013 ↗
23. The influence of polishing on the mechanical properties of zirconia—a systematic review10.3390/oral3010010 ↗
24. Scientific trends in clinical Research on zirconia dental implants: a bibliometric review10.3390/ma13235534 ↗
25. Influence of yttria content and surface treatment on the strength of translucent zirconia materials10.1016/j.prosdent.2021.07.001 ↗
26. Clinical outcomes of zirconia implants: a systematic review and meta-analysis10.1007/s00784-023-05401-8 ↗
27. Influence of aging on biaxial flexural strength and hardness of translucent 3Y-TZP10.3390/ma13010027 ↗
28. Monoclinic phase transformation and mechanical durability of zirconia ceramic after fatigue and autoclave aging10.1002/jbm.b.33720 ↗
29. The effects of mechanical and hydrothermal aging on microstructure and biaxial flexural strength of an anterior and a posterior monolithic zirconia10.1016/j.jdent.2017.05.021 ↗
30. Quantitative analysis of monoclinic phase in 3Y-TZP by Raman spectroscopy10.1111/j.1551-2916.2010.03635.x ↗
31. Fractured zirconia implants and related implant designs: scanning electron microscopy analysis10.1111/j.1600-0501.2011.02411.x ↗
32. Survival and success of zirconia compared with titanium implants: a systematic review and meta-analysis10.1007/s00784-023-05242-5 ↗
33. Histologic osseointegration level comparing titanium and zirconia dental implants: meta-analysis of preclinical studies10.11607/jomi.10142 ↗
34. Titanium corrosion mechanisms in the oral environment: a retrieval study10.3390/ma6115258 ↗
35. Spectroscopic and microscopic investigation of the effects of bacteria on dental implant surfaces10.1039/C6RA07760A ↗
36. Phase transformation, roughness, and microhardness of artificially aged yttria‐ and magnesia‐stabilized zirconia femoral heads10.1002/jbm.a.31438 ↗
37. Do zirconia dental implants present better clinical results than titanium dental implants? A systematic review and meta-analysis10.1016/j.jormas.2022.10.023 ↗
38. Effect of hydrothermal, chemical, and mechanical degradation on flexural strength and phase transformation of ground, glazed, and polished zirconia
39. Assessment of low-temperature degradation of Y-TZP ceramics based on Raman-spectroscopic analysis and hardness indentation10.1016/j.jeurceramsoc.2014.07.018 ↗
40. Zirconia surface modifications for implant dentistry10.1016/j.msec.2019.01.062 ↗
41. Evaluation of oral microbial corrosion on the surface degradation of dental implant materials10.1002/JPER.18-0110 ↗
42. Can oral bacteria and mechanical fatigue degrade zirconia dental implants in vitro?10.1021/acsbiomaterials.9b00223 ↗
43. Biological characterization of surface-treated dental implant materials in contact with mammalian host and bacterial cells: titanium versus zirconia10.1039/C9RA06010C ↗
44. Succession of oral bacterial colonizers on dental implant materials: an in vitro biofilm model10.1016/j.dental.2021.12.021 ↗
45. Wear and corrosion interactions at the titanium/zirconia interface: dental implant application10.1111/jopr.12769 ↗
46. Is zirconia a viable alternative to titanium for oral implant? A critical review10.1016/j.jpor.2017.07.003 ↗
47. Effect of hydrofluoric acid concentration and etching duration on select surface roughness parameters for zirconia10.1016/j.prosdent.2015.01.001 ↗
48. The lactic acid fermentation of Streptococci10.1128/jb.43.6.725-731.1942 ↗
49. Dental zirconia can be etched by hydrofluoric acid10.4012/dmj.2013-243 ↗
50. Surface modifications for zirconia dental implants: a review10.3389/fdmed.2021.733242 ↗
51. Influence of surface modifications on the fracture resistance of aged zirconia implants: a systematic review of in vitro experimental studies10.1016/j.ajoms.2023.06.001 ↗
52. Effects of acid treatment on dental zirconia: an in vitro study
53. Effects of low-temperature degradation on the surface roughness of yttria-stabilized tetragonal zirconia polycrystal ceramics: a systematic review and meta-analysis10.1016/j.prosdent.2020.01.005 ↗
54. Evaluation of structural stability, mechanical properties, and corrosion resistance of magnesia partially stabilized zirconia (Mg-PSZ)10.3390/molecules28166054 ↗
55. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
56. Yttrium ion release and phase transformation in yttria-stabilized zirconia under acidic conditions: implications for dental implant durability10.3390/ma18143311 ↗
57. Hardness and indentation fracture toughness of slip cast alumina and alumina-zirconia ceramics10.3390/ma13010122 ↗