journal article·2017-07

Atomistic origin of size effects in fatigue behavior of metallic glasses

Zhendong Sha, Wei Hin Wong, Qingxiang Pei, Paulo Sergio Branicio, Zishun Liu, Tiejun Wang, Tianfu Guo, Huajian Gao

Publisher page

Abstract

Abstract While many experiments and simulations on metallic glasses (MGs) have focused on their tensile ductility under monotonic loading, the fatigue mechanisms of MGs under cyclic loading still remain largely elusive. Here we perform molecular dynamics (MD) and finite element simulations of tension-compression fatigue tests in MGs to elucidate their fatigue mechanisms with focus on the sample size effect. Shear band (SB) thickening is found to be the inherent fatigue mechanism for nanoscale MGs. The difference in fatigue mechanisms between macroscopic and nanoscale MGs originates from whether the SB forms partially or fully through the cross-section of the specimen. Furthermore, a qualitative investigation of the sample size effect suggests that small sample size increases the fatigue life while large sample size promotes cyclic softening and necking. Our observations on the size-dependent fatigue behavior can be rationalized by the Gurson model and the concept of surface tension of the nanovoids. The present study sheds light on the fatigue mechanisms of MGs and can be useful in interpreting previous experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Material Dynamics and Properties · Glass properties and applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. A transition from localized shear banding to homogeneous superplastic flow in nanoglass10.1063/1.4833018 ↗
2. Craze initiation in glassy polymers - Revisited10.1016/j.polymer.2011.03.019 ↗
3. Suppression of repeated adiabatic shear banding by dynamic large strain extrusion machining10.1016/j.jmps.2014.09.004 ↗
4. Fatigue damage in bulk metallic glass I: simulation10.1016/j.scriptamat.2005.10.006 ↗
5. Structural processes that initiate shear localization in metallic glass10.1016/j.actamat.2009.07.016 ↗
6. Effects of size on the mechanical response of metallic glasses investigated through in situ TEM bending and compression experiments10.1016/j.actamat.2009.08.070 ↗
7. Intrinsic size effects in the mechanical response of taper-free nanopillars of metallic glass10.1103/PhysRevB.83.180201 ↗
8. Local order influences initiation of plastic flow in metallic glass: effects of alloy composition and sample cooling history10.1016/j.actamat.2008.07.011 ↗
9. The structure of shear bands in metallic glasses10.1016/0001-6160(81)90177-2 ↗
10. Cyclic compression behavior of a Cu-Zr-Al-Ag bulk metallic glass10.1016/j.intermet.2011.03.023 ↗
11. Fatigue of a Zr-Ti-Cu-Ni-Be bulk amorphous metal: stress/life and crack-growth behavior10.1016/S1359-6462(97)00522-8 ↗
12. Shear bands in metallic glasses10.1016/j.mser.2013.04.001 ↗
13. Plasticity in small-sized metallic systems: intrinsic versus extrinsic size effect10.1016/j.pmatsci.2011.01.005 ↗
14. Warp3D—release 13.5
15. Thermal and vapor pressure effects on cavitation and void growth10.1023/A:1012924626044 ↗
16. Modeling vapor pressure effects on void rupture and crack growth resistance10.1016/S1359-6454(02)00162-3 ↗
17. Vapor pressure and void size effects on failure of a constrained ductile film10.1016/S0022-5096(03)00007-3 ↗
18. Continuum theory of ductile rupture by void nucleation and growth: Part I—yield criteria and flow rules for porous ductile materials10.1115/1.3443401 ↗
19. Accelerated molecular dynamics: a promising and efficient simulation method for biomolecules10.1063/1.1755656 ↗
20. Fatigue damage in bulk metallic glass II: experiments10.1016/j.scriptamat.2005.10.007 ↗
21. Examining the initial stages of shear localization in amorphous metals10.1016/j.actamat.2013.09.050 ↗
22. Inhomogeneous deformation in metallic glasses10.1016/S0022-5096(01)00115-6 ↗
23. A note on the effect of surface energy and void size to void growth10.1016/S0997-7538(99)00133-3 ↗
24. Fatigue deformation of microsized metallic glasses10.1016/j.scriptamat.2012.12.011 ↗
25. Transition from a strong-yet-brittle to a stronger-and-ductile state by size reduction of metallic glasses10.1038/nmat2622 ↗
26. Effects of size on the strength and deformation mechanism in Zr-based metallic glasses10.1016/j.ijplas.2010.09.010 ↗
27. On the origin of shear banding instability in metallic glasses10.1016/j.jmps.2009.04.008 ↗
28. 3D metallic glass cellular structures10.1016/j.actamat.2015.11.057 ↗
29. Structural relaxation and self-repair behavior in nano-scaled Zr-Cu metallic glass under cyclic loading: molecular dynamics simulations10.1016/j.intermet.2010.01.012 ↗
30. Low-cycle fatigue of metallic glass nanowires10.1016/j.actamat.2014.12.038 ↗
31. Shear-band dynamics in metallic glasses10.1002/adfm.201404223 ↗
32. Tunable tensile ductility in metallic glasses10.1038/srep01096 ↗
33. Stress-life fatigue behavior of a Zr-based bulk metallic glass10.1016/j.actamat.2005.10.021 ↗
34. Fatigue crack initiation and small-crack propagation in Zr-based bulk metallic glass10.2320/matertrans.MJ200758 ↗
35. Fast parallel algorithms for short-range molecular-dynamics10.1006/jcph.1995.1039 ↗
36. Macroscopic tensile plasticity of bulk metallic glass through designed artificial defects10.1016/j.msea.2011.11.082 ↗
37. Designing tensile ductility in metallic glasses10.1038/ncomms3158 ↗
38. From brittle to ductile: density optimization for Zr-BMG cellular structures10.1016/j.scriptamat.2013.02.030 ↗
39. Overview No. 144 - mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
40. Statistical composition-structure-property correlation and glass-forming ability based on the full icosahedra in Cu-Zr metallic glasses10.1063/1.3310278 ↗
41. Effect of aspect ratio on the mechanical properties of metallic glasses10.1016/j.scriptamat.2014.08.025 ↗
42. On the notch sensitivity of CuZr metallic glasses10.1063/1.4819099 ↗
43. Cyclic deformation in metallic glasses10.1021/acs.nanolett.5b03045 ↗
44. Compression-compression fatigue study on model metallic glass nanowires by molecular dynamics simulations10.1063/1.3610443 ↗
45. Cavitation in materials with distributed weak zones: implications on the origin of brittle fracture in metallic glasses10.1016/j.jmps.2012.12.001 ↗
46. Notch sensitivity in nanoscale metallic glass specimens: insights from continuum simulations10.1016/j.jmps.2015.10.001 ↗
47. Cavitation-induced fracture causes nanocorrugations in brittle metallic glasses10.1103/PhysRevLett.117.044302 ↗
48. Structure-property relationships in nanoporous metallic glasses10.1016/j.actamat.2015.12.026 ↗
49. The fracture of bulk metallic glasses10.1016/j.pmatsci.2015.05.002 ↗
50. Room temperature homogeneous ductility of micrometer-sized metallic glass10.1002/adma.201401123 ↗
51. Influence of voids on shear band instabilities under plane strain condition10.1007/BF00036191 ↗
52. Real-time, high-resolution study of nanocrystallization and fatigue cracking in a cyclically strained metallic glass10.1073/pnas.1320235110 ↗
53. Fatigue behavior and fracture morphology of Zr 50 Al 10 Cu 40 and Zr 50 Al 10 Cu 30 Ni 10 bulk-metallic glasses10.1016/j.intermet.2004.04.038 ↗
54. Progress in studying the fatigue behavior of Zr-based bulk-metallic glasses and their composites10.1016/j.intermet.2009.01.017 ↗
55. Size effects on the fatigue behavior of bulk metallic glasses10.1063/1.3664846 ↗
56. Bulk metallic glasses10.1016/j.mser.2004.03.001 ↗
57. Shear band-mediated fatigue cracking mechanism of metallic glass at high stress level10.1016/j.msea.2015.01.008 ↗
58. Shear band propagation and plastic softening of metallic glass under cyclic compression10.1016/j.jallcom.2016.11.039 ↗
59. Notch fatigue behavior: metallic glass versus ultra-high strength steel10.1038/srep35557 ↗
60. Densification and strain hardening of a metallic glass under tension at room temperature10.1103/PhysRevLett.111.135504 ↗
61. High-speed imaging of a bulk metallic glass during uniaxial compression10.1063/1.4811744 ↗
62. Fatigue-strength enhancement of cast Zr50Cu40Al10 glassy alloys10.2320/matertrans.47.1286 ↗
63. Effect of surface energy on the yield strength of nanoporous materials