A phase field electro-chemo-mechanical formulation for predicting void evolution at the Li–electrolyte interface in all-solid-state batteries
Source abstract
Abstract
We present a mechanistic theory for predicting void evolution in the Li metal electrode during the charge and discharge of all-solid-state battery cells. A phase field formulation is developed to model vacancy annihilation and nucleation, and to enable the tracking of the void-Li metal interface. This is coupled with a viscoplastic description of Li deformation, to capture creep effects, and a mass transfer formulation accounting for substitutional (bulk and surface) Li diffusion and current-driven flux. Moreover, we incorporate the interaction between the electrode and the solid electrolyte, resolving the coupled electro-chemical-mechanical problem in both domains. This enables predicting the electrolyte current distribution and thus the emergence of local current ‘hot spots’, which act as precursors for dendrite formation and cell death. The theoretical framework is numerically implemented, and single and multiple void case studies are carried out to predict the evolution of voids and current hot spots as a function of the applied pressure, material properties and charge (magnitude and cycle history). For both plating and stripping, insight is gained into the interplay between bulk diffusion, Li dissolution and deposition, creep, and the nucleation and annihilation of vacancies. The model is shown to capture the main experimental observations, including not only key features of electrolyte current and void morphology but also the sensitivity to the applied current, the role of pressure in increasing the electrode–electrolyte contact area, and the dominance of creep over vacancy diffusion.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. An elastic-viscoplastic model for lithium10.1149/2.0861906jes ↗
2. Phase field modeling for the morphological and microstructural evolution of metallic materials under environmental attack10.1038/s41524-021-00612-7 ↗
3. A cosserat crystal plasticity and phase field theory for grain boundary migration10.1016/j.jmps.2018.03.006 ↗
4. Numerical experiments in revisited brittle fracture10.1016/S0022-5096(99)00028-9 ↗
5. Lithium metal electrode kinetics and ionic conductivity of the solid lithium ion conductors Li7La3Zr2O12 and Li7-xLa3Zr2-xTaxO12 with garnet-type structure10.1016/j.jpowsour.2012.01.094 ↗
6. Phase-field study of dendritic morphology in lithium metal batteries
7. Modulation of dendritic patterns during electrodeposition: A nonlinear phase-field model10.1016/j.jpowsour.2015.09.055 ↗
8. Overview (2) non-equilibrium models for diffusive cavitation of grain interfaces10.1016/0001-6160(79)90021-X ↗
9. A phase field formulation for dissolution-driven stress corrosion cracking10.1016/j.jmps.2020.104254 ↗
10. Ductile fracture by vacancy condensation in f.c.c. single crystals10.1016/1359-6454(95)00220-0 ↗
11. Failure mode of lithium metal batteries with a block copolymer electrolyte analyzed by X-ray microtomography10.1149/2.0721507jes ↗
12. Self-diffusion barriers: Possible descriptors for dendrite growth in batteries?10.1039/C8EE01448E ↗
13. A solid future for battery development10.1038/nenergy.2016.141 ↗
14. Critical stripping current leads to dendrite formation on plating in lithium anode solid electrolyte cells10.1038/s41563-019-0438-9 ↗
15. Dendritic cracking in solid electrolytes driven by lithium insertion10.1016/j.jpowsour.2019.227226 ↗
16. Toward a fundamental understanding of the lithium metal anode in solid-state batteries - an electrochemo-mechanical study on the garnet-type solid electrolyte Li 6.25 Al 0.25 La 3 Zr 2 O 1210.1021/acsami.9b02537 ↗
17. A phase field model for elastic-gradient-plastic solids undergoing hydrogen embrittlement10.1016/j.jmps.2020.104093 ↗
18. An assessment of phase field fracture: crack initiation and growth10.1098/rsta.2021.0021 ↗
19. Lithium mechanics: Roles of strain rate and temperature and implications for lithium metal batteries10.1149/2.0221902jes ↗
20. Phase field crystal modeling of grain boundary structures and growth in polycrystalline graphene10.1016/j.jmps.2017.12.013 ↗
21. Reviving the lithium metal anode for high-energy batteries10.1038/nnano.2017.16 ↗
22. Wrinkling and ratcheting of a thin film on cyclically deforming plastic substrate: Mechanical instability of the solid-electrolyte interphase in Li–ion batteries10.1016/j.jmps.2018.08.006 ↗
23. Interfacial stability of li metal-solid electrolyte elucidated via in situ electron microscopy10.1021/acs.nanolett.6b03223 ↗
24. Mechanical failure of garnet electrolytes during li electrodeposition observed by in-operando microscopy10.1016/j.jpowsour.2018.11.041 ↗
25. Dendrite growth in lithium/polymer systems10.1149/1.1606686 ↗
26. The effect of interfacial deformation on electrodeposition kinetics10.1149/1.1710893 ↗
27. The impact of elastic deformation on deposition kinetics at lithium/polymer interfaces10.1149/1.1850854 ↗
28. A large deformation elastic–viscoplastic model for lithium10.1016/j.eml.2018.08.006 ↗
29. On modeling the detrimental effects of inhomogeneous plating-and-stripping at a lithium-metal/solid-electrolyte interface in a solid-state-battery10.1149/1945-7111/ab75c1 ↗
30. Effect of prestress on the stability of electrode-electrolyte interfaces during charging in lithium batteries10.1016/j.jmps.2016.05.007 ↗
31. Plastic creep flow effects in the diffusive cavitation of grain boundaries
32. Interactions are important: Linking multi-physics mechanisms to the performance and degradation of solid-state batteries10.1016/j.mattod.2021.02.011 ↗
33. Journal of physics : Energy 2020 roadmap on solid-state batteries10.1088/2515-7655/ab95f4 ↗
34. Mechanism of lithium metal penetration through inorganic solid electrolytes10.1002/aenm.201701003 ↗
35. Current limit diagrams for dendrite formation in solid-state electrolytes for Li-ion batteries10.1016/j.jpowsour.2017.01.037 ↗
36. Direct observation of lithium dendrites inside garnet-type lithium-ion solid electrolyte10.1016/j.elecom.2015.05.001 ↗
37. A consistent framework for chemo-mechanical cohesive fracture and its application in solid-state batteries10.1016/j.jmps.2021.104612 ↗
38. An assessment of a mechanism for void growth in Li anodes10.1016/j.eml.2021.101307 ↗
39. More pressure needed10.1038/s41560-019-0478-z ↗
40. In-situ, non-destructive acoustic characterization of solid state electrolyte cells10.1016/j.jpowsour.2016.05.062 ↗
41. The initiation of void growth during stripping of Li electrodes in solid electrolyte cells
42. Dendrites as climbing dislocations in ceramic electrolytes: Initiation of growth10.1016/j.jpowsour.2020.227989 ↗
43. Growth rate of lithium filaments in ceramic electrolytes10.1016/j.actamat.2020.06.060 ↗
44. Sodium/Na β alumina interface: Effect of pressure on voids10.1021/acsami.9b17786 ↗
45. Characterizing the Li-solid-electrolyte interface dynamics as a function of stack pressure and current density10.1016/j.joule.2019.06.017 ↗
46. Creep-enabled 3D solid-state lithium-metal battery10.1016/j.chempr.2020.09.005 ↗
47. Current status and future directions of all-solid-state batteries with lithium metal anodes, sulfide electrolytes, and layered transition metal oxide cathodes10.1016/j.nanoen.2021.106081 ↗
48. Elastic properties of the solid electrolyte Li7La3Zr2O12 (LLZO)10.1021/acs.chemmater.5b03854 ↗
49. A compliant and low-expansion 2-phase micro-architectured material, with potential application to solid-state li-ion batteries10.1016/j.jmps.2021.104683 ↗