Oxide growth and stress evolution underneath cracked environmental barrier coatings

Stephen Sehr, Virginia Collier, Frank Zok, Matthew R. Begley

Abstract

SiC composites at elevated temperatures are prone to oxidation, prompting the use of environmental barrier coatings to limit or prevent the ingress of oxidants. Cracks in such coatings can provide fast diffusion pathways that can lead to accelerated local oxide growth. The localized oxide confined at the tip of such features generates significant stress due to the large molar volume change associated with converting SiC to SiO2. In this work, a multi-physics computational framework is used to simulate the evolution of such internal oxide domains; the framework integrates analyses of oxidant transport, oxide growth (domain evolution) in dry air environments and stress evolution mitigated by creep. Significant insights regarding oxidation-driven damage are obtained from a broad parametric study involving the crack opening, the effective diffusivity of the coating, the crack spacing and the magnitude of applied loads. (i) Oxide growth at the tip of the crack is comparable to that of a bare surface; even very narrow open channels lead to rapid, localized oxidation. (ii) Coatings with low diffusivity produce highly confined oxide ‘bubbles’ at the tip of the crack; confinement produces high compressive stresses in the oxide and significant tensile stresses in the surrounding material. Stresses along the coating/substrate interface and in the substrate beneath the bubble can be 2–7 times those arising from mechanical loading alone, promoting coating decohesion and substrate cracking. (iii) Significant applied stress reduces high hydrostatic stresses in the oxide and mitigate the stress elevation associated with local oxidation. The paper concludes with a brief discussion of the implications of these observations for damage mechanisms occurring at elevated temperature, and indicate the importance of further study of the impact of wet environments and different oxide compositions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Semiconductor materials and devices · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Begley · 2017
2. A coupled mechanical-chemical model for reflecting the influence of stress on oxidation reactions in thermal barrier coating10.1063/1.5019848 ↗
3. Oxidation kinetics of silicon carbide crystals and ceramics: I, in dry oxygen10.1111/j.1151-2916.1986.tb07470.x ↗
4. Mechanical properties testing and results for thermal barrier coatings10.1007/BF02646313 ↗
5. General relationship for the thermal oxidation of silicon10.1063/1.1713945 ↗
6. Viscosity of silica10.1063/1.1515132 ↗
7. Oxidation behavior of chemically-vapor-deposited silicon carbide and silicon nitride from 1200 to 1600 c10.1111/j.1151-2916.1998.tb02431.x ↗
8. Recent advances in models for thermal oxidation of silicon10.1006/jcph.2001.6884 ↗
9. Growth stress in SiO 2 during oxidation of SiC fibers10.1063/1.3698305 ↗
10. Environmental effects of ceramics and composites
11. Model for SiC fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
12. Viscosity of vitreous silica
13. Oxidation and corrosion of ceramics and ceramic matrix composites10.1016/S1359-0286(01)00009-2 ↗
14. Protective coatings for gas turbines 4.4.2-1 Introduction
15. Elastic response of thermal spray deposits under indentation tests10.1111/j.1151-2916.1997.tb03093.x ↗
16. Relationships between the microstructure and properties of thermally sprayed deposits10.1361/105996302770348754 ↗
17. Potential application of ceramic matrix composites to aero-engine components10.1016/S1359-835X(98)00139-0 ↗
18. Variation on the oxidation rate of silicon carbide with vapour pressure10.1111/j.1151-2916.1999.tb01810.x ↗
19. The hotter the engine, the better10.1126/science.1179327 ↗
20. Poirier · 2016
21. Passive-oxidation kinetics of high-purity silicon carbide from 800°C to 1100°C10.1111/j.1151-2916.1996.tb08724.x ↗
22. On modelling thermal oxidation of Silicon I: Theory10.1002/(SICI)1097-0207(20000110/30)47:1/3<341::AID-NME774>3.0.CO;2-Z ↗
23. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor10.1111/jace.13792 ↗
24. Fracture mechanisms of ytterbium monosilicate environmental barrier coatings during cyclic thermal exposure10.1016/j.actamat.2015.10.019 ↗
25. Response of ytterbium disilicate-silicon environmental barrier coatings to thermal cycling in water vapor10.1016/j.actamat.2015.12.053 ↗
26. Sehr · 2020
27. An integrated analysis of transport, oxidation, and creep during oxidation of interior pores in SiC
28. Triangle: Engineering a 2D quality mesh generator and delaunay triangulator
29. Delaunay refinement algorithms for triangular mesh generation10.1016/S0925-7721(01)00047-5 ↗
30. Reformulation of oxide growth equations for oxidation of silicon bond coat in environmental barrier coating systems10.1016/j.jeurceramsoc.2019.06.057 ↗
31. A coupled model of stress, creep, and diffusion in the film/substrate system10.1063/5.0018968 ↗
32. Model of oxidation-induced fiber fracture in SiC/SiC composites10.1111/jace.13180 ↗
33. Ceramic-matrix composites enable revolutionary gains in turbine engine efficiency
34. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗