The influence of mean strain on the high-cycle fatigue of Nitinol with application to medical devices
Source abstract
Abstract
One of the contentious issues associated with the high-cycle fatigue of Nitinol, a nominally equiatomic alloy of nickel and titanium, is the claim that increasing the applied mean strain can increase, or at least have no negative impact, on the fatigue lifetime, in conflict with reported behavior for the vast majority of other metallic materials. To investigate this in further detail, cyclic fatigue tests in bending were carried out on electropolished medical grade Nitinol at 37 °C for lives of up to 400 million cycles of strain involving various levels of the mean strain. A constant life model was developed through statistical analysis of the fatigue data, with 90% reliability at a confidence level of 95% on the effective fatigue strain. Our results show that the constant life diagram, a plot of strain amplitude versus mean strain, is monotonic yet nonlinear for lives of 400 million cycles of fatigue loading. Specifically, we find that in contradiction to the aforementioned claim, the strain amplitude limit at zero mean strain is 0.55% to achieve a 400 million cycle lifetime, at 90% reliability with 95% confidence; however, to achieve the same lifetime, reliability and confidence level in the presence of a 3% or more mean strain, the required strain amplitude limit is decreased by over a factor of three to 0.16%. Moreover, for mean strains from 3% to 7%, the strain amplitude limit that allows a 400 million cycle lifetime, at 90% reliability with 95% confidence, is ~ 0.16%, and essentially independent of mean strain. We conclude that the debatable claim that an increase in the applied mean strain can increase the fatigue life of Nitinol components is not supported by the current data.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Shape-memory alloys: modelling and numerical simulations of the finite-strain superelastic behavior10.1016/S0045-7825(96)01147-4 ↗
2. Shape-memory alloys: macromodelling and numerical simulations of the superelastic behavior10.1016/S0045-7825(96)01232-7 ↗
3. The exponential law of endurance tests
4. In vivo MR angiographic quantification of axial and twisting deformations of the superficial femoral artery resulting from maximum hip and knee flexion10.1097/01.RVI.0000220367.62137.E8 ↗
5. A study of the effect of cyclic thermal stresses on ductile metal
6. Duerig · 1990
7. An overview of nitinol medical applications10.1016/S0921-5093(99)00294-4 ↗
8. Inferior vena cava filters: analysis of five currently available devices
9. High compressive pre-strains reduce the bending fatigue life of nitinol wire10.1016/j.jmbbm.2014.12.007 ↗
10. Statistical modeling of high cycle fatigue with censored data10.1520/MPC20150053 ↗
11. Hertzberg · 1996
12. Bard Recovery filters: evaluation and management of vena cava limb perforation, fracture and migration10.1016/j.jvir.2008.09.032 ↗
13. Bending of pseudoelastic NiTi tubes10.1016/j.ijsolstr.2017.06.032 ↗
14. Fatigue life of Ti-50 at% Ni and Ti-40Ni-10Cu (at%) shape memory alloy wires
15. Influence of breathing movements and Valsalva maneuver on vena caval dynamics10.4329/wjr.v6.i10.833 ↗
16. Safety and efficacy of a self-expanding versus a balloon-expandable bioprosthesis for transcatheter aortic valve replacement in patients with symptomatic severe aortic stenosis: a randomised non-inferiority trial10.1016/S0140-6736(19)32220-2 ↗
17. In situ EBSD investigations of the asymmetric stress-induced martensitic transformation in TiNi shape memory alloys under bending10.1016/j.msea.2008.07.072 ↗
18. Meeker · 1998
19. Meyer · 1965
20. Milnor · 1982
21. Fundamentals of modern fatigue analysis for design
22. Fatigue life of Ti-50 at% Ni and Ti-40Ni-10Cu (at%) shape memory alloy wires10.1016/S0921-5093(99)00344-5 ↗
23. Mean strain effects and microstructural observations during in vitro fatigue testing of NiTi
24. Evaluation of wall motion and dynamic geometry of the inferior vena cava using intravascular ultrasound: implications for future device design10.1583/08-2424.1 ↗
25. Nelson · 1990
26. Physical metallurgy of Ti-Ni-based shape memory alloys10.1016/j.pmatsci.2004.10.001 ↗
27. Nitinol fatigue: a review of microstructures and mechanisms10.1007/s11665-011-9864-9 ↗
28. Optimisation of processing and properties of medical-grade Nitinol wire10.3109/13645700009063057 ↗
29. Fatigue testing of diamond-shaped specimens
30. Fatigue and durability of nitinol stents10.1016/j.jmbbm.2007.08.001 ↗
31. The influence of melt practice on final fatigue properties of superelastic NiTi wires
32. Mechanical fatigue and fracture of Nitinol10.1179/1743280411Y.0000000009 ↗
33. Application of classical fatigue and fatigue-to-fracture techniques for very-high-cycle life qualification of cardiac devices
34. Effect of prestrain on the fatigue life of superelastic Nitinol10.1007/s11665-019-04334-2 ↗
35. Fatigue reliability analysis framework for medical devices based on a probabilistic finite element approach
36. Hydrogen effects on nitinol fatigue
37. Self-expanding Nitinol stents: material and design considerations10.1007/s00330-003-2022-5 ↗
38. Stulen, F.B., 1965. Fatigue life data displayed by a single quantity relating alternating and mean stress, technical report AFML-TR-65-121, Air Force Materials Laboratory, Wright-Patterson Air Force Base OH.
39. Suresh · 1998
40. Mean stress effects on fatigue of NiTi10.1016/S0921-5093(99)00340-8 ↗
41. Mean strain effects on the fatigue properties of superelastic NiTi10.1007/s11661-001-0164-0 ↗
42. Cyclic properties of superelastic nitinol: design implications
43. Finite element framework for fatigue performance assessment of superelastic Nitinol used in medical devices
44. Weibull · 1961
45. Bending fatigue characteristics of nitinol