Abstract
The mechanical properties of brick-and-mortar composites depend on their interface fracture properties, which have not been evaluated to date, preventing a rational optimization of the microstructure and of the resulting mechanical properties. Micro-(cantilever) and macro-scale (Single Edge Notched Bending) tests on nacre-like alumina both result in crack initiation at the interface between the platelets. We assess crack initiation and predict the failure force by means of 2D and 3D finite element simulations employing the same fracture modeling approach at both scales, namely the coupled criterion. The interface fracture properties are determined by means of inverse identification based on both micro-and macro-scale experiments. The interface exhibits typical values of 625 MPa tensile strength and 1.9 J/m 2 toughness. The forces at crack initiation predicted employing these parameters are in good agreement with the forces measured experimentally for both micro-and macro-scale tests. The quantitative determination of the interface fracture properties should help the design and optimization of this class of brick-and-mortar materials.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Calcium Carbonate Crystallization and Inhibition · Bone Tissue Engineering Materials · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Discrete-element modeling of nacre-like materials: effects of random microstructures on strain localization and mechanical performance10.1016/j.jmps.2017.11.003 ↗
2. Designing nacre-like materials for simultaneous stiffness, strength, and toughness: optimum materials, composition, microstructure and size10.1016/j.jmps.2014.08.008 ↗
3. An experimental investigation of deformation and fracture of nacre-mother of pearl10.1007/s11340-007-9040-1 ↗
4. On the mechanics of mother-of-pearl: a key feature in the material hierarchical structure10.1016/j.jmps.2006.07.007 ↗
5. Micromechanical models to guide the development of synthetic brick and mortar composites10.1016/j.jmps.2012.03.002 ↗
6. Strong and tough nacre-like aluminas: process-structure-performance relationships and position within the nacre-inspired composite landscape
7. Strong, tough and stiff bioinspired ceramics from brittle constituents10.1038/nmat3915 ↗
8. Comparison between models based on a coupled criterion for the prediction of the failure of adhesively bonded joints10.1016/j.engfracmech.2015.03.004 ↗
9. The mechanical behaviour of some molluscan hard tissues10.1111/j.1469-7998.1974.tb04122.x ↗
10. Tough and stiff composites with simple building blocks10.1557/jmr.2013.88 ↗
11. Experimental characterization and numerical modeling of crack initiation in rhombus hole pmma specimens under compression10.1016/j.euromechsol.2019.04.013 ↗
12. Damage onset modeling in woven composites based on a coupled stress and energy criterion10.1016/j.engfracmech.2016.11.021 ↗
13. Mesoscale analysis of damage growth in woven composites10.1016/j.compositesa.2017.02.018 ↗
14. Revisiting the strength of micron-scale ceramic platelets10.1111/jace.17148 ↗
15. Uo2 micron scale specimen fracture: parameter identification and influence of porosities10.1016/j.tafmec.2020.102665 ↗
16. 3D application of the coupled criterion to crack initiation prediction in epoxy/aluminum specimens under four point bending10.1016/j.ijsolstr.2018.03.005 ↗
17. Comparison between 2D and 3D applications of the coupled criterion to crack initiation prediction in scarf adhesive joints10.1016/j.ijadhadh.2018.05.022 ↗
18. Numerical modeling of the nucleation of facets ahead of a primary crack under modeI+III10.1007/s10704-018-0305-8 ↗
19. Numerical implementation of the coupled criterion: matched asymptotic and full finite element approaches10.1016/j.finel.2019.103344 ↗
20. 3D printing bioinspired ceramic composites10.1038/s41598-017-14236-9 ↗
21. Micromechanical strength of al2o3 platelets10.1016/j.scriptamat.2017.01.008 ↗
22. Predicting crack patterns at bi-material junctions: acoupled stress and energy approach10.1016/j.ijsolstr.2019.01.015 ↗
23. Interface failure in nacre-like alumina10.1016/j.jeurceramsoc.2020.05.068 ↗
24. Magnetically assisted slip casting of bioinspired heterogeneous composites
25. Strength or toughness? A criterion for crack onset at a notch10.1016/S0997-7538(01)01184-6 ↗
26. Interface crack onset at a circular cylindrical inclusion under a remote transverse tension. application of a coupled stress and energy criterion10.1016/j.ijsolstr.2008.10.036 ↗
27. Crack onset and growth at the fibre-matrix interface under a remote biaxial transverse load. Application of a coupled stress and energy criterion10.1016/j.ijsolstr.2012.04.023 ↗
28. A twofold strength and toughness criterion for the onset of free-edge shear delamination in angle ply laminates10.1016/j.ijsolstr.2010.01.018 ↗
29. A coupled strength and toughness criterion for the prediction of the open hole tensile strength of a composite plate10.1016/j.ijsolstr.2012.08.020 ↗
30. Using graphene networks to build bioinspired self-monitoring ceramics10.1038/ncomms14425 ↗
31. Failure mode transition in nacre and bone-like materials.10.1016/j.actbio.2010.04.008 ↗
32. Strength and toughness trade-off optimization of nacre-like ceramic composites10.1016/j.compositesb.2019.107699 ↗
33. A numerical implementation of the coupled criterion of finite fracture mechanics for elastic interfaces10.1016/j.tafmec.2020.102607 ↗
34. A simple approach to bulk bioinspired tough ceramics
35. A model for brittle failure in adhesive lap joints of arbitrary joint configuration10.1016/j.compstruct.2015.07.100 ↗
36. Elastic constants of alumina10.1007/BF03172465 ↗
37. Deformation mechanisms in nacre10.1557/JMR.2001.0340 ↗