Tensile and mixed-mode strength of a thin film-substrate interface under laser induced pulse loading
Source abstract
Abstract
Laser induced stress waves are used to characterize intrinsic interfacial strength of thin films under both tensile and mixed-mode conditions. A short-duration compressive pulse induced by pulsed-laser ablation of a sacrificial layer on one side of a substrate is allowed to impinge upon a thin test film on the opposite surface. Laser-interferometric measurements of test film displacement enable calculation of the stresses generated at the interface. The tensile stress at the onset of failure is taken to be the intrinsic tensile strength of the interface. Fused-silica substrates, with their negative nonlinear elasticity, cause the compressive stress wave generated by the pulse laser to evolve a decompression shock, critical for generation of the fast fall times needed for significant loading of surface film interfaces. By allowing the stress pulse to mode convert as it reflects from an oblique surface, a high amplitude shear wave with rapid fall time is generated and used to realize mixed-mode loading of thin film interfaces. We report intrinsic strengths of an aluminum/fused silica interface under both tensile and mixed-mode conditions. The failure mechanism under mixed-mode loading differs significantly from that observed under pure tensile loading, resulting in a higher interfacial strength for the mixed-mode case. Inferred strengths are found to be independent, as they should be, of experimental parameters.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Advanced Fiber Optic Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Mechanical properties of thin films10.1146/annurev.ms.20.080190.002135 ↗
2. Measurement and control of ice adhesion to aluminum 6061 alloy10.1016/S0022-5096(98)00014-3 ↗
3. Ion beam bonding of thin films10.1016/0168-583X(85)90488-4 ↗
4. Shock wave studies of PMMA, fused silica and sappire10.1063/1.1658439 ↗
5. Determination of the bond strength of some micron coatings using the laser shock technique10.1051/epjap:1999123 ↗
6. An experimental study of the fracture resistance of bimaterial interfaces10.1016/0167-6636(89)90020-3 ↗
7. A test specimen for determining the fracture resistance of bimaterial interfaces10.1115/1.3176069 ↗
8. Chu, Y.Z., Jeong, H.S., White, R.C., Durning, C.J., 1992. Characterization of adhesion in thin-film materials by the blister test. MRS Symposium Proceedings, Vol. 276, pp. 209–220.10.1557/PROC-276-209 ↗
9. Fracture resistance of metal/ceramic/intermetallic interfaces10.1016/0956-716X(91)90492-J ↗
10. The thermomechanical integrity of thin films and multilayers10.1016/0956-7151(94)00444-M ↗
11. Blow-off pressures for adhering layers10.1002/app.1987.070330512 ↗
12. Graff · 1991
13. Characterizing adhesion of thermal barrier coatings
14. Measurement of interface strength by the modified laser-spallation technique10.1063/1.354699 ↗
15. Measurement of interface strength by laser pulse-induced spallation10.1016/0921-5093(90)90116-K ↗
16. Measurement of interface strength by a laser spallation technique10.1016/0022-5096(92)90296-E ↗
17. Recent developments in the laser spallation technique to measure the interface strength and its relationship to interface toughness with applications to metal/ceramic, ceramic/ceramic and ceramic/polymer interfaces10.1163/156856194X00447 ↗
18. Interfacial adhesion and its degradation in selected metal/oxide and dielectric/oxide in multi-layer devices10.1016/S0042-207X(00)00282-7 ↗
19. Some factors influencing the adhesion of films produced by vacuum evaporation10.1051/jphysrad:01950001107035500 ↗
20. Measurement of thin film adhesion10.1016/0042-207X(87)90018-2 ↗
21. Mixed-mode cracking in layered materials10.1016/S0065-2156(08)70164-9 ↗
22. Measurement of adhesion of thin evaporated films glass substrates by means of the direct pull method10.1016/0040-6090(73)90205-8 ↗
23. Elasto-plastic analysis of the peel test for thin film adhesion10.1115/1.3226047 ↗
24. Quantitative adhesion measures of multilayer films10.1557/JMR.1999.0404 ↗
25. Quantitative adhesion measures of multilayer films10.1557/JMR.1999.0405 ↗
26. The development of the scratch technique for the determination of the adhesion of coatings10.1016/0040-6090(81)90700-8 ↗
27. Biaxial loading experiments for determining interfacial fracture toughness10.1115/1.2897248 ↗
28. Mattox, D.M., 1978. Adhesion measurement of thin films, thick films and bulk coatings, Am. Soc. Test. Mater. Spec. Tech. ASTM, Philadelphia.
29. Miklowitz · 1978
30. Mittal, K.L., 1978. Adhesion measurement: recent progress, unsolved problems, and prospects. Adhesion Measurement of Thin Films, Thick Films, and Bulk Coatings, ASTM STP 640, American Society for Testing and Materials, Philadelphia, pp. 5–17.10.1520/STP38620S ↗
31. Selected bibliography on adhesion measurement of films and coatings10.1163/156856187X00265 ↗
32. Delamination cracking in a laminated ceramic matrix composite
33. On the cleaning of surfaces10.1063/1.1751951 ↗
34. Fracture mechanics of a model interface under mixed-mode loading10.1016/0956-7151(90)90186-K ↗
35. Fracture mechanics for thin film adhesion10.1147/rd.384.0367 ↗
36. Experimental study of the mechanisms of crack extension along an oxide/metal interface acta materialia
37. Vossen, J.L., 1978. Measurements of film–substrate bond strength by laser spallation. Adhesion Measurement of Thin Films, Thick Films and Bulk Coatings ASTM STP 640, American Society for Testing and Materials, Philadelphia, pp. 122–123.10.1520/STP38629S ↗
38. Wang, J., 2002. Thin film adhesion measurement by laser induced stress waves. Ph.D. Thesis, University of Illinois.
39. Experimental determination of interfacial toughness using brazil-nut-sandwich10.1016/0956-7151(90)90200-Z ↗
40. A parametric study of laser induced thin film spallation10.1007/BF02411054 ↗
41. Mixed-mode failure of thin films using laser generated shear waves10.1007/BF02410531 ↗
42. Laser induced decompression shock development in fused silica10.1063/1.1574175 ↗
43. Adhesion of thin films10.1116/1.568754 ↗
44. Stress waves generated in thin metallic films by a Q-switched ruby laser10.1063/1.1663636 ↗
45. Measurement of in situ fiber/matrix interfacial strength in graphite/epoxy composites10.1016/S0266-3538(98)00048-7 ↗
46. Measurement of interface strength by the modified laser-spallation technique10.1063/1.354698 ↗
47. Measurement of interface strength by the modified laser-spallation technique10.1063/1.354700 ↗