Abstract

Abstract Nanostructured metallic multilayers with carefully designed mechanical and functional properties are omnipresent in cutting edge technological applications. To ensure the mechanical integrity of such coatings, the Mode I critical Stress Intensity Factor KIC is used to quantify their fracture toughness in order to avoid material failure by appropriate design. In this article, we present a novel approach for the KIC determination of thin and ultrathin films on compliant substrate, based on micro-displacement field analysis using Digital Image Correlation within SEM. Using this method, KIC of a Cu/W nano-multilayer with a total coating thickness of 240 nm was determined as K IC = 4.8 ± 0.05 MPa m , showing excellent agreement with the values published for comparable systems in the literature. To verify the validity of the chosen approach, two independent finite element simulations were employed, thus revealing the role and effect of the compliant substrate on the stress and displacement fields arising around the crack tip in thin films.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Electronic Packaging and Soldering Technologies · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Review article: stress in thin films and coatings: current status, challenges, and prospects
2. Toughness evaluation of hard coatings and thin films10.1016/j.tsf.2011.09.036 ↗
3. E. Hintsala, & D. Kiener, & J. Jackson, W.W. Gerberich, In-Situ Measurements of Free-Standing, Ultra-Thin Film Cracking in Bending, (n.d.). doi:10.1007/s11340-015-0069-2.10.1007/s11340-015-0069-2 ↗
4. New method of determining strength and fracture toughness of thin hard coatings10.1016/S0040-6090(00)01312-2 ↗
5. Fracture toughness measurement of thin films on compliant substrate using controlled buckling test10.1016/j.tsf.2006.01.044 ↗
6. The fracture of brittle thin films on compliant substrates in flexible displays10.1016/S0013-7944(01)00104-7 ↗
7. Fracture mechanics based analysis of the scratch resistance of thin brittle coatings on a soft interlayer10.1016/j.wear.2015.01.081 ↗
8. Supertough wear-resistant coatings with “chameleon” surface adaptation10.1016/S0040-6090(00)00917-2 ↗
9. Measuring notch toughness of thin film metallic glasses using focused ion beam-based microcantilever method: comparison with Ti and TiN crystalline films10.1016/j.msea.2017.05.002 ↗
10. Microcantilever bending experiments in NiAl - Evaluation, size effects, and crack tip plasticity10.1557/jmr.2014.240 ↗
11. Understanding the extremely low fracture toughness of freestanding gold thin films by in-situ bulge testing in an AFM10.1016/j.msea.2017.03.037 ↗
12. A new technique to measure through film thickness fracture toughness10.1016/S0040-6090(01)01613-3 ↗
13. Relationship between the mechanical properties and the microstructure of nanocomposite TiN/SiN1.3 coatings prepared by low temperature plasma enhanced chemical vapor deposition10.1016/S0040-6090(03)00028-2 ↗
14. The effect of eigenstrain induced by ion beam damage on the apparent strain relief in FIB-DIC residual stress evaluation10.1016/j.matdes.2015.12.015 ↗
15. Nanoscale structural damage due to focused ion beam milling of silicon with Ga ions
16. High failure resistance layered ceramics using crack bifurcation and interface delamination as reinforcement mechanisms10.1016/j.engfracmech.2010.02.020 ↗
17. Radiation tolerance of Cu/W multilayered nanocomposites10.1016/j.jnucmat.2011.03.030 ↗
18. Probing the deformation and fracture properties of Cu/W nano-multilayers by in situ SEM and synchrotron XRD strain microscopy10.1016/j.surfcoat.2017.01.065 ↗
19. A better way to construct the sunflower head10.1016/0025-5564(79)90080-4 ↗
20. C. Eberl, Digital image correlation and tracking, MATLAB cent. File exch. (2020). https://www.mathworks.com/matlabcentral/fileexchange/12413-digital-image-correlation-and-tracking (accessed July 22, 2020).
21. Anderson · 2017
22. Nano-scale residual stress depth profiling in Cu/W nano-multilayers as a function of magnetron sputtering pressure10.1016/j.surfcoat.2019.125142 ↗
23. DuPont, DuPont Kapton HN, (2019) 2. https://www.dupont.com/content/dam/dupont/amer/us/en/products/ei-transformation/documents/DEC-Kapton-HN-datasheet.pdf (accessed July 27, 2020).
24. Size effect on fracture toughness of freestanding copper nano-films10.1016/j.msea.2011.07.071 ↗
25. Tensile and fracture behavior of free-standing copper films10.1016/0921-5093(96)10253-7 ↗
26. Size-dependent fracture toughness of tungsten10.1016/j.actamat.2017.07.030 ↗
27. A maximum in ductility and fracture toughness in nanostructured Cu/Cr multilayer films10.1016/j.scriptamat.2009.10.030 ↗
28. Evaluation of the interfacial shear strength and residual stress of TiAlN coating on ZIRLO™ fuel cladding using a modified shear-lag model approach10.1016/j.jnucmat.2015.06.003 ↗
29. Vergani · 2006