Effect of Spray Particle Velocity on Cavitation Erosion Resistance Characteristics of HVOF and HVAF Processed 86WC-10Co4Cr Hydro Turbine Coatings
Source abstract
Abstract
The hydro plants utilizing silt-laden water for power generation suffer from severe metal wastage due to particle-induced erosion and cavitation. High-velocity oxy-fuel process (HVOF)-based coatings is widely applied to improve the erosion life. The process parameters such as particle velocity, size, powder feed rate, temperature, affect their mechanical properties. The high-velocity air fuel (HVAF) technology, with higher particle velocities and lower spray temperatures, gives dense and substantially nonoxidized coating. In the present study, the cavitation resistance of 86WC-10Co4Cr-type HVOF coating processed at 680 m/s spray particle velocity was compared with HVAF coatings made at 895, 960, and 1010 m/s. The properties such as porosity, hardness, indentation toughness, and cavitation resistance were investigated. The surface damage morphology has been analyzed in SEM. The cohesion between different layers has been examined qualitatively through scratch depth measurements across the cross section. The HVAF coatings have shown a lower porosity, higher hardness, and superior cavitation resistance. Delamination, extensive cracking of the matrix interface, and detachment of the WC grains were observed in HVOF coating. The rate of metal loss is low in HVAF coatings implying that process parameters play a vital role in achieving improved cavitation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. J.F. Santa, L.A. Espitia, J.A. Blanco, S.A. Romo, and A. Toro, Slurry and Cavitation Erosion Resistance of Thermal Spray Coatings, Wear, 2009, 267, p 160-16710.1016/j.wear.2009.01.018 ↗
2. M.K. Padhy and R.P. Saini, A Review on Silt Erosion in Hydro Turbines, Renew. Sustain. Energy Rev., 2008, 12, p 1974-198710.1016/j.rser.2007.01.025 ↗
3. R.P. Singh, Silt Damage Control Measures for Underwater Parts: Nathpa Jhakri Hydro Power Station: Case Study of a Success Story, Water Energy Int., 2009, 66, p 36-42
4. R. Singh, S.K. Tiwari, and S.K. Mishra, Cavitation Erosion in Hydraulic Turbine Components and Mitigation by Coatings: Current Status and Future Needs, J. Mater. Eng. Perform., 2012, 21, p 1539-155110.1007/s11665-011-0051-9 ↗
5. B. Thapa, P. Chaudhary, O.G. Dahlhaug, and P. Upadhyay, Study of Combined Effect of Sand Erosion and Cavitation in Hydraulic Turbines, Int. Conf. Small Hydropower, 2007, 22, p 24
6. K. Zhao, C. Gu, F. Shen, and B. Lou, Study on Mechanism of Combined Action of Abrasion and Cavitation Erosion on Some Engineering Steels, Wear, 1993, 162–164, p 811-81910.1016/0043-1648(93)90082-W ↗
7. P.P. Gohil and R.P. Saini, Coalesced Effect of Cavitation and Silt Erosion in Hydro Turbines: A review, Renew. Sustain. Energy Rev., 2014, 33, p 280-28910.1016/j.rser.2014.01.075 ↗
8. L.M. Berger, S. Saaro, T. Naumann, M. Wiener, V. Weihnacht, S. Thiele, and J. Suchanek, Microstructure and Properties of HVOF-Sprayed Chromium Alloyed WC-Co and WC-Ni Coatings, Surf. Coatings Technol., 2008, 2008(202), p 4417-442110.1016/j.surfcoat.2008.04.019 ↗
9. S.J. Matthews, B.J. James, and M.M. Hyland, Microstructural Influence on Erosion Behavior of Thermal Spray Coatings, Mater. Charact., 2007, 58, p 59-6410.1016/j.matchar.2006.03.014 ↗
10. M. Factor and I. Roman, Use of Microhardness as a Simple Means of Estimating Relative Wear Resistance of Carbide Thermal Spray Coatings: Part 2 Wear Resistance of Cemented Carbide Coatings, J. Therm. Spray Technol., 2002, 11(4), p 482-49510.1361/105996302770348619 ↗
11. H. Li, K.A. Khor, and P. Cheang, Young’s Modulus and Fracture Toughness Determination of High Velocity Oxy-Fuel-Sprayed Bioceramic Coatings, Surf. Coat. Technol., 2002, 155, p 21-3210.1016/S0257-8972(02)00026-9 ↗
12. L.-M. Berger, P. Ettmayer, P. Vuoristo, T. Mäntylä, and W. Kunert, Microstructure and Properties of WC-10% Co-4% Cr Spray Powders and Coatings: Part 1. Powder Characterization, J. Therm. Spray Technol., 2001, 10(2), p 311-32510.1361/105996301770349402 ↗
13. S. Wirojanupatump, P.H. Shipway, and D.G. McCartney, The Influence of HVOF Powder Feedstock Characteristics on the Abrasive Wear Behavior of CrxCy: NiCr Coatings, Wear, 2001, 249, p 829-83710.1016/S0043-1648(01)00821-3 ↗
14. H.L.D.V. Lovelock, Powder/Processing/Structure Relationships in WC-Co Thermal Spray Coatings: A Review of the Published Literature, J. Therm. Spray Technol., 1998, 7(3), p 357-37310.1361/105996398770350846 ↗
15. H.H. Tawfik and F. Zimmerman, Mathematical Modeling of the Gas and Powder Flow in HVOF Systems, J. Therm. Spray Technol., 1997, 6(3), p 345-35210.1007/s11666-997-0069-6 ↗
16. S.L. Liu, X.P. Zheng, and G.Q. Geng, Influence of Nano-WC-12Co Powder Addition in WC-10Co-4Cr AC-HVAF Sprayed Coatings on Wear and Erosion Behaviour, Wear, 2010, 269, p 362-36710.1016/j.wear.2010.04.019 ↗
17. G. Bolelli, L.-M. Berger, T. Börner, H. Koivuluoto, L. Lusvarghi, C. Lyphout et al., Tribology of HVOF- and HVAF-Sprayed WC–10Co4Cr Hard Metal Coatings: A Comparative Assessment, Surf. Coatings Technol., 2015, 265, p 125-14410.1016/j.surfcoat.2015.01.048 ↗
18. C. Deng, M. Liu, C. Wu, K. Zhou, and J. Song, Impingement Resistance of HVAF WC-Based Coatings, J. Therm. Spray Technol., 2007, 16(5–6), p 604-60910.1007/s11666-007-9111-y ↗
19. Q. Wang, S. Zhang, Y. Cheng, J. Xiang, X. Zhao, and G. Yang, Wear and Corrosion Performance of WC-10Co4Cr Coatings Deposited by Different HVOF and HVAF Spraying Processes, Surf. Coat. Technol., 2013, 218, p 127-13610.1016/j.surfcoat.2012.12.041 ↗
20. G. Bolelli, T. Börner, A. Milanti, L. Lusvarghi, J. Laurila, and H. Koivuluoto, Kari Niemi and Petri Vuoristo, Tribological behavior of HVOF- and HVAF-Sprayed Composite Coatings Based on Fe-Alloy+WC–12% Co, Surf. Coat. Technol., 2014, 248, p 104-11210.1016/j.surfcoat.2014.03.037 ↗
21. L. Jacobs, M.M. Hyland, and M. De Bonte, Comparative Study of WC-Cermet Coatings Sprayed via the HVOF and the HVAF Process, J. Therm. Spray Technol., 1998, 7(2), p 213-21810.1361/105996398770350954 ↗
22. T.C. Hanson and G.S. Settles, Particle Temperature and Velocity Effects on the Porosity and Oxidation of an HVOF Corrosion-Control Coating, J. Therm. Spray Technol., 2003, 12(3), p 403-41510.1361/105996303770348276 ↗
23. M. Watanabe, A. Owada, S. Kuroda, and Y. Gotoh, Effect of WC Size on the Interface Fracture Toughness of WC-Co HVOF Sprayed Coatings, Surf. Coat. Technol., 2006, 201, p 619-62710.1016/j.surfcoat.2005.12.019 ↗
24. P. Suresh Babu, B. Basu, and G. Sundararajan, Processing-Structure-Property Correlation and Decarburization Phenomenon in Detonation Sprayed WC-12Co Coatings, Acta Mater., 2008, 56, p 5012-502610.1016/j.actamat.2008.06.023 ↗
25. T. Varis, T. Suhonen, A. Ghabchi, A. Valarezo, S. Sampath, X. Liu, and S.P. Hannula, Formation Mechanisms, Structure, and Properties of HVOF-Sprayed WC-CoCr Coatings: An Approach Toward Process Maps, J. Therm. Spray Technol., 2014, 23(6), p 1009-101810.1007/s11666-014-0110-5 ↗
26. K. Niihara, A Fracture Mechanics Analysis of Indentation-Induced Palmqvist Cracks in Ceramics, J. Mater. Sci. Lett., 1983, 2, p 221-22310.1007/BF00725625 ↗
27. P.S. Prevey, Current Applications of X-ray Diffraction Residual Stress Measurement, Dev. Mater. Charact. Technol. G. Vander Voort and J. Friel (Eds.), 1996, p 103–110
28. J. Steller, International Cavitation Erosion Test and Quantitative Assessment of Material Resistance to Cavitation, Wear, 1999, 233–235, p 51-6410.1016/S0043-1648(99)00195-7 ↗
29. R.K. Kumar, S. Seetharamu, and M. Kamaraj, Quantitative Evaluation of 3D Surface Roughness Parameters During Cavitation Exposure of 16Cr – 5Ni Hydro Turbine Steel, Wear, 2014, 320, p 16-2410.1016/j.wear.2014.07.015 ↗
30. D.A. Stewart, P.H. Shipway, and D.G. McCartney, Microstructural Evolution in Thermally Sprayed WC-Co Coatings: Comparison Between Nanocomposite and Conventional Starting Powders, Acta Mater., 2000, 48, p 1593-160410.1016/S1359-6454(99)00440-1 ↗
31. M.M. Lima, C. Godoy, J.C. Avelar-Batista, and P.J. Modenesi, Toughness Evaluation of HVOF WC-Co Coatings Using Non-linear Regression An alysis, Mater. Sci. Eng. A., 2003, 357, p 337-34510.1016/S0921-5093(03)00204-1 ↗
32. Y.Y. Santana, P.O. Renault, M. Sebastiani, J.G. LA Barbera, J. Lesage, E. Bemporad et al., Characterization and Residual Stresses of WC-Co Thermally Sprayed Coatings, Surf. Coat. Technol., 2008, 202, p 4560-456510.1016/j.surfcoat.2008.04.042 ↗
33. P. Bansal, P.H. Shipway, S.B. Leen, and L.C. Driver, Experimental Validation of FE Predicted Fracture Behavior in Thermally Sprayed Coatings, Mater. Sci. Eng. A., 2006, 430, p 104-11210.1016/j.msea.2006.05.139 ↗
34. P. Bansal, P.H. Shipway, and S.B. Leen, Effect of Particle Impact on Residual Stress Development in HVOF Sprayed Coatings, J. Therm. Spray Technol., 2006, 15(4), p 570-57510.1361/105996306X146703 ↗
35. R.K. Kumar, M. Kamaraj and S. Seetharamu, Cavitation Erosion Resistance Characteristics of HVOF and HVAF Processed 86WC-10Co4Cr Hydro Turbine Coatings, Proc. 6th Asian Therm. Spray Conf. (ATSC-2014), 2014, p 2–3
36. J. Nohava, B. Bonferroni, G. Bolelli, and L. Lusvarghi, Interesting Aspects of Indentation and Scratch Methods for Characterization of Thermally-Sprayed Coatings, Surf. Coat. Technol., 2010, 205, p 1127-113110.1016/j.surfcoat.2010.08.086 ↗