Abstract

Poor corrosion resistance is a significant limitation of magnesium alloys as structural materials. To address this problem, the objective of this study was to apply to a magnesium alloy a corrosion-resistant barrier coating that has galvanic compatibility with magnesium and a hardness value no less than that of magnesium. Aluminum coatings were applied to ZE41A-T5 Mg by the cold spray process. A custom-made high-purity Al-5 wt.% Mg powder was produced by spray metal forming for the coating evaluation. In addition, coatings of commercially pure Al (99.5 wt.%), high-purity Al (99.95 wt.%), AA5356, and AA4047 were used for comparison. Coating evaluation included mechanical testing (hardness and adhesion strength) and corrosion testing (salt spray, galvanic coupling, and crevice corrosion). The Al-5% Mg powder resulted in the best overall performance, including a high hardness, 125 Hv100, and an adhesion strength, over 60 MPa, when treated for over 1000 h in a salt spray chamber and with a low galvanic current.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. B.A. Shaw and R.C. Wolfe, Corrosion Resistance of Magnesium Alloys, ASM Handbook, Vol 13B, Corrosion: Materials, ASM International, Materials Park, OH, 2005, p 205-22710.31399/asm.hb.v13b.a0003820 ↗
2. I.J. Polmear, Introduction to Magnesium in ASM Specialty Handbook: Magnesium and Magnesium Alloys, ASM International, Materials Park, OH, 1999, p 3-15
3. G.L. Song and A. Atrens, Corrosion Mechanisms of Magnesium Alloys, Adv. Eng. Mater., 1999, 1(1), p 11-3310.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
4. E. Ghali, Magnesium and Magnesium Alloys in Uhlig’s Corrosion Handbook, 2nd ed., John Wiley & Sons, Inc., New York, 2000, p 793
5. J.E. Gray and B. Luan, Protective Coatings on Magnesium and Its Alloys: A Critical Review, J. Alloys Compd., 2002, 336(1), p 88-11310.1016/S0925-8388(01)01899-0 ↗
6. J.D. Hanawalt, C.E. Nelson, and J.A. Peloubet, Corrosion Studies of Magnesium, Trans. AIME, 1942, 147, p 273-299
7. M.R. Bothwell, Galvanic Relationships between Aluminum Alloys and Magnesium Alloys II. Aluminum Claddings on Magnesium, J. Electrochem. Soc., 1959, 106, p 1019-102110.1149/1.2427201 ↗
8. R.C. Dykhuizen and M.F. Smith, Gas Dynamic Principles of Cold Spray, J. Therm. Spray Technol., 1998, 7(2), p 205-21210.1361/105996398770350945 ↗
9. A.O. Tokarev, Structure of Aluminium Powder Coating Produced by Cold Gas Dynamic Deposition, Metallovedenie i Termicheskaya Obrabotka Metallov, 1996, 3, p 36-39
10. M.F. Amateau and T. Eden, High Velocity Particle Consolidation Technology, iMast Q., 2000, 2, p 306
11. V.K. Champagne, Jr., D. Helfritch, P. Leyman, S. Grendahl, and B. Klotz, Interface Material Mixing Formed by the Deposition of Copper on Aluminum by Means of the Cold Spray Process, J. Therm. Spray Technol., 2005, 14(3), p 330-33410.1361/105996305X59332 ↗
12. D.L. Gilmore, R.C. Dykhuizen, R.A. Neiser, T.J. Roemer, and M.F. Smith, Particle Velocity and Deposition Efficiency in the Cold Spray Process, J. Therm. Spray Technol., 1999, 8(4), p 576-58210.1361/105996399770350278 ↗
13. M. Grujicic, C. Tong, W.S. DeRosset, and D. Helfritch, Flow Analysis and Nozzle-Shape Optimization for the Cold-Gas Dynamic-Spray Process, Proc. IME B J. Eng. Manufact., 2003, 217(11), p 1603-161310.1243/095440503771909980 ↗
14. W.-Y. Li and C.-J. Li, Optimization of Spray Conditions in Cold Spraying Based on Numerical Analysis of Particle Velocity, Trans. Nonferrous Met. Soc. China (English Ed.), 2004, 14(Suppl. 2), p 43-48
15. T. Eden, High Strength Aluminum Alloys Produced By Spray Metal Forming, iMAST Q., 2005, 2, p 4