Abstract

The cavitation and erosion resistance of 21 thermal spray coatings and four weld repair materials were investigated in the laboratory using cavitation jet and slurry erosion testing. Of the thermal spray coatings, Stellite® 6 deposited by the high velocity oxyfuel (HVOF) process had the lowest cavitation rate (11.7 mg/h). This was higher than the corresponding cavitation rate (3.2 mg/h) of 308 stainless steel weld metal currently used as a reference. In the slurry erosion testing, the volume loss of Stellite® 6 applied by the HVOF process was 5.33 cubic mm/h, much lower than the corresponding loss (11.17 cubic mm/h) in the currently used stainless steel 304 reference. Furthermore, the electrochemical potential difference between the carbon steel and HVOF sprayed Stellite 6 coating was 0.25 volts, half the potential difference between the 304 stainless steel carbon steel substrate, and will result in reduced galvanic corrosion of the substrate near the contact areas. Stellite 6 deposited by the HVOF process was recommended for repair of damage resulting from erosion and subsequent cavitation by caused by surface roughening.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Coal Combustion and Slurry Processing · Ultrasound and Cavitation Phenomena · Cavitation Phenomena in Pumps

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.