journal article·2011-12

Wear Behavior of Plasma-Sprayed Carbon Nanotube-Reinforced Aluminum Oxide Coating in Marine and High-Temperature Environments

Anup Kumar Keshri, Arvind Agarwal

Publisher page

Abstract

Wear behavior of plasma-sprayed carbon nanotube (CNT)-reinforced aluminum oxide (Al2O3) composite coatings are investigated at room temperature (298 K), elevated temperature (873 K), and in sea water. Lowest wear volume loss was observed in the sea water as compared to dry sliding at 298 and 873 K. Relative improvement in the wear resistance of Al2O3-8 wt.% CNT coating compared to Al2O3 was 72% at 298 K, 76% at 873 K, and 66% in sea water. The improvement in the wear resistance of Al2O3-CNT coatings is attributed to (i) larger area coverage by protective film on the wear surface at room temperature and in sea water, (ii) higher fracture toughness of Al2O3-CNT coatings due to CNT bridging between splats, and (iii) anti-friction effect of sea water. The average coefficient of friction (COF) was the lowest (0.55) in sea water and the highest (0.83) at 873 K for Al2O3-8 wt.% CNT coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Tribology and Wear Analysis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. K. Balani and A. Agarwal, Process Map for Plasma Sprayed Aluminum Oxide-Carbon Nanotube Nanocomposite Coatings, Surf. Coat. Technol., 2008, 202, p 4270-427710.1016/j.surfcoat.2008.03.024 ↗
2. E.H. Jordan and M. Gell, Nano Crystalline Ceramic and Ceramic Coatings Made by Conventional and Solution Plasma Spray, Nanomaterials Technology for Military Vehicle Structural Applications, RTO-MP-AVT-122, 3-4 October, 2005
3. G.R. Karagedov and N.Z. Lyakhov, Preparation and Sintering of Nanosized Alpha-Al2O3 Powder, Nanostruct. Mater., 1999, 11, p 559-57210.1016/S0965-9773(99)00331-1 ↗
4. H. Luo, D. Goberman, L. Shaw, and M. Gell, Indentation Fracture Behavior of Plasma-Sprayed Nanostructured Al2O3-13 wt.% TiO2 Coatings, Mater. Sci. Eng. A, 2003, 346, p 237-24510.1016/S0921-5093(02)00523-3 ↗
5. L.L. Shaw, D. Goberman, R. Ren, M. Gell, S. Jiang, Y. Wang, D.T. Xiao, and P.R. Strutt, The Dependency of Microstructure and Properties of Nanostructured Coatings on Plasma Spray Conditions, Surf. Coat. Technol., 2000, 180, p 1-810.1016/S0257-8972(00)00673-3 ↗
6. Y. Wang, S. Jiang, M. Wang, S. Wang, T.D. Xiao, and P.R. Strutt, Abrasive Wear Characteristics of Plasma Sprayed Nanostructured Alumina/Titania Coatings, Wear, 2000, 237, p 176-18510.1016/S0043-1648(99)00323-3 ↗
7. H.Y. Ding, Z.D. Dai, S.C. Skuiry, and D. Hui, Corrosion Wear Behaviors of Micro-Arc Oxidation Coating of Al2O3 on 2024Al in Different Aqueous Environments at Fretting Contact, Tribol. Int., 2010, 43, p 868-87510.1016/j.triboint.2009.12.022 ↗
8. A.K. Keshri, J. Huang, W. Choi, and A. Agarwal, Intermediate Temperature Tribological Behavior of Carbon Nanotube Reinforced Plasma Sprayed Aluminum Oxide Coating, Surf. Coat. Technol., 2010, 204, p 1847-185510.1016/j.surfcoat.2009.11.032 ↗
9. X. Lin, Y. Zenga, C. Ding, and P. Zhang, Effects of Temperature on Tribological Properties of Nanostructured and Conventional Al2O3-3 wt.% TiO2 Coatings, Wear, 2004, 256, p 1018-102510.1016/S0043-1648(03)00541-6 ↗
10. D. Yan, J. He, X. Li, Y. Liu, J. Zhang, and H. Ding, An Investigation of the Corrosion Behavior of Al2O3-Based Ceramic Composite Coatings in Dilute HCl Solution, Surf. Coat. Technol., 2001, 141, p 1-610.1016/S0257-8972(01)01170-7 ↗
11. I. Ahmad, A. Kennedy, and Y.Q. Zhu, Wear Resistant Properties of Multi Walled Carbon Nanotubes Reinforced Al2O3 Nanocomposites, Wear, 2010, 269, p 71-7810.1016/j.wear.2010.03.009 ↗
12. J.W. An, D.H. You, and D.S. Lim, Tribological Properties of Hot-Pressed Alumina-CNT Composites, Wear, 2003, 255, p 677-68110.1016/S0043-1648(03)00216-3 ↗
13. K. Balani, S.P. Harimkar, A.K. Keshri, Y. Chen, N.B. Dahotre, and A. Agarwal, Multiscale Wear of Plasma-Sprayed Carbon-Nanotube-Reinforced Aluminum Oxide Nanocomposite Coating, Acta Mater., 2008, 56, p 5984-599410.1016/j.actamat.2008.08.020 ↗
14. D.S. Lim, J.W. An, and H.J. Lee, Effect of Carbon Nanotube Addition on the Tribological Behavior of Carbon/Carbon Composites, Wear, 2002, 252, p 512-51710.1016/S0043-1648(02)00012-1 ↗
15. D.S. Lim, D.H. You, H.J. Choi, S.H. Lim, and H. Jang, Effect of CNT Distribution on Tribological Behavior of Alumina-CNT Composites, Wear, 2005, 259, p 539-54410.1016/j.wear.2005.02.031 ↗
16. A.K. Keshri, R. Patel, and A. Agarwal, Comprehensive Process Maps to Synthesize High Density Plasma Sprayed Aluminum Oxide Composite Coatings with Varying Carbon Nanotube Content, Surf. Coat. Technol., 2010, 205, p 690-70210.1016/j.surfcoat.2010.07.007 ↗
17. G.R. Anstis, P. Chantikul, B.R. Lawn, and D.B. Marshall, A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: Direct Crack Measurements, J. Am. Ceram. Soc., 1981, 64, p 533-53810.1111/j.1151-2916.1981.tb10320.x ↗
18. J. Wang, F. Yana, and Q. Xue, Tribological Behavior of PTFE Sliding Against Steel in Sea Water, Wear, 2009, 267, p 1634-164110.1016/j.wear.2009.06.015 ↗
19. X. Wang, N.P. Padture, and H. Tanaka, Contact-Damage-Resistant Ceramic/Single-Wall Carbon Nanotubes and Ceramic/Graphite Composites, Nat. Mater., 2004, 3, p 539-54410.1038/nmat1161 ↗
20. G.D. Zhan, J.D. Kuntz, J. Wan, and A.K. Mukherjee, Single Walled Carbon Nanotube as Attractive Toughening Agents in Alumina Based Nanocomposites, Nat. Mater., 2003, 2, p 38-4210.1038/nmat793 ↗
21. G.D. Quinn and R.C. Bradt, On the Vickers Indentation Fracture Toughness Test, J. Am. Ceram. Soc., 2007, 90, p 673-68010.1111/j.1551-2916.2006.01482.x ↗
22. S.S. Kim, Y.H. Chae, and D.J. Kim, Tribological Characteristics of Silicon Nitride at Elevated Temperatures, Tribol. Lett., 2000, 9, p 227-23210.1023/A:1018873208419 ↗
23. J. Li and D. Xiong, Tribological Behavior of Graphite-Containing Nickel-Based Composite as Function of Temperature, Load and Counterface, Wear, 2009, 266, p 360-36710.1016/j.wear.2008.06.020 ↗
24. S. Wilson and A.T. Alpas, Dry Sliding Wear of a PVD TiN Coating Against Si3N4 at Elevated Temperatures, Surf. Coat. Technol., 1996, 86-87, p 75-8110.1016/S0257-8972(96)02963-5 ↗
25. FACTSAGE, Thermodynamic Equilibrium Software, Version 5.0, Center for Research in Computational Thermochemistry of the Ecole Polythechnique at the Université de Montréal and GTT-Technologies, GmbH, Aachen, Germany, 2001
26. Y.S. Feng, S.M. Zhou, Y. Li, and L.D. Zhang, Preparation of the SnO2/SiO2 Xerogel with a Large Specific Surface Area, Mater. Lett., 2003, 57, p 2409-241210.1016/S0167-577X(02)01245-4 ↗
27. N. Koshizaki, H. Umehara, and T. Oyama, XPS Characterization and Optical Properties of Si/SiO2, Si/Al2O3 and Si/MgO Co-Sputtered Films, Thin Solid Films, 1998, 325, p 130-13610.1016/S0040-6090(98)00512-4 ↗
28. S. Osswald, M. Havel, and Y. Gogotsi, Monitoring Oxidation of Multiwalled Carbon Nanotubes by Raman Spectroscopy, J. Raman Spectrosc., 2007, 38, p 728-73610.1002/jrs.1686 ↗
29. C. Li, D. Wang, T. Liang, X. Wang, J. Wu, X. Hu, and J. Liang, Oxidation of Multiwalled Carbon Nanotubes by Air: Benefits for Electric Double Layer Capacitors, Powder Technol., 2004, 142, p 175-17910.1016/j.powtec.2004.04.037 ↗
30. A.G. Evans and B. Marshall, Wear Mechanism in Ceramics, Fundamentals of Friction and Wear of Materials, D.A. Rigney, Ed., ASM International, Metals Park, OH, 1981, p 439-452