Abstract
The composition WC-(W,Cr)2C-Ni is one of the standard compositions used for the preparation of thermally sprayed coatings by high velocity oxy-fuel (HVOF) spraying. Surprisingly, this composition has been poorly investigated in the past. Frequent use of commercial designations WC-‘CrC’-Ni, WC-Cr3C2-Ni, and WC-NiCr indicates the insufficient knowledge about the phase compositions of these powders and coatings. The properties of these coatings differ significantly from those of WC-Co and WC-CoCr coatings. In this paper, the results of different series of experiments conducted on HVOF-sprayed WC-(W,Cr)2C-Ni coatings are compiled and their specific benefits pointed out. The focus of this study is on the analysis of the microstructures and phase compositions of the feedstock powders and coatings. Unlike WC-Co and Cr3C2-NiCr, WC-(W,Cr)2C-Ni is not a simple binary hard phase—binder metal composite. The phase (W,Cr)2C with unknown physical and mechanical properties appears as a second hard phase, which is inhomogeneously distributed in the feedstock powders and coatings. As examples of coating properties, the oxidation resistance and dry sliding wear properties are compared with those of WC-10%Co-4%Cr coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. J.F. Pelton and J.M. Koffskey Jr., Process of Flame Spraying a Tungsten Carbide-Chromium Carbide-Nickel Coating, and Article Produced Thereby, US Patent 3,071,489 (filing date: 28.05.1958, granted: 01.01.1963)
2. R. Okada, M. Yamada, Effect of Heat Treatment on Hardness and Wear Resistance of WC-NiCr Sprayed Coatings, J. Jpn. Inst. Met. 1994, 58 (7), p 763-767 (in Japanese)10.2320/jinstmet1952.58.7_763 ↗
3. Y. Ishikawa, J. Kawakita, S. Osawa, T. Itsukaichi, Y. Sakamoto, M. Takaya, S. Kuroda, Evaluation of Corrosion and Wear Resistance of Hard Cermet Coatings Sprayed by Using an Improved HVOF Process, J. Thermal Spray Techn. 2005, 14 (3), p 384-39010.1361/105996305X59378 ↗
4. Y. Ishikawa, J. Kawakita, S. Kuroda, Effect of Spray Condition and Heat Treatment on the Structure and Adhesive Wear Properties of WC Cermet Coatings, Mater. Trans. 2005, 46 (7), p 1671-167610.2320/matertrans.46.1671 ↗
5. Y. Ishikawa, S. Kuroda, J. Kawakita, Y. Sakamoto, M. Takaya, Sliding Wear Properties of HVOF Sprayed WC-20%Cr3C2-7%Ni Cermet Coatings, Surf. Coat. Tech. 2007, 201 (8), p 4718-472710.1016/j.surfcoat.2006.10.007 ↗
6. M. Yoshida, K. Tani, A. Nakahira, A. Nakajima, and T. Mawatari, Durability and Tribological Properties of Thermally Sprayed WC Cermet Coating in Rolling/Sliding Contact, Thermal Spraying: Current Status and Future Trends, Vol. 2, A. Ohmori, Ed., May 22-26, Kobe, High Temperature Society of Japan, Japan, 1995, p 663-668
7. A. Nakajima, T. Mawatari, M. Yoshida, K. Tani, A. Nakahira, Effects of Coating Thickness and Slip Ratio on Durability of Thermally Sprayed WC Cermet Coatings in Rolling/Sliding Contact, Wear 2000, 241 (2), p 166-17310.1016/S0043-1648(00)00371-9 ↗
8. D.M. Nuruzzaman, A. Nakajima, T. Mawatari, Effects of Substrate Surface Finish and Substrate Material on Durability of Thermally Sprayed WC Cermet Coatings in Rolling with Sliding Contact, Tribol. Int. 2006, 39 (7), p 678-68510.1016/j.triboint.2005.06.003 ↗
9. D. Toma, W. Brandl, G. Marginean, Wear and Corrosion Behaviour of Thermally Sprayed Cermet Coatings, Surf. Coat. Tech., 2001, 138 (2-3), p 149-15810.1016/S0257-8972(00)01141-5 ↗
10. H. Henke, D. Adam, A. Köhler, R.B. Heimann, Development and Testing of HVOF-Sprayed Tungsten Carbide Coatings Applied to Moulds for Concrete Roof Tiles, Wear 2004, 256 (1-2), p 81-8710.1016/S0043-1648(03)00348-X ↗
11. J.E. Cho, S.Y. Hwang, K.Y. Kim, Corrosion Behaviour of Thermal Sprayed WC Cermet Coatings Having Various Metallic Binders in Strong Acidic Environment, Surf. Coat. Tech. 2006, 200 (8), p 2653-266210.1016/j.surfcoat.2004.10.142 ↗
12. H. Kreye, High Velocity Flame Spraying—Process and Coating Characteristics, Proc. 2nd Plasma-Technik-Symposium, Vol. 1, S. Blum-Sandmeier, H. Eschnauer, P. Huber, and A.R. Nicoll, Eds., June 5-7, Plasma-Technik AG (Lucerne, Switzerland), 1991, p 39-47
13. P. Stecher, F. Benesovsky, H. Nowotny, Untersuchungen im System Chrom-Wolfram-Kohlenstoff (Investigations in the System Chromium-Tungsten-Carbon), Planseeber. Pulvermet., 1964, 12(2), p 89-95 (in German)
14. V.N. Eremenko, T.Y. Velikanova, and A.A. Bondar, The Cr-W-C Phase Diagram at High Temperatures, Dokl. Akad. Nauk Ukrainskoj SSR, Ser. A, Fiz.-Mat. Nauki 1986, (11), p 74-78 (in Russian)
15. L.-M. Berger, R. Zieris, and S. Saaro, Oxidation of HVOF-Sprayed Hardmetal Coatings, Proc. Int. Thermal Spray Conf. ITSC 2005, May 2-4, DVS-Verlag (Basel, Switzerland), 2005, CD, 8 p10.31399/asm.cp.itsc2005p0969 ↗
16. S. Zimmermann, H. Keller, and G. Schwier, New Carbide Based Materials for HVOF Spraying, Thermal Spray 2003: Advancing the Science and Applying the Technology, Vol. 1, B.R. Marple and C. Moreau, Eds., May 5-8, ASM International (Orlando, FL), 2003, p 227-23210.31399/asm.cp.itsc2003p0227 ↗
17. J. Beczkowiak, J. Fischer, and G. Schwier, Cermets für das Hochgeschwindigkeits-Flammspritzen (Cermets for HVOF-Spraying), Thermische Spritzkonferenz ‘93, Vol. 152, Deutscher Verlag für Schweißtechnik, DVS-Berichte, Aachen, Germany, March 3-5, 1993, p 32-36 (in German)
18. L.-M. Berger, S. Saaro, and M. Woydt, Reib-/Gleitverschleiß von thermisch gespritzten Hartmetallschichten (Sliding Wear of Thermally Sprayed Hardmetal Coatings), Jahrbuch Oberflächentechnik 2007, Vol. 63, R. Suchentrunk, Ed., Eugen G. Leuze Verlag, 2007, p 242-267 (in German)
19. L.-M. Berger, M. Woydt, S. Zimmermann, H. Keller, G. Schwier, R. Enžl, and S. Thiele, Tribological Behavior of HVOF-Sprayed Cr3C2-NiCr and TiC-Based Coatings under High-Temperature Dry Sliding Conditions, Thermal Spray 2004: Advances in Technology and Application, May 10-12, ASM International (Osaka, Japan), 2004, p 468-47710.31399/asm.cp.itsc2004p0468 ↗
20. L.-M. Berger, M. Woydt, and R. Zieris, Comparative Study of HVOF-Sprayed Hardmetal Coatings under High Temperature Dry Sliding Conditions, Proc. 16th Int. Plansee Seminar, May 30-June 3, 2005, Vol. 2 (Reutte/Tirol, Austria), G. Kneringer, P. Rödhammer, H. Wildner, Eds., Reutte, Plansee Holding AG, 2005, p 878-892
21. L.-M. Berger, S. Saaro, and M. Woydt, Influence of Oxidation on the Dry Sliding Properties of HVOF-Sprayed Hardmetal Coatings, Proc. Euro PM2006, Congress & Exhibition, October 23-25, 2006, Vol. 1 (Ghent, Belgium), Eur. Powder Metallurgy Ass., Shrewsbury, UK, 2006, p 225-232
22. L.-M. Berger, Hardmetals as Thermal Spray Coatings, Powder Met. 2007, 50(3), p 205-21410.1179/174329007X246078 ↗
23. C. Verdon, A. Karimi, J.-L. Martin, A Study of High Velocity Oxy-Fuel Thermally Sprayed Tungsten Carbide Based Coatings. Part 1: Microstructures, Mater. Sci. Eng. 1998, A246 (1-2), p 11-2410.1016/S0921-5093(97)00759-4 ↗
24. D.A. Stewart, P.H. Shipway, D.G. McCartney, Microstructural Evolution in Thermally Sprayed WC-Co Coatings: Comparison between Nanocomposite and Conventional Starting Powders, Acta Mater. 2000, 48 (7), p 1593-160410.1016/S1359-6454(99)00440-1 ↗
25. M. Oechsle, Carbide Containing Spray Powders and HVOF-Coatings, 7. HVOF-Kolloquium 2006, Gemeinschaft Thermisches Spritzen e.V., Erding, Germany, November 9-10, 2006, p 57-62
26. L.-M. Berger, P. Vuoristo, T. Mäntylä, and W. Gruner, A Study of Oxidation Behaviour of WC-Co, Cr3C2-NiCr and TiC-Based Materials in Thermal Spray Processes, Proc. 15th Int. Thermal Spray Conf. ITSC 1998, Vol. 1, C. Coddet, Ed., ASM International, Nice, France, May 25-29, 1998, p 75-8210.31399/asm.cp.itsc1998p0075 ↗
27. L.-M. Berger, M. Woydt, and S. Saaro, Comparison of Self-Mated Hardmetal Coatings under Dry Sliding Conditions up to 600°C, Wear, 2008. doi: 10.106/j.wear.2008.04.013