Hierarchical Formation of Intrasplat Cracks in Thermal Spray Ceramic Coatings
Source abstract
Abstract
Intrasplat cracks, an essential feature of thermally sprayed ceramic coatings, play important roles in determining coating properties. However, final intrasplat crack patterns are always considered to be disordered and irregular, resulting from random cracking during splat cooling, since the detailed formation process of intrasplat cracks has scarcely been considered. In the present study, the primary formation mechanism for intrasplat cracking was explored based on both experimental observations and mechanical analysis. The results show that the intrasplat crack pattern in thermally sprayed ceramic splats presents a hierarchical structure with four sides and six neighbors, indicating that intrasplat crack patterns arise from successive domain divisions due to sequential cracking during splat cooling. The driving forces for intrasplat cracking are discussed, and the experimental data quantitatively agree well with theoretical results. This will provide insight for further coating structure designs and tailoring by tuning of intrasplat cracks.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Materials Engineering and Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. A. Ohmori and C.J. Li, Quantitative Characterization of the Structure of Plasma-Sprayed Al2O3 Coating by Using Copper Electroplating, Thin Solid Films, 1991, 201(2), p 241-25210.1016/0040-6090(91)90114-D ↗
2. R. Mcpherson, A Model for the Thermal-Conductivity of Plasma-Sprayed Ceramic Coatings, Thin Solid Films, 1984, 112(1), p 89-9510.1016/0040-6090(84)90506-6 ↗
3. I.O. Golosnoy, S.A. Tsipas, and T.W. Clyne, An Analytical Model for Simulation of Heat Flow in Plasma-Sprayed Thermal Barrier Coatings, J. Therm. Spray Technol., 2005, 14(2), p 205-21410.1361/10599630523764 ↗
4. H. Xie, Y.C. Xie, G.J. Yang, C.X. Li, and C.J. Li, Modeling Thermal Conductivity of Thermally Sprayed Coatings with Intrasplat Cracks, J. Therm. Spray Technol., 2013, 22(8), p 1328-133610.1007/s11666-013-0005-x ↗
5. G.R. Li, B.W. Lv, G.J. Yang, W.X. Zhang, C.X. Li, and C.J. Li, Relationship Between Lamellar Structure and Elastic Modulus of Thermally Sprayed Thermal Barrier Coatings with Intra-splat Cracks, J. Therm. Spray Technol., 2015, 24(8), p 1355-136710.1007/s11666-015-0292-5 ↗
6. S. Kuroda and T.W. Clyne, The Quenching Stress in Thermally Sprayed Coatings, Thin Solid Films, 1991, 200(1), p 49-6610.1016/0040-6090(91)90029-W ↗
7. N. Mifune and Y. Harada, Mechanism of Vertical Microcracking in CaO·SiO2-CaO·ZrO2 Sprayed Thermal Barrier Top Coating, Mater. Trans., 2004, 45(5), p 1788-179310.2320/matertrans.45.1788 ↗
8. K. Ito, H. Kuriki, and M. Enoki, A Numerical Study on Generation Mechanism of Vertical Cracks in Top Coat of TBCs During APS Deposition, J. Therm. Spray Technol., 2015, 24(5), p 730-73810.1007/s11666-015-0232-4 ↗
9. P. Bengtsson and C. Persson, Modelled and Measured Residual Stresses in Plasma Sprayed Thermal Barrier Coatings, Surf. Coat. Technol., 1997, 92(1-2), p 78-8610.1016/S0257-8972(97)00082-0 ↗
10. C.J. Li and A. Ohmori, Relationships Between the Microstructure and Properties of Thermally Sprayed Deposits, J. Therm. Spray Technol., 2002, 11(3), p 365-37410.1361/105996302770348754 ↗
11. S. Rangarajan and A.H. King, Non-destructive Evaluation of Delamination in Ceramic Thin Films on Metal Substrates by Scanning Electron Microscopy, Thin Solid Films, 2001, 385(1-2), p 22-2810.1016/S0040-6090(00)01904-0 ↗
12. T. Chraska and A.H. King, Effect of Different Substrate Conditions Upon Interface with Plasma Sprayed Zirconia—A TEM Study, Surf. Coat. Technol., 2002, 157(2-3), p 238-24610.1016/S0257-8972(02)00181-0 ↗
13. B. Liang and C.X. Ding, Thermal Shock Resistances of Nanostructured and Conventional Zirconia Coatings Deposited by Atmospheric Plasma Spraying, Surf. Coat. Technol., 2005, 197(2-3), p 185-19210.1016/j.surfcoat.2004.08.225 ↗
14. D.Y. Chen, M. Gell, E.H. Jordan, E. Cao, and X.Q. Ma, Thermal Stability of Air Plasma Spray and Solution Precursor Plasma Spray Thermal Barrier Coatings, J. Am. Ceram. Soc., 2007, 90(10), p 3160-316610.1111/j.1551-2916.2007.01864.x ↗
15. Y.Z. Xing, Y. Li, C.J. Li, C.X. Li, and G.J. Yang, Influence of Substrate Temperature on Microcracks Formation in Plasma-Sprayed Yttria-Stabilized Zirconia Splats, Key Eng. Mater., 2008, 373-374, p 69-7210.4028/www.scientific.net/KEM.373-374.69 ↗
16. C.J. Li, G.J. Yang, and C.X. Li, Development of Particle Interface Bonding in Thermal Spray Coatings: A Review, J. Therm. Spray Technol., 2013, 22(2-3), p 192-20610.1007/s11666-012-9864-9 ↗
17. J. Matejicek, S. Sampath, P.C. Brand, and H.J. Prask, Quenching, Thermal and Residual Stress in Plasma Sprayed Deposits: NiCrAlY and YSZ Coatings, Acta Mater., 1999, 47(2), p 607-61710.1016/S1359-6454(98)00360-7 ↗
18. J. Matejicek and S. Sampath, In Situ Measurement of Residual Stresses and Elastic Moduli in Thermal Sprayed Coatings—Part 1: Apparatus and Analysis, Acta Mater., 2003, 51(3), p 863-87210.1016/S1359-6454(02)00478-0 ↗
19. C.M. Weyant, K.T. Faber, J.D. Almer, and J.V. Guiheen, Residual Stress and Microstructural Evolution in Tantalum Oxide Coatings on Silicon Nitride, J. Am. Ceram. Soc., 2005, 88(8), p 2169-217610.1111/j.1551-2916.2005.00396.x ↗
20. J. Go, Y.G. Jung, S. Kim, and U. Paik, Analysis of Thermoelastic Characteristics for Vertical-Cracked Thermal Barrier Coatings Through Mathematical Approaches, Surf. Coat. Technol., 2011, 206(7), p 1615-162010.1016/j.surfcoat.2011.07.083 ↗
21. K. Huang, H.Y. Lee, and J.B. Goodenough, Sr- and Ni- Doped LaCoO3 and LaFeO3 Perovskites New Cathode Materials for Solid-Oxide Fuel Cells, J. Electrochem. Soc., 1998, 145(9), p 3220-322710.1149/1.1838789 ↗
22. M. Gao, C.-J. Li, C.-X. Li, G.-J. Yang, and S.-Q. Fan, Microstructure, Oxygen Stoichiometry and Electrical Conductivity of Flame-Sprayed Sm0.7Sr0.3CoO3−δ, J. Power Sources, 2009, 191(2), p 275-27910.1016/j.jpowsour.2009.02.016 ↗
23. K.S. Anil, S.N. Nair, J. Alias, and S. Date, Evolution of the Cluster Glass System La0.5Sr0.5CoO3, J. Mater. Chem., 1998, 8(10), p 2245-225110.1039/a802952k ↗
24. S. Bohn, S. Douady, and Y. Couder, Four Sided Domains in Hierarchical Space Dividing Patterns, Phys. Rev. Lett., 2005, 94(5), p 05450310.1103/PhysRevLett.94.054503 ↗
25. S. Bohn, Hierarchical Crack Patterns: A Comparison with Two-Dimensional Soap Foams, Colloid Surf. A, 2005, 263(1-3), p 46-5110.1016/j.colsurfa.2004.11.013 ↗
26. J.W. Hutchinson and Z. Suo, Mixed-Mode Cracking in Layered Materials, Adv. Appl. Mech., 1992, 29, p 63-19110.1016/S0065-2156(08)70164-9 ↗
27. S. Kuroda, T. Dendo, and S. Kitahara, Quenching Stress in Plasma-Sprayed Coatings and Its Correlation with the Deposit Microstructure, J. Therm. Spray Technol., 1995, 4(1), p 75-8410.1007/BF02648531 ↗
28. S. Kuroda, T. Fukushima, and S. Kitahara, Significance of Quenching Stress in the Cohesion and Adhesion of Thermally Sprayed Coatings, J. Therm. Spray Technol., 1992, 1(4), p 325-33210.1007/BF02647160 ↗
29. T.W. Clyne, Residual Stresses in Surface Coatings and Their Effects on Interfacial Debonding, Interfacial Effects Part. Fibrous Layered Compos. Mater., 1996, 116-117, p 307-330
30. T.W. Clyne and S.C. Gill, Residual Stresses in Thermal Spray Coatings and Their Effect on Interfacial Adhesion: A Review of Recent Work, J. Therm. Spray Technol., 1996, 5(4), p 401-41810.1007/BF02645271 ↗
31. P. Scardi, M. Leoni, and L. Bertamini, Influence of Phase Stability on the Residual Stress in Partially Stabilized Zirconia TBC Produced by Plasma Spray, Surf. Coat. Technol., 1995, 76(1-3), p 106-11210.1016/0257-8972(95)02496-4 ↗
32. P.J. Withers and H.K.D.H. Bhadeshia, Overview—Residual Stress Part 2—Nature and Origins, Mater. Sci. Technol.-Lond., 2001, 17(4), p 366-37510.1179/026708301101510087 ↗
33. P. Hidnert, and W. Souder, Thermal Expansion of Solids, NBS Circular, 1950, p 486
34. A. Groisman and E. Kaplan, An Experimental-Study of Cracking Induced by Desiccation, Europhys. Lett., 1994, 25(6), p 415-42010.1209/0295-5075/25/6/004 ↗
35. D. Mal, S. Sinha, T. Dutta, S. Mitra, and S. Tarafdar, Formation of Crack Patterns in Clay Films: Desiccation and Relaxation, J. Phys. Soc. Jpn., 2007, 76(1), p 01480110.1143/JPSJ.76.014801 ↗
36. N. Lecocq and N. Vandewalle, Experimental Study of Cracking Induced by Desiccation in 1-Dimensional Systems, Eur. Phys. J. E, 2002, 8(4), p 445-45210.1140/epje/i2002-10040-2 ↗
37. S. Bohn, L. Pauchard, and Y. Couder, Hierarchical Crack Pattern as Formed by Successive Domain Divisions. I. Temporal and Geometrical Hierarchy, Phys. Rev. E, 2005, 71(4), p 04621410.1103/PhysRevE.71.046214 ↗
38. S. Bohn, J. Platkiewicz, B. Andreotti, M. Adda-Bedia, and Y. Couder, Hierarchical Crack Pattern as Formed by Successive Domain Divisions. II. From Disordered to Deterministic Behavior, Phys. Rev. E, 2005, 71(4), p 04621510.1103/PhysRevE.71.046215 ↗
39. J. Richardi, A.T. Ngo, and M.P. Pileni, Simulations of Cracks Supported by Experiments: The Influence of the Film Height and Isotropy on the Geometry of Crack Patterns, J. Phys. Chem. C, 2010, 114(41), p 17324-1733210.1021/jp104329g ↗
40. K.A. Shorlin, J.R. de Bruyn, M. Graham, and S.W. Morris, Development and Geometry of Isotropic and Directional Shrinkage-Crack Patterns, Phys. Rev. E, 2000, 61(6), p 6950-695710.1103/PhysRevE.61.6950 ↗
41. J. Stavans, The Evolution of Cellular Structures, Rep. Prog. Phys., 1993, 56(6), p 733-78910.1088/0034-4885/56/6/002 ↗
42. D. Weaire and N. Rivier, Soap, Cells and Statistics - Random Patterns in Two Dimensions (Reprinted from Contemporary Physics, vol 25, page 59, 1984), Contemp. Phys., 2009, 50(1), p 199-23910.1080/00107510902734680 ↗
43. Y. Couder, L. Pauchard, C. Allain, M. Adda-Bedia, and S. Douady, The Leaf Venation as Formed in a Tensorial Field, Eur. Phys. J. B, 2002, 28(2), p 135-13810.1140/epjb/e2002-00211-1 ↗
44. C.A. Tang, Y.B. Zhang, Z.Z. Liang, T. Xu, L.G. Tham, P.A. Lindqvist, S.Q. Kou, and H.Y. Liu, Fracture Spacing in Layered Materials and Pattern Transition from Parallel to Polygonal Fractures, Phys. Rev. E, 2006, 73(5), p 05612010.1103/PhysRevE.73.056120 ↗
45. K. Leung and Z. Neda, Pattern Formation and Selection in Quasistatic Fracture, Phys. Rev. Lett., 2000, 85(3), p 662-66510.1103/PhysRevLett.85.662 ↗
46. K.T. Leung and Z. Neda, Criticality and Pattern Formation in Fracture by Residual Stresses, Phys. Rev. E, 2010, 82(4), p 04611810.1103/PhysRevE.82.046118 ↗
47. S. Nag, S. Sinha, S. Sadhukhan, T. Dutta, and S. Tarafdar, Crack Patterns in Desiccating Clay-Polymer Mixtures with Varying Composition, J. Phys. Condens. Mater., 2010, 22(1), p 01540210.1088/0953-8984/22/1/015402 ↗
48. M.D. Thouless, E. Olsson, and A. Gupta, Cracking of Brittle Films on Elastic Substrates, Acta Metall. Mater., 1992, 40(6), p 1287-129210.1016/0956-7151(92)90429-I ↗
49. R.T. Murray, C.J. Kiely, and M. Hopkinson, Crack Formation in III-V Epilayers Grown Under Tensile Strain on InP(001) Substrates, Philos. Mag. A, 1996, 74(2), p 383-39310.1080/01418619608242149 ↗
50. R.T. Murray, C.J. Kiely, and M. Hopkinson, General Characteristics of Crack Arrays in Epilayers Grown Under Tensile Strain, Semicond. Sci. Technol., 2000, 15(4), p 325-3305110.1088/0268-1242/15/4/304 ↗
51. A. Kelly, Strong Solids, Oxford University Press, Oxford, 1966, p 3-11
52. A. Kelly and W.R. Tyson, Tensile Properties of Fibre-Reinforced Metals: Copper/Tungsten and Copper/Molybdenum, J. Mech. Phys. Solids, 1965, 13(6), p 329-35010.1016/0022-5096(65)90035-9 ↗
53. A.C. Kimber and J.G. Keer, On the Theoretical Average Crack Spacing in Brittle Matrix Composites Containing Continuous Aligned Fibers, J. Mater. Sci. Lett., 1982, 1(8), p 353-35410.1007/BF00726486 ↗